# US 2025/0096314 A1 · Solid electrolyte material and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0096314 A1
- Document ID: US20250096314A1
- Status: Published application
- Kind: A1
- Application number: 18/961,130
- Filed: 2024-11-26
- Published: 2025-03-20
- Earliest claimed: 2022-06-07
- Assignees: Panasonic Intellectual Property Management Co., Ltd.
- Applicants: Panasonic Intellectual Property Management Co., Ltd.
- Inventors: EIICHI KOGA
- Web page: https://patentgrep.com/patent/US20250096314A1

## CPC

- H01M 10/0562: Solid materials
- C01G 23/002: {Compounds containing titanium, with or without oxygen or hydrogen, and containing two or more other elements (C01G23/001, C01G23/003 take precedence)}
- H01B 1/06: mainly consisting of other non-metallic substances
- H01B 13/00: Apparatus or processes specially adapted for manufacturing conductors or cables
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2300/008: Halides
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The solid electrolyte material of the present disclosure is a solid electrolyte material containing Li, Ti, and F, comprising an amorphous substance containing Li, Ti, and F. The solid electrolyte material of the present disclosure may further comprise a crystalline phase containing Li, Ti, and F. The solid electrolyte material production method of the present disclosure comprises: (A) synthesizing a compound comprising a crystalline phase containing Li, Ti, and F; and (B) performing a treatment to disturb the crystal of the compound. The compound may be mechanochemically treated in the step (B).

## Claims

### Claim 1

A solid electrolyte material containing Li, Ti, and F, comprising an amorphous substance containing Li, Ti, and F.

### Claim 2 (depends on 1)

The solid electrolyte material according to claim 1, wherein the solid electrolyte material is a solid solution.

### Claim 3 (depends on 1)

The solid electrolyte material according to claim 1, wherein in an X-ray diffraction pattern obtained by powder X-ray diffraction measurement of the solid electrolyte material, at least one peak is present in each of a first range in which the diffraction angle 2θ is greater than or equal to 20° and less than or equal to 22°, a second range in which the diffraction angle 2θ is greater than or equal to 40° and less than or equal to 42°, and a third range in which the diffraction angle 2θ is greater than or equal to 26° and less than or equal to 28°, and wherein the half width of the strongest peak in the first range is greater than or equal to 1°.

### Claim 4 (depends on 3)

The solid electrolyte material according to claim 3, wherein the strongest peak in the first range has a higher intensity than the strongest peak in the second range, and the strongest peak in the second range has a higher intensity than the strongest peak in the third range.

### Claim 5 (depends on 1)

The solid electrolyte material according to claim 1, wherein the solid electrolyte material is in particulate form.

### Claim 6 (depends on 5)

The solid electrolyte material according to claim 5, wherein the crystallinity of the surface of the solid electrolyte material is lower than the crystallinity in the center of the solid electrolyte material.

### Claim 7 (depends on 1)

The solid electrolyte material according to claim 1, further containing at least one selected from the group consisting of Ni, Mo, Cr, Fe, and ZrO2.

### Claim 8 (depends on 1)

The solid electrolyte material according to claim 1, further comprising a crystalline phase containing Li, Ti, and F.

### Claim 9 (depends on 8)

The solid electrolyte material according to claim 8, wherein the crystalline phase comprises a tetragonal crystal.

### Claim 10

A method for producing a solid electrolyte material, comprising:
(A) synthesizing a compound comprising a crystalline phase containing Li, Ti, and F; and
(B) performing a treatment to disturb the crystal of the compound.

### Claim 11 (depends on 10)

The method for producing a solid electrolyte material according to claim 10, wherein the compound is synthesized in the step (A) by heat-treatment of a mixture of raw materials.

### Claim 12 (depends on 11)

The method for producing a solid electrolyte material according to claim 11, wherein the mass change rate of the compound before and after the heat-treatment is less than or equal to 1%.

### Claim 13 (depends on 10)

The method for producing a solid electrolyte material according to claim 10, wherein the compound is mechanochemically treated in the step (B).

### Claim 14 (depends on 13)

The method for producing a solid electrolyte material according to claim 13, wherein the mechanochemical treatment is ball milling.