# US 2025/0096310 A1 · Lithium-Based Solid-State Electrolyte with Lithium Ions Exchanged by Ions Having a Larger Ionic Radius

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0096310 A1
- Document ID: US20250096310A1
- Status: Published application
- Kind: A1
- Application number: 18/884,537
- Filed: 2024-09-13
- Published: 2025-03-20
- Earliest claimed: 2023-09-18
- Applicants: Brown University
- Inventors: Brian W. Sheldon; Yue Qi; Sydney Morris; Harsh D. Jagad; Stephen J. Harris
- Web page: https://patentgrep.com/patent/US20250096310A1

## CPC

- H01M 10/0562: Solid materials
- H01M 10/052: Li-accumulators
- H01M 10/054: Accumulators with insertion or intercalation of metals other than lithium, e.g. with magnesium or aluminium
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present disclosure describes a method of providing residual compressive stress to a lithium-based solid electrolyte by ion exchanging lithium ions with ions having a larger ionic radius that the lithium ions.

## Claims

### Claim 1

A method of providing residual compressive stress to a lithium-based solid electrolyte comprising
subjecting the lithium-based solid electrolyte to ion exchange conditions where lithium ions within the lithium-based solid electrolyte are exchanged with ions in a sub surface region of the lithium-based solid electrolyte so as to impart residual compressive stresses in the sub-surface region of the lithium-based solid electrolyte,
wherein the ions have a larger ionic radius than the lithium ions.

### Claim 2 (depends on 1)

The method of claim 1 wherein the ions are members of the group consisting of potassium ions, silver ions, sodium ions, and calcium ions and mixtures thereof.

### Claim 3 (depends on 1)

The method of claim 1 wherein lithium ions are exchanged with ions having a larger ionic radius than the lithium ions in an amount to allow sufficient lithium ion diffusion for performance of the solid state electrolyte in a solid-state battery.

### Claim 4 (depends on 1)

The method of claim 1 wherein the ions are potassium ions.

### Claim 5 (depends on 1)

The method of claim 1 wherein between 2% and 5% lithium ions of the lithium-based solid electrolyte are exchanged with potassium ions.

### Claim 6 (depends on 1)

The method of claim 1 wherein between 3% and 4% lithium ions of the lithium-based solid electrolyte are exchanged with potassium ions.

### Claim 7 (depends on 1)

The method of claim 1 wherein 3.4% lithium ions of the lithium-based solid electrolyte are exchanged with potassium ions.

### Claim 8 (depends on 1)

The method of claim 1 wherein the lithium-based solid electrolyte comprises lithium lanthanum zirconium oxide.

### Claim 9 (depends on 1)

The method of claim 1 wherein the lithium-based solid electrolyte is contacted with a source of ions and heated to a temperature sufficient to promote exchange of lithium ions of the lithium-based solid electrolyte with ions of the source of ions.

### Claim 10 (depends on 1)

The method of claim 1 wherein the residual compressive stresses inhibit dendrite formation in the lithium-based solid electrolyte.

### Claim 11 (depends on 1)

The method of claim 1 wherein the subsurface region is at least 40 microns deep from the surface of the lithium-based solid electrolyte.

### Claim 12 (depends on 1)

The method of claim 1 wherein the subsurface region is at least 20 microns deep from the surface of the lithium-based solid electrolyte.

### Claim 13 (depends on 1)

The method of claim 1 wherein the ion exchange depth ratio is 0.2% to 4% of the thickness of the lithium-based solid electrolyte.

### Claim 14 (depends on 1)

The method of claim 1 wherein lithium ions diffuse out of the lithium-based solid electrolyte and the ions from a source of ions diffuse into the lithium-based solid electrolyte.

### Claim 15 (depends on 1)

The method of claim 1 wherein the ions are silver ions.

### Claim 16 (depends on 1)

The method of claim 1 wherein the ions are monovalent or divalent cationic ions.

### Claim 17

A lithium-based solid electrolyte comprising diffused potassium ions or diffused silver ions.

### Claim 18 (depends on 17)

The lithium-based solid electrolyte of claim 17 wherein the amount of diffused potassium ions or diffused silver ions allow sufficient lithium ion diffusion for performance of the solid-state electrolyte in a solid-state battery.

### Claim 19 (depends on 17)

The lithium-based solid electrolyte of claim 17 comprising lithium lanthanum zirconium oxide.

### Claim 20 (depends on 17)

The lithium-based solid electrolyte of claim 17 having a higher residual compressive stress compared to a lithium-based solid electrolyte lacking diffused potassium ions or diffused silver ions.

### Claim 21 (depends on 17)

The lithium-based solid electrolyte of claim 17 resistant to dendrite formation.

### Claim 22 (depends on 17)

A solid-state battery comprising the lithium-based solid electrolyte of claim 17.