# US 2025/0096229 A1 · Anode for lithium secondary battery, lithium secondary battery including the same and method of preparing anode composition for lithium secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0096229 A1
- Document ID: US20250096229A1
- Status: Published application
- Kind: A1
- Application number: 18/889,379
- Filed: 2024-09-19
- Published: 2025-03-20
- Earliest claimed: 2023-09-20
- Assignees: SK On Co., Ltd.
- Applicants: SK On Co., Ltd.
- Inventors: So Hyun PARK
- Web page: https://patentgrep.com/patent/US20250096229A1

## CPC

- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An anode for a lithium secondary battery includes an anode current collector, and an anode mixture layer formed on at least one surface of the anode current collector. The anode mixture layer includes mixture materials that includes an anode active material including a silicon-based active material and a carbon-based active material. A binding force between the mixture materials in the anode mixture layer is in a range from 0.335 kN/m to 0.55 kN/m. An adhesion force between the anode current collector and the anode mixture layer is in a range from 5.8 gf/cm to 11 gf/cm.

## Claims

### Claim 1

An anode for a lithium secondary battery, comprising:
an anode current collector; and
an anode mixture layer formed on at least one surface of the anode current collector, the anode mixture layer comprising mixture materials that includes an anode active material including a silicon-based active material and a carbon-based active material, and
wherein a binding force between the mixture materials in the anode mixture layer is in a range from 0.335 kN/m to 0.55 kN/m, and
an adhesion force between the anode current collector and the anode mixture layer is in a range from 5.8 gf/cm to 11 gf/cm.

### Claim 2 (depends on 1)

The anode for a lithium secondary battery according to claim 1, wherein the binding force is in a range from 0.35 kN/m to 0.45 kN/m.

### Claim 3 (depends on 1)

The anode for a lithium secondary battery according to claim 1, wherein the adhesion force is in a range from 6 gf/cm to 10.5 gf/cm.

### Claim 4 (depends on 1)

The anode for a lithium secondary battery according to claim 1, wherein a standard deviation of the adhesion force is in a range from 0.008 to 0.047.

### Claim 5 (depends on 1)

The anode for a lithium secondary battery according to claim 1, wherein the silicon-based active material includes at least one selected from the group consisting of silicon, a silicon oxide (SiOx, 0<x<2), and a carbon-silicon composite active material.

### Claim 6 (depends on 1)

The anode for a lithium secondary battery according to claim 1, wherein the carbon-based active material includes a graphite-based active material.

### Claim 7 (depends on 1)

The anode for a lithium secondary battery according to claim 1, wherein a weight ratio between the silicon-based active material and the carbon-based active material is in a range from 5:95 to 95:5.

### Claim 8 (depends on 1)

The anode for a lithium secondary battery according to claim 1, wherein a weight ratio between the silicon-based active material and the carbon-based active material is in a range from 40:60 to 60:40.

### Claim 9 (depends on 1)

The anode for a lithium secondary battery according to claim 1, wherein the anode mixture layer is the mixture layer formed by coating and drying the anode composition including the mixture materials and an organic acid-based additive on the anode current collector, and the organic acid-based additive includes at least one selected from the group consisting of acetic acid, citric acid, oxalic acid, maleic acid, palmitic acid, tartaric acid, methacrylic acid, glutaric acid and fumaric acid.

### Claim 10 (depends on 9)

The anode for a lithium secondary battery according to claim 9, wherein a content of the organic acid-based additive is in a range from 20 wt % to 60 wt % based on the total weight of the anode composition.

### Claim 11 (depends on 1)

The anode for a lithium secondary battery according to claim 1, wherein the anode mixture layer further includes a thickener.

### Claim 12 (depends on 9)

The anode for a lithium secondary battery according to claim 9, wherein the thickener includes carboxymethyl cellulose.

### Claim 13 (depends on 1)

The anode for a lithium secondary battery according to claim 1, wherein the anode mixture layer further includes a conductive material and a binder.

### Claim 14 (depends on 1)

A lithium secondary battery, comprising:
an anode for a lithium secondary battery according to claim 1; and
a cathode facing the anode.

### Claim 15

A method for preparing an anode composition for a lithium secondary battery, comprising:
preparing a dispersion including an organic acid-based additive and a silicon-based active material and having a pH in a range from 6 to 12; and
mixing a carbon-based active material and a thickener into the dispersion.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the pH of the dispersion is in a range from 7 to 11.

### Claim 17 (depends on 15)

The method according to claim 15, wherein the dispersion is prepared to include 1 part by weight to 100 parts by weight of the organic acid additive relative to 100 parts by weight of the silicon-based active material.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the dispersion is prepared to include 30 part by weight to 70 parts by weight of the organic acid additive relative to 100 parts by weight of the silicon-based active material.

### Claim 19 (depends on 15)

The method according to claim 15, wherein mixing the carbon-based active material into the dispersion so that a weight ratio between the silicon-based active material and the carbon-based active material is in the range of 5:95 to 95:5.

### Claim 20 (depends on 15)

The method according to claim 15, wherein the anode composition is prepared to include the organic acid-based additive in a range of 20 wt % to 60 wt % based on the total weight of the anode composition.