# US 2025/0096224 A1 · Method of producing electrode, and method of producing secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0096224 A1
- Document ID: US20250096224A1
- Status: Published application
- Kind: A1
- Application number: 18/822,470
- Filed: 2024-09-03
- Published: 2025-03-20
- Earliest claimed: 2023-09-19
- Assignees: Toyota Jidosha Kabushiki Kaisha
- Applicants: Toyota Jidosha Kabushiki Kaisha
- Inventors: Tomofumi HIRUKAWA; Toru KOMATSUZAKI; Yuki MASUDA; Takeshi KONDO; Tomokuni ABE
- Web page: https://patentgrep.com/patent/US20250096224A1

## CPC

- H01M 4/043: {involving compressing or compaction}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0435: {Rolling or calendering}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/139: Processes of manufacture
- H01M 4/366: {as layered products}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An electrode production method that can suppress the thickness nonuniformity in an electrode is provided. The electrode production method includes: forming a first active material layer on a first face of a current collector; pressing the first active material layer for the first time; and pressing the first active material layer for the second time after said first pressing, wherein the proportion of a pressing linear pressure P2 in said second pressing to a pressing linear pressure P1 in said first pressing is 100% to 200%.

## Claims

### Claim 1

A method of producing an electrode, the method comprising:
forming a first active material layer on a first face of a current collector;
pressing the first active material layer for a first time; and
pressing the first active material layer for a second time after said first pressing, wherein
a proportion of a pressing linear pressure P2 in said second pressing to a pressing linear pressure P1 in said first pressing is 100% to 200%.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the proportion is 100% to 125%.

### Claim 3 (depends on 1)

The method according to claim 1, further comprising:
heating the first active material layer between said first pressing and said second pressing.

### Claim 4 (depends on 1)

The method according to claim 1, further comprising:
forming a second active material layer on a second face of the current collector between said first pressing and said second pressing.

### Claim 5 (depends on 1)

A method of producing a secondary battery, the method comprising:
preparing an electrode by the electrode production method according to claim 1; and
preparing a secondary battery by use of the electrode.