# US 2025/0095991 A1 · Etching method and plasma processing apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0095991 A1
- Document ID: US20250095991A1
- Status: Published application
- Kind: A1
- Application number: 18/966,174
- Filed: 2024-12-03
- Published: 2025-03-20
- Earliest claimed: 2022-06-10
- Assignees: Tokyo Electron Limited
- Applicants: Tokyo Electron Limited
- Inventors: Koki MUKAIYAMA; Takayuki KATSUNUMA
- Web page: https://patentgrep.com/patent/US20250095991A1

## CPC

- H10P 76/4085: {characterised by the processes involved to create the masks}
- H01J 37/32449: {Gas control, e.g. control of the gas flow}
- H01J 37/32522: {Temperature}
- H01J 37/32724: {Temperature}
- H10P 50/242: {of Group IV materials}
- H10P 50/283: {by chemical means}
- H10P 50/285: {of materials not containing Si, e.g. PZT or Al2O3}
- H10P 50/73: {using masks for insulating materials}
- H01J 2237/334: Etching
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

Provided is a technique for improving a mask selectivity in etching. An etching method according to the present disclosure includes step (a) preparing a substrate including a silicon-containing film and a mask on the silicon-containing film, the mask including an opening pattern, step (b) forming a metal-containing film on the mask, and step (c) etching the silicon-containing film by generating the plasma from a first processing gas containing a hydrogen fluoride gas.

## Claims

### Claim 1

An etching method comprising:
step (a) providing a substrate including a silicon-containing film and a mask on the silicon-containing film, the mask including an opening pattern;
step (b) forming a metal-containing film on the mask; and
step (c) etching the silicon-containing film by generating plasma from a first processing gas containing a hydrogen fluoride gas.

### Claim 2 (depends on 1)

The etching method according to claim 1, wherein the silicon-containing film includes a silicon oxide film, a silicon nitride film, a polysilicon film, or a laminated film including two or more types of the silicon oxide film, the silicon nitride film and the polysilicon film.

### Claim 3 (depends on 1)

The etching method according to claim 1, wherein the mask includes a silicon-containing film different from the silicon-containing film, a carbon-containing film or a metal-containing film.

### Claim 4 (depends on 1)

The etching method according to claim 1, wherein the mask includes an amorphous carbon film or a spin-on carbon film.

### Claim 5 (depends on 1)

The etching method according to claim 1, wherein the mask includes a film including at least one type of metal selected from the group including tungsten, molybdenum, titanium, and ruthenium, or
wherein the mask includes an oxide film, a nitride film, or a carbon film including the at least one type of metal.

### Claim 6 (depends on 1)

The etching method according to claim 1, wherein step (b) includes forming the metal-containing film from a second processing gas containing a metal-containing gas.

### Claim 7 (depends on 6)

The etching method according to claim 6, wherein the metal-containing gas includes at least one type of metal selected from the group including tungsten, molybdenum, titanium, and ruthenium.

### Claim 8 (depends on 7)

The etching method according to claim 7, wherein the metal-containing gas includes tungsten hexafluoride or molybdenum hexafluoride.

### Claim 9 (depends on 6)

The etching method according to claim 6, wherein step (b) includes forming the metal-containing film by generating plasma from the second processing gas.

### Claim 10 (depends on 1)

The etching method according to claim 1, wherein step (b) includes forming the metal-containing film by causing the mask to adsorb a metal-containing precursor.

### Claim 11 (depends on 10)

The etching method according to claim 10, wherein step (b) includes forming the metal-containing film by generating plasma from a second processing gas that oxidizes or reduces at least a portion of the metal-containing precursor adsorbed by the mask.

### Claim 12 (depends on 11)

The etching method according to claim 11, wherein in step (b), a portion of the metal-containing precursor adsorbed by the mask is not oxidized or reduced.

### Claim 13 (depends on 1)

The etching method according to claim 1, wherein step (b) includes forming the metal-containing film by physical vapor deposition (PVD).

### Claim 14 (depends on 13)

The etching method according to claim 13, wherein step (a) includes disposing the substrate on a substrate support, and
step (b) includes forming the metal-containing film by sputtering a metal-containing electrode disposed to face the substrate support.

### Claim 15 (depends on 1)

The etching method according to claim 1, wherein the first processing gas further includes a phosphorus-containing gas.

### Claim 16 (depends on 15)

The etching method according to claim 15, wherein the phosphorus-containing gas includes phosphorus halide or phosphorus chloride.

### Claim 17 (depends on 1)

The etching method according to claim 1, wherein the first processing gas includes a carbon-containing gas.

### Claim 18 (depends on 1)

The etching method according to claim 1, wherein the first processing gas further includes a halogen-containing gas.

### Claim 19 (depends on 1)

The etching method according to claim 1, wherein the first processing gas includes at least one type of gas selected from the group including an oxygen-containing gas, a boron-containing gas, and a metal-containing gas.

### Claim 20 (depends on 1)

The etching method according to claim 1, wherein the first processing gas includes hydrogen fluoride, and
wherein a flow rate of the hydrogen fluoride gas is highest among gasses present in the first processing gas.

### Claim 21 (depends on 1)

The etching method according to claim 1, wherein in step (b), a temperature of the substrate support that supports the substrate is set to a first temperature, and
in step (c), the temperature of the substrate support is set to a second temperature that is lower than the first temperature.

### Claim 22 (depends on 21)

The etching method according to claim 21, wherein the first temperature is 0° C. or higher, and the second temperature is lower than 0° C.

### Claim 23 (depends on 1)

The etching method according to claim 1, wherein a cycle including step (b) and step (c) is repeated multiple times.

### Claim 24

An etching method comprising:
step (a) preparing a substrate including a silicon-containing film and a mask on the silicon-containing film, the mask including an opening pattern;
step (b) forming a metal-containing film on the mask; and
step (c) etching the silicon-containing film by generating plasma from a first processing gas.

### Claim 25 (depends on 24)

The etching method according to claim 24, wherein the first processing gas includes one or more gases that generate a hydrogen fluoride species.

### Claim 26

A plasma processing apparatus comprising:
a power source;
a chamber including an electrostatic chuck;
a temperature controller;
a gas introducer including a shower head; and
circuitry configured to:
control at least the temperature controller to prepare a substrate including a silicon-containing film and a mask on the silicon-containing film in the chamber, the mask including an opening pattern,
control at least the gas introducer to form a metal-containing film on the mask, and
control at least the power source, the gas introducer and the electrostatic chuck to etch the silicon-containing film by generating plasma from a first processing gas containing a hydrogen fluoride gas.