# US 2025/0096277 A1 · Current collector for secondary battery and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0096277 A1
- Document ID: US20250096277A1
- Status: Published application
- Kind: A1
- Application number: 18/726,860
- Filed: 2023-01-05
- Published: 2025-03-20
- Earliest claimed: 2022-01-07
- Assignees: Lillem Co.,Ltd.
- Applicants: Lillem Co.,Ltd.
- Inventors: Sung Min PARK; Sungwook MOON; Kyudong HAN
- Web page: https://patentgrep.com/patent/US20250096277A1

## CPC

- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/052: Li-accumulators
- H01M 4/667: {in the form of layers, e.g. coatings}
- H01M 4/74: Meshes or woven material; Expanded metal
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention relates to a current collector for a secondary battery and a method of preparing the same, and more specifically, comprises a conductive substrate comprising a first metal; and a coating layer coated on a surface of the conductive substrate. The coating layer comprises a second metal, carbon (C), phosphorus (P), and oxygen (O), and the second metal is different from the first metal, and a first water contact angle (A) of a surface of the coating layer is 1° to 45°.

## Claims

### Claim 1

A current collector for a secondary battery comprising:
a conductive substrate comprising a first metal; and
a coating layer coated on a surface of the conductive substrate,
wherein the coating layer comprises a second metal, carbon (C), phosphorus (P), and oxygen (O), and the second metal is different from the first metal, and a first water contact angle (A) of a surface of the coating layer is 1° to 45°.

### Claim 2 (depends on 1)

The current collector for a secondary battery of claim 1, wherein the first metal is one or an alloy of at least two selected from the group consisting of aluminum, copper, stainless steel, nickel-plated copper, nickel, titanium, palladium, iron alloys, and aluminum alloys.

### Claim 3 (depends on 1)

The current collector for a secondary battery of claim 1, wherein the second metal is at least one selected from the group consisting of chromium (Cr), iron (Fe), cobalt (Co), manganese (Mn), nickel (Ni), zirconium (Zr) and titanium (Ti).

### Claim 4 (depends on 1)

The current collector for a secondary battery of claim 1, wherein in a result of energy dispersive spectroscopy (EDX) analysis of surface of the current collector, atomic fraction of the first metal is 40 at % to 90 at %, and total atomic fraction of the second metal, the carbon (C), the phosphorus (P), and the oxygen (O) is 10 at % to 60 at %.

### Claim 5 (depends on 1)

The current collector for a secondary battery of claim 1, wherein in a result of energy dispersive spectroscopy (EDX) analysis of surface of the current collector,
ratio of number of carbon (C) atoms to number of atoms of the second metal is 10 to 50;
ratio of number of phosphorus (P) atoms to number of atoms of the second metal is 15 to 35; and
ratio of number of oxygen (O) atoms to number of atoms of the second metal is 85 to 150.

### Claim 6 (depends on 1)

The current collector for a secondary battery of claim 1, wherein the conductive substrate has a form of film, sheet, foil, mesh, net, porous body, foam, or nonwoven fabric.

### Claim 7 (depends on 1)

The current collector for a secondary battery of claim 1, wherein the coating layer has a thickness of 10 nm to 5 μm.

### Claim 8 (depends on 1)

An electrode for a secondary battery comprising:
the secondary battery current collector of claim 1; and
an active material layer on the current collector.

### Claim 9 (depends on 8)

A secondary battery comprising a cathode, an anode, a separator between the cathode and the anode, and an electrolyte,
wherein at least one of the cathode and the anode comprises the electrode for a secondary battery of claim 8.

### Claim 10

A current collector for a secondary battery comprising:
a conductive substrate comprising a first metal; and
a coating layer coated on a surface of the conductive substrate,
wherein the coating layer comprises a second metal, carbon (C), phosphorus (P), and oxygen (O); the second metal is different from the first metal; surface of the coating layer has a first water contact angle (A); the surface of the conductive substrate has a second water contact angle (B); and difference (B−A) between the second water contact angle (B) and the first water contact angle (A) is 10° to 140°.

### Claim 11 (depends on 10)

A current collector for a secondary battery of claim 10, wherein the difference (B−A) is 20° to 100°.

### Claim 12 (depends on 10)

The current collector for a secondary battery of claim 10, wherein the first water contact angle (A) is 1° to 45°, and the second water contact angle (B) is 50° to 140°.

### Claim 13 (depends on 10)

The current collector for a secondary battery of claim 10, wherein the first metal is one or an alloy of at least two selected from the group consisting of aluminum, copper, stainless steel, nickel-plated copper, nickel, titanium, palladium, iron alloys, and aluminum alloys.

### Claim 14 (depends on 10)

The current collector for a secondary battery of claim 10, wherein the second metal is at least one selected from the group consisting of chromium (Cr), iron (Fe), cobalt (Co), manganese (Mn), nickel (Ni), zirconium (Zr) and titanium (Ti).

### Claim 15

A method of preparing a current collector for a secondary battery, comprising:
adding a metal compound, an inorganic acid, an organic acid, and a first conductive agent into a first solvent to prepare a coating composition; and
coating the coating composition on a surface of a conductive substrate to form a coating layer,
wherein the conductive substrate comprises a first metal,
a second metal of the metal compound is different from the first metal, and
surface of the coating layer has a first water contact angle (A) of 1° to 45°.

### Claim 16 (depends on 15)

The method of preparing a current collector for a secondary battery of claim 15, wherein surface of the conductive substrate has a second water contact angle (B), and the second water contact angle (B) is larger than the first water contact angle (A).

### Claim 17 (depends on 15)

The method of preparing a current collector for a secondary battery of claim 15, wherein the metal compound comprises at least one selected from the group consisting of:
chromium potassium alum (KCr(SO4)2·12H2O), chromium chloride (CrCl3), chromium fluoride (CrF3), chromium hydroxide (Cr(OH)3), chromium nitrate (Cr(NO3)3), chromium phosphate (CrPO4), iron chromate (FeCr2O4) and hydrates thereof;
cobalt chloride (CoCl2), cobalt acetate (Co(CH3COO)2·4H2O), cobalt sulfate (CoSO4), zinc sulfate (ZnSO4), manganese sulfate (MnSO4), nickel sulfate (NiSO4) and hydrates thereof;
zirconium phosphate (Zr(HPO4)2), zirconium sulfate (Zr(SO4)2), zirconium nitrate (ZrO(NO3)2), zirconium hydroxide (Zr(OH)4);
zirconium fluoride (H2ZrF6) and its soluble salts (Na2ZrF6, K2ZrF6, Zr(NH4)2F6); and
titanium dioxide (TiO2).

### Claim 18 (depends on 15)

The method of preparing a current collector for a secondary battery of claim 15, wherein the first metal is at least one selected from the group consisting of aluminum, copper, stainless steel, nickel-plated copper, nickel, titanium, palladium, and an aluminum alloy.