# US 2025/0096305 A1 · Method for preparing lithium-ion batteries

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0096305 A1
- Document ID: US20250096305A1
- Status: Published application
- Kind: A1
- Application number: 18/964,244
- Filed: 2024-11-29
- Published: 2025-03-20
- Earliest claimed: 2024-11-07
- Assignees: Zhejiang Jinko Energy Storage Co., Ltd.
- Applicants: Zhejiang Jinko Energy Storage Co., Ltd.
- Inventors: Jing CHEN; Zixiang YANG
- Web page: https://patentgrep.com/patent/US20250096305A1

## CPC

- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/052: Li-accumulators
- H01M 10/0567: characterised by the additives
- H01M 10/0568: characterised by the solutes
- H01M 10/0569: characterised by the solvents
- H01M 10/058: Construction or manufacture
- H01M 10/0587: of accumulators having only wound construction elements, i.e. wound positive electrodes, wound negative electrodes and wound separators
- H01M 2300/0037: Mixture of solvents
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed is a method for preparing lithium-ion batteries including: winding or sheet-stacking a positive electrode sheet, a negative electrode sheet, and a separator, and then placing them into a case to form an initial cell; injecting a first electrolyte into the initial cell, where the first electrolyte includes: 0.5 wt % to 2 wt % vinylene carbonate, 5 wt % to 15 wt % lithium salt, and non-aqueous organic solvent (all by weight); performing a formation process on the initial cell to form an initial solid electrolyte interphase film; injecting a second electrolyte into the initial cell, where the second electrolyte includes: 5 wt % to 20 wt % vinylene carbonate, 5 wt % to 15 wt % lithium salt, 0.005 wt % to 30 wt % infiltrant stabilizer, and non-aqueous organic solvent (all by weight); where the first electrolyte or the second electrolyte further includes: at least one of 1,3-propane sultone or fluoroethylene carbonate.

## Claims

### Claim 1

A method for preparing lithium-ion batteries, comprising:
providing a positive electrode sheet, a negative electrode sheet, and a separator;
winding or sheet-stacking the positive electrode sheet, the negative electrode sheet, and the separator, and then placing them into a case to form an initial cell, wherein the separator is positioned between the positive electrode sheet and the negative electrode sheet;
injecting a first electrolyte into the initial cell, wherein the first electrolyte comprises:
0.5 wt % to 2 wt % vinylene carbonate, 5 wt % to 15 wt % lithium salt, and non-aqueous organic solvent (all by weight);
performing a formation process on the initial cell to form an initial solid electrolyte interphase (SEI) film; and
injecting a second electrolyte into the initial cell, wherein the second electrolyte comprises: 5 wt % to 20 wt % vinylene carbonate, 5 wt % to 15 wt % lithium salt, 0.005 wt % to 30 wt % infiltrant stabilizer, and non-aqueous organic solvent (all by weight);
wherein the first electrolyte or the second electrolyte further comprises: at least one of 1,3-propane sultone or fluoroethylene carbonate, wherein an amount of 1,3-propane sultone is within a range of 0.1 wt % to 2 wt % by weight, and an amount of fluoroethylene carbonate is within a range of 0.1 wt % to 2 wt % by weight.

### Claim 2 (depends on 1)

The method for preparing lithium-ion batteries according to claim 1, wherein the first electrolyte comprises 0.1 wt % to 2 wt % 1,3-propane sultone and 0.1 wt % to 2 wt % fluoroethylene carbonate.

### Claim 3 (depends on 1)

The method for preparing lithium-ion batteries according to claim 1, wherein the lithium salt is selected from lithium perchlorate (LiClO4), lithium tetrafluoroborate (LiBF4), lithium hexafluoroarsenate (LiAsF6), and lithium hexafluorophosphate (LiPF6).

### Claim 4 (depends on 1)

The method for preparing lithium-ion batteries according to claim 1, wherein the first electrolyte further comprises at least one of positive electrode film-forming agent or negative electrode film-forming agent.

### Claim 5 (depends on 4)

The method for preparing lithium-ion batteries according to claim 4, wherein an amount of the positive electrode film-forming agent is within a range of 0.1 wt % to 0.3 wt %, 0.3 wt % to 0.5 wt %, 0.5 wt % to 2 wt %, 2 wt % to 3 wt %, 3 wt % to 4 wt %, or 4 wt % to 5 wt %.

### Claim 6 (depends on 4)

The method for preparing lithium-ion batteries according to claim 4, wherein the positive electrode film-forming agent is at least one of lithium difluorophosphate, 1,5,2,4-dioxadithiane 2,2,4,4-tetraoxide, 1,3,2-dioxathiolane 2,2-dioxide, prop-1-ene-1,3-sultone, tris(trimethylsilyl) borate, tris(trimethylsilyl) phosphate, 1H-Imidazole-1-carboxylicacid, 2-propynylester(9CI), triallyl isocyanurate, 2,4-toluene diisocyanate, 2-phenyl-1-yl 1H-imidazole-1-sulfonic acid ester, hexamethylene diisocyanate, lithium bis[ethanedioato(2-)-κO1,κO2]difluorophosphate(1-), 2-fluoropyridine, lithium bis(oxalate) borate, or lithium difluoro(oxalato)borate(1-).

### Claim 7 (depends on 4)

The method for preparing lithium-ion batteries according to claim 4, wherein an amount of the negative electrode film-forming agent is within a range of 0.1 wt % to 0.3 wt %, 0.3 wt % to 0.5 wt %, 0.5 wt % to 2 wt %, or 2 wt % to 3 wt %.

### Claim 8 (depends on 4)

The method for preparing lithium-ion batteries according to claim 4, wherein the negative electrode film-forming agent is at least one of 1,3,2-dioxathiolane 2,2-dioxide, 1,5,2,4-dioxadithiane 2,2,4,4-tetraoxide, lithium difluoro(oxalato)borate(1-), propylene sulfate, lithium bis[ethanedioato(2-)-κO1,κO2]difluorophosphate(1-), tris(trimethylsilyl) phosphate, lithium bis(oxalato) borate, 1,3-propylene disulfonic acid methyl ester, and trimethylsilyl phosphate.

### Claim 9 (depends on 4)

The method for preparing lithium-ion batteries according to claim 4, wherein the first electrolyte comprises 0.5 wt % to 2 wt % vinylene carbonate, 5 wt % to 15 wt % lithium salt, 0.5 wt % to 3 wt % positive electrode film-forming agent, and non-aqueous organic solvent (all by weight).

### Claim 10 (depends on 4)

The method for preparing lithium-ion batteries according to claim 4, wherein the first electrolyte comprises 0.5 wt % to 2 wt % vinylene carbonate, 5 wt % to 15 wt % lithium salt, 0.5 wt % to 2 wt % negative electrode film-forming agent, and non-aqueous organic solvent (all by weight).

### Claim 11 (depends on 4)

The method for preparing lithium-ion batteries according to claim 4, wherein the first electrolyte comprises 0.5 wt % to 2 wt % vinylene carbonate, 5 wt % to 15 wt % lithium salt, 0.5 wt % to 3 wt % positive electrode film-forming agent, 0.5 wt % to 2 wt % negative electrode film-forming agent and non-aqueous organic solvent (all by weight).

### Claim 12 (depends on 1)

The method for preparing lithium-ion batteries according to claim 1, wherein the non-aqueous organic solvent of the first electrolyte comprises two or more of ethyl methyl carbonate, dimethyl carbonate, diethyl carbonate, methyl ethyl carbonate, ethyl acetate, n-propyl acetate, methyl propionate, methyl acetate, ethyl propionate, propyl propionate, ethyl butyrate, methyl propyl carbonate, propylene carbonate, γ-butyrolactone, and γ-valerolactone.

### Claim 13 (depends on 1)

The method for preparing lithium-ion batteries according to claim 1, wherein after performing the formation process on the initial cell and before injecting the second electrolyte into the initial cell, the method further comprises: performing a replenishment treatment on the initial cell, wherein the first electrolyte is replenished into the initial cell.

### Claim 14 (depends on 13)

The method for preparing lithium-ion batteries according to claim 13, wherein before performing the formation process on the initial cell, the method comprises:
weighing the initial cell to obtain a first mass of the initial cell; and
after performing the formation process on the initial cell, the method comprises:
weighing the initial cell again to obtain a second mass of the initial cell;
wherein a mass of the first electrolyte replenished during the replenishment treatment is a difference between the first mass and the second mass.

### Claim 15 (depends on 1)

The method for preparing lithium-ion batteries according to claim 1, wherein the infiltrant stabilizer is selected from: one of poly(ethyleneglycol) 2-[ethyl[(heptadecafluorooctyl)sulfonyl]amino]ethyl ether, 2-(N-Ethylperfluorooctanesulfonamido)ethyl methacrylate, fluorobenzene, 2,2,3,3-tetrafluoro-1-(1,1,2,2-tetrafluoroethoxy)propane, hexafluoropropyl ethylene glycol, and trifluoro(trifluoromethyl)oxirane.

### Claim 16 (depends on 1)

The method for preparing lithium-ion batteries according to claim 1, wherein the first electrolyte comprises: at least one of positive electrode film-forming agent or negative electrode film-forming agent, where an amount of the positive electrode film-forming agent is within a range of 0.5 wt % to 3 wt % by weight, and an amount of the negative electrode film-forming agent is within a range of 0.5 wt % to 2 wt % by weight.

### Claim 17 (depends on 1)

The method for preparing lithium-ion batteries according to claim 1, wherein the first electrolyte accounts for 65 wt % to 90 wt % by weight of a total mass of the first electrolyte and the second electrolyte.

### Claim 18 (depends on 1)

The method for preparing lithium-ion batteries according to claim 1, wherein an injection volume of the first electrolyte is within a range of 3.5 g/Ah to 4 g/Ah; and an injection volume of the second electrolyte is within a range of 3.5 g/Ah to 4 g/Ah.

### Claim 19 (depends on 1)

The method for preparing lithium-ion batteries according to claim 1, wherein the formation process comprises: first high-temperature standing, negative-pressure formation, and aging standing.

### Claim 20 (depends on 19)

The method for preparing lithium-ion batteries according to claim 19, wherein after injecting the second electrolyte into the initial cell, the method comprises: performing a second high-temperature standing process on the initial cell, wherein a temperature of the second high-temperature standing process is higher than that of the first high-temperature standing process.