# US 2025/0096222 A1 · Secondary battery and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0096222 A1
- Document ID: US20250096222A1
- Status: Published application
- Kind: A1
- Application number: 18/945,351
- Filed: 2024-11-12
- Published: 2025-03-20
- Earliest claimed: 2024-09-27
- Assignees: Zhejiang Jinko Energy Storage Co., Ltd.
- Applicants: Zhejiang Jinko Energy Storage Co., Ltd.
- Inventors: Lili CHEN; Zixiang YANG; Hanzhang SUN
- Web page: https://patentgrep.com/patent/US20250096222A1

## CPC

- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0435: {Rolling or calendering}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/1397: of electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/366: {as layered products}
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/622: {being polymers}
- H01M 10/0587: of accumulators having only wound construction elements, i.e. wound positive electrodes, wound negative electrodes and wound separators
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Secondary battery and preparation method thereof are provided. Lithium source, iron source, phosphorus source, transition metal salt source, bismuth source, and solvent are mixed to obtain intermediate solution. PH of intermediate solution ranges from 1.0 to 4.0. Intermediate solution is subjected to hydrothermal reaction, to obtain precursor by drying. Precursor is subjected to heat treatment to obtain core. Core includes lithium iron phosphate and bismuth salt. Core is coated with coating material to obtain cathode material. Cathode material includes core and conductive polymer coating layer arranged on at least surface of core. Finally, cathode material is prepared into secondary battery. Cathode material in present disclosure has advantages of high compaction density and high conductivity, which can significantly enhance energy density, cycle performance, and high-and-low temperature performance when cathode material is applied to secondary battery.

## Claims

### Claim 1

A method for preparing a secondary battery, comprising:
mixing a lithium source, an iron source, a phosphorus source, a transition metal salt source, a bismuth source, and a solvent to obtain an intermediate solution having a pH ranging from 1.0 to 4.0;
subjecting the intermediate solution to a hydrothermal reaction to obtain a product, and drying the product to obtain a precursor;
subjecting the precursor to heat treatment to obtain a core, wherein the core comprises lithium iron phosphate and a bismuth salt;
coating the core with a coating material to obtain a cathode material, wherein the cathode material comprises the core and a conductive polymer coating layer arranged on at least a surface of the core;
coating a cathode current collector with the cathode material to obtain a cathode plate by rolling;
coating an anode current collector with an anode material to obtain an anode plate by rolling;
winding the cathode plate, the anode plate, and a separator to obtain a wound cell;
assembling the wound cell to obtain a battery module; and
injecting an electrolyte into the battery module to obtain the secondary battery.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the mixing the lithium source, the iron source, the phosphorus source, the transition metal salt source, the bismuth source, and the solvent to obtain the intermediate solution comprises:
mixing the lithium source, the phosphorus source, the iron source, and the solvent to obtain a mixed solution comprising the phosphorus source, the lithium source, and the iron source; and
adding the transition metal salt source and the bismuth source to the mixed solution, and adding an acid solution to obtain the intermediate solution.

### Claim 3 (depends on 1)

The method according to claim 1, wherein a molar ratio of the phosphorus source, the lithium source, the iron source, to the bismuth source is (1.0 to 1.15):(1.0 to 1.15): 1:(0.01 to 0.03).

### Claim 4 (depends on 1)

The method according to claim 1, wherein a molar ratio of the transition metal salt source to the bismuth source is (2.0 to 2.15):1.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the phosphorus source comprises at least one of iron phosphate, ammonium monohydrogen phosphate, ammonium dihydrogen phosphate, ammonium phosphate, or ferrous monohydrogen phosphate.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the lithium source comprises at least one of lithium carbonate, lithium phosphate, lithium hydroxide, or lithium chloride.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the iron source comprises a soluble iron salt, and
wherein the iron source further comprises at least one of ferrous sulfate, ferric nitrate, ferric chloride, ferric sulfate, or ferric oxalate.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the transition metal salt source comprises at least one of a tungsten source, a molybdenum source, or a vanadium source,
wherein the tungsten source comprises at least one of sodium tungstate, ammonium tungstate, or calcium tungstate,
wherein the molybdenum source comprises at least one of sodium molybdate or ammonium molybdate, and
wherein the vanadium source comprises at least one of ammonium metavanadate or vanadic acid.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the bismuth source comprises an other bismuth salt, the other bismuth salt comprises at least one of bismuth nitrate, bismuth oxide, or bismuth chloride.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the solvent comprises at least one of water, ethylene glycol, or anhydrous ethanol.

### Claim 11 (depends on 1)

The method according to claim 1, wherein an amount of the solvent to be added ranges from 120 ml to 200 ml.

### Claim 12 (depends on 1)

The method according to claim 1, wherein a temperature of the hydrothermal reaction ranges from 140° C. to 200° C., and/or
wherein a duration time of the hydrothermal reaction ranges from 12 h to 20 h.

### Claim 13 (depends on 1)

The method according to claim 1, wherein a temperature of the heat treatment ranges from 400° C. to 800° C., and/or
wherein a duration time of the heat treatment ranges from 3 h to 8 h.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the coating the core with the coating material comprises mixing a polymer monomer, an oxidant, and the core.

### Claim 15 (depends on 14)

The method according to claim 14,
wherein:
the polymer monomer comprises at least one of aniline, pyrrole, amide, acrylic acid, or ethylene oxide; and/or
the oxidant comprises at least one of persulfate, hydrogen peroxide, or potassium dichromate; and/or
a molar ratio of the polymer monomer to the core is (2 to 8): 1; and/or
a molar ratio of the polymer monomer to the oxidant is 1:(0.2 to 0.8).

### Claim 16 (depends on 14)

The method according to claim 14, wherein a temperature of the mixing the polymer monomer, the oxidant, and the core ranges from 0° C. to 5° C., and/or
wherein a duration time of the mixing the polymer monomer, the oxidant, and the core ranges from 4 h to 8 h.

### Claim 17 (depends on 1)

The method according to claim 1, wherein the secondary battery comprises:
the cathode plate;
the anode plate;
the separator; and
the electrolyte,
wherein the cathode plate comprises the cathode current collector and the cathode material arranged on at least one surface of the cathode current collector, and
wherein the cathode material comprises the core and a coating layer distributed on at least part of a surface of the core, at least part of the lithium iron phosphate and the bismuth salt are connected by a chemical bond, and a material of the coating layer comprises a conductive polymer.

### Claim 18 (depends on 17)

The method according to claim 17, wherein an average diameter of the lithium iron phosphate is greater than an average diameter of the bismuth salt, and
wherein the average diameter of the lithium iron phosphate ranges from 3 μm to 5 μm, and the average diameter of the bismuth salt ranges from 1 μm to 2 μm.

### Claim 19 (depends on 17)

The method according to claim 17, wherein the bismuth salt comprises at least one of bismuth tungstate, bismuth molybdate, or bismuth vanadate, and/or
wherein the conductive polymer comprises at least one of polyaniline, polypyrrole, polyamide, polyacrylic acid, or polyethylene oxide.

### Claim 20 (depends on 17)

The method according to claim 17, wherein a morphology of the lithium iron phosphate is spheroidal, and/or
wherein a morphology of the bismuth salt is at least one of a flower shape, a line shape, a nest shape, or a plate shape, and/or
wherein a molar ratio of the lithium iron phosphate to the bismuth salt is 100:(1 to 3), and/or
wherein a tap density of the cathode material ranges from 2.5 g/cm3 to 2.6 g/cm3, and/or
wherein an electrical resistivity of the cathode material ranges from 10 Ω·m to 20 Ω·m.