- Assignees: United Semiconductor (Xiamen) Co., Ltd.
- Applicants: United Semiconductor (Xiamen) Co., Ltd.
- Inventors: Jian Liu; CHEN CHEN; Chin-Chun Huang; WEN YI TAN; JINJIAN OUYANG
- Web page: https://patentgrep.com/patent/US20250095994A1

## CPC

- H10P 30/22: using masks
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention uses the thinned second pad oxide layer as the pad oxide layer for the subsequent shallow trench isolation process. Therefore, it is not necessary to remove the entire pad oxide layer on the substrate surface after the P-type high-voltage ion well thermal drive-in process. The subsequent step of re-growing the pad oxide layer is omitted, thereby simplifying the process complexity.

## Claims

### Claim 1

A method for forming a semiconductor structure, comprising:
providing a substrate having a first device region and a second device region thereon;
forming a first pad oxide layer on the substrate over the first device region and the second device region, wherein the first pad oxide layer has a first thickness;
forming a nitride hard mask layer on the first pad oxide layer over the first device region and the second device region;
removing the nitride hard mask layer from the second device region;
thermally growing a second pad oxide layer on the substrate within the second device region, wherein the second pad oxide layer has a second thickness that is greater than the first thickness;
forming an ion well in the substrate within the second device region;
thinning down the second pad oxide layer to a third thickness;
removing the nitride hard mask layer from the first device region;
forming a pad nitride layer on the first pad oxide layer and the second pad oxide layer; and
forming a trench isolation structure in the pad nitride layer, the first pad oxide layer, the second pad oxide layer, and the substrate.

### Claim 2 (depends on 1)

The method for forming a semiconductor structure according to claim 1, wherein the first thickness is 90-130 angstroms and the second thickness is 380-420 angstroms.

### Claim 3 (depends on 1)

The method for forming a semiconductor structure according to claim 1, wherein the third thickness is equal to the first thickness.

### Claim 4 (depends on 1)

The method for forming a semiconductor structure according to claim 1, wherein the first device region is a low-voltage device region and the second device region is a medium-voltage device region or a high-voltage device region.

### Claim 5 (depends on 1)

The method for forming a semiconductor structure according to claim 1, wherein the ion well is a P-type well.

### Claim 6 (depends on 1)

The method for forming a semiconductor structure according to claim 1 further comprising:
subjecting the ion well to a thermal drive in process after forming the ion well in the substrate within the second device region.

### Claim 7 (depends on 1)