# US 2025/0096254 A1 · Lithium battery positive material and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0096254 A1
- Document ID: US20250096254A1
- Status: Published application
- Kind: A1
- Application number: 18/494,778
- Filed: 2023-10-26
- Published: 2025-03-20
- Earliest claimed: 2023-09-15
- Assignees: Nan Ya Plastics Corporation
- Applicants: Nan Ya Plastics Corporation
- Inventors: Te-Chao Liao; Wei-Sheng Cheng; Chia-Shan Chang; Yu-Chi Hsieh
- Web page: https://patentgrep.com/patent/US20250096254A1

## CPC

- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/366: {as layered products}
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/625: {Carbon or graphite}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A lithium battery positive material includes lithium nickel manganese oxide (LNMO) doped with copper, titanium, nitrogen, and carbon. In addition, a manufacturing method of the lithium battery positive material is also provided.

## Claims

### Claim 1

A lithium battery positive material, comprising lithium nickel manganese oxide doped with copper, titanium, nitrogen, and carbon.

### Claim 2 (depends on 1)

The lithium battery positive material according to claim 1, wherein a weight ratio of lithium nickel manganese oxide: copper/titanium: nitrogen/carbon in the lithium nickel manganese oxide doped with copper, titanium, nitrogen, and carbon ranges from 1:0.4:0.1 to 1:0.1:0.1.

### Claim 3 (depends on 1)

The lithium battery positive material according to claim 1, wherein an average particle size of the lithium nickel manganese oxide doped with copper, titanium, nitrogen, and carbon is 0.5 microns to 20 microns.

### Claim 4

A manufacturing method for manufacturing a lithium battery positive material, the manufacturing method comprising:
using a copper source, a titanium source, and lithium nickel manganate powder to form a precursor of lithium nickel manganese oxide doped with copper and titanium by performing a co-precipitation method, a filtration process, and a sintering process; and
mixing the precursor of the lithium nickel manganese oxide doped with copper and titanium with a carbon source, and coating a nitrogen source by a supercritical fluid extraction method to obtain the lithium nickel manganese oxide doped with copper, titanium, nitrogen, and carbon.

### Claim 5 (depends on 4)

The manufacturing method for manufacturing the lithium battery positive material according to claim 4, wherein the copper source comprises copper chloride, copper sulfate, copper sulfite, copper nitrate, copper acetate, or a combination thereof.

### Claim 6 (depends on 4)

The manufacturing method for manufacturing the lithium battery positive material according to claim 4, wherein the titanium source comprises titanium chloride, titanium sulfate, titanium nitrate, or a combination thereof.

### Claim 7 (depends on 4)

The manufacturing method for manufacturing the lithium battery positive material according to claim 4, wherein the nitrogen source comprises dopamine, p-phenylenediamine, or a combination thereof.

### Claim 8 (depends on 4)

The manufacturing method for manufacturing the lithium battery positive material according to claim 4, wherein the carbon source comprises graphene, glucose, or a combination thereof.

### Claim 9 (depends on 4)

The manufacturing method for manufacturing the lithium battery positive material according to claim 4, wherein a co-precipitation agent used in the co-precipitation method comprises water, ethanol, isopropyl alcohol, acetone, methyl ethyl ketone, ammonia, sodium hydroxide, sodium carbonate, or a combination thereof; a co-precipitation reaction temperature in the co-precipitation method ranges from 25° C. to 100° C., and a co-precipitation reaction time in the co-precipitation method ranges from 1 minute to 30 minutes.

### Claim 10 (depends on 4)

The manufacturing method for manufacturing the lithium battery positive material according to claim 4, wherein a temperature of the sintering process ranges from 400° C. to 1000° C.