# US 2025/0096233 A1 · Manufacturing method of lithium battery negative electrode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0096233 A1
- Document ID: US20250096233A1
- Status: Published application
- Kind: A1
- Application number: 18/493,718
- Filed: 2023-10-24
- Published: 2025-03-20
- Earliest claimed: 2023-09-18
- Assignees: Nan Ya Plastics Corporation
- Applicants: Nan Ya Plastics Corporation
- Inventors: Te-Chao Liao; Chun-Che Tsao; Li-Ting Wang
- Web page: https://patentgrep.com/patent/US20250096233A1

## CPC

- H01M 4/139: Processes of manufacture
- H01M 4/0452: {from solutions}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0568: characterised by the solutes
- H01M 10/0569: characterised by the solvents
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A manufacturing method of a lithium battery negative electrode includes the following. A copper foil is providing. An electroplating process is performed to form a lithium deposition layer on the copper foil. An electrolyte solution used in the electroplating process includes an organic solvent and fluorine-containing lithium salt. The organic solvent includes ester solvents, ether solvents, alcohol solvents, or combinations thereof, and the fluorine-containing lithium salt includes LiPF6, LiFSI, LiTF, LiDFOB, LiTFSI, or combinations thereof.

## Claims

### Claim 1

A manufacturing method of a lithium battery negative electrode, comprising:
providing a copper foil; and
performing an electroplating process to form a lithium deposition layer on the copper foil, wherein an electrolyte solution used in the electroplating process comprises an organic solvent and fluorine-containing lithium salt, wherein the organic solvent comprises an ester solvent, an ether solvent, an alcohol solvent, or a combination thereof, and the fluorine-containing lithium salt comprises lithium hexafluorophosphate, lithium bis(fluorosulfonyl)imide, lithium trifluoromethanesulfonate, lithium difluoro(oxalato)borate, lithium bis(trifluoromethanesulfonyl)imide, or a combination thereof.

### Claim 2 (depends on 1)

The manufacturing method of the lithium battery negative electrode according to claim 1, wherein the electrolyte solution at least comprises the ester solvent, and a volume ratio thereof accounts for more than 50%.

### Claim 3 (depends on 1)

The manufacturing method of the lithium battery negative electrode according to claim 1, wherein a usage ratio of the fluorine-containing lithium salt in the electrolyte solution is between 0.1 mol/L and 5 mol/L.

### Claim 4 (depends on 1)

The manufacturing method of the lithium battery negative electrode according to claim 1, wherein a current density in the electroplating process is between 1 mA/cm2 and 5 mA/cm2.

### Claim 5 (depends on 1)

The manufacturing method of the lithium battery negative electrode according to claim 1, wherein a thickness of the lithium deposition layer is between 1 micron and 20 microns.

### Claim 6 (depends on 1)

The manufacturing method of the lithium battery negative electrode according to claim 1, wherein the electrolyte solution further comprises an additive, and the additive comprises lithium nitrate.

### Claim 7 (depends on 6)

The manufacturing method of the lithium battery negative electrode according to claim 6, wherein a usage ratio of the additive in the electrolyte solution is between 1 wt % and 10 wt %.

### Claim 8 (depends on 1)

The manufacturing method of the lithium battery negative electrode according to claim 1, wherein the organic solvent is selected from a combination of the ester solvent and the ether solvent.

### Claim 9 (depends on 8)

The manufacturing method of the lithium battery negative electrode according to claim 8, wherein a volume ratio of the ester solvent and the ether solvent is between 3:1 and 1:1.

### Claim 10 (depends on 1)

The manufacturing method of the lithium battery negative electrode according to claim 1, wherein a surface of the lithium deposition layer comprises a fluorine-containing compound.