# US 2025/0093780 A1 · Water soluble protective coatings for engineered optical devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0093780 A1
- Document ID: US20250093780A1
- Status: Published application
- Kind: A1
- Application number: 18/885,477
- Filed: 2024-09-13
- Published: 2025-03-20
- Earliest claimed: 2023-09-14
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Amit Kumar ROY; Srobona SEN; Kankona S. ROY; Xiaopei DENG; Gopi Chandran Ramachandran; Robert VISSER
- Web page: https://patentgrep.com/patent/US20250093780A1

## CPC

- G03F 7/11: having cover layers or intermediate layers, e.g. subbing layers {(G03F7/091 - G03F7/093, B41N3/03 take precedence)}
- G03F 7/162: {Coating on a rotating support, e.g. using a whirler or a spinner}
- G03F 7/168: {Finishing the coated layer, e.g. drying, baking, soaking}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

Embodiments of the present disclosure generally relate to optical devices, and more specifically, protective coatings for optical devices and methods for preparing protective coatings on optical devices and other devices. In one or more embodiments, a method for protecting a photoresist on a workpiece is provided and includes depositing a photoresist layer on a first surface of a substrate, and depositing a protective coating on the photoresist layer disposed on the first surface, wherein the protective coating contains a water-soluble polymeric material. Thereafter, the method includes exposing a second surface of the substrate to one or more fabrication processes, where the first surface is covered by the photoresist layer and the protective coating, and the second surface is uncovered. Thereafter, the method further includes removing the protective coating by at least partially dissolving the water-soluble polymeric material with a removal solution containing water or an aqueous solution.

## Claims

### Claim 1

A method for protecting a photoresist on a workpiece, comprising:
depositing a photoresist layer on a first surface of a substrate, wherein the photoresist layer comprises a poly(methyl methacrylate) (PMMA);
depositing a protective coating on the photoresist layer disposed on the first surface, wherein the protective coating comprises a water-soluble polymeric material; then
exposing a second surface of the substrate to one or more fabrication processes, wherein the first surface is covered by the photoresist layer and the protective coating, and the second surface is uncovered; then
removing the protective coating by at least partially dissolving the water-soluble polymeric material with a removal solution comprising water, deionized water, an aqueous solution, isopropanol, methanol, ethanol, or any combination thereof.

### Claim 2 (depends on 1)

The method of claim 1, wherein the water-soluble polymeric material comprises a poly(acrylamide) (PAM), a polyvinyl pyrrolidone (PVP), a polyvinyl alcohol (PVA), a poly(acrylic acid) (PAA), a polyethylene oxide (PEO), a polyvinyl acetate (PVAc), salts thereof, derivatives thereof, or any combination thereof.

### Claim 3 (depends on 1)

The method of claim 1, wherein the water-soluble polymeric material has an average molecular weight (MW) from about 1 kDa to about 1,500 kDa.

### Claim 4 (depends on 1)

The method of claim 1, wherein the water-soluble polymeric material comprises a polyvinyl pyrrolidone (PVP).

### Claim 5 (depends on 4)

The method of claim 4, wherein the PVP has an average molecular weight (MW) from about 20 kDa to about 100 kDa.

### Claim 6 (depends on 1)

The method of claim 1, wherein the water-soluble polymeric material is deposited on the photoresist layer by a spin-coating process to produce the protective coating.

### Claim 7 (depends on 1)

The method of claim 1, wherein the workpiece comprising at least the substrate, the photoresist layer, and the protective coating is heated during a curing process to a temperature in a range from about 80° C. to about 150° C. for about 1 minute to about 30 minutes prior to removing the protective coating.

### Claim 8 (depends on 7)

The method of claim 7, wherein the temperature is in a range from about 110° C. to about 130° C. for about 5 minutes to about 15 minutes during the curing process.

### Claim 9 (depends on 1)

The method of claim 1, wherein the protective coating is removed from the photoresist layer during a removal process, the removal process comprises exposing the protective coating to sonication and the removal solution at a temperature in a range from about 20° C. to about 150° C. for about 1 minute to about 12 minutes while at least partially dissolving the water-soluble polymeric material.

### Claim 10 (depends on 1)

The method of claim 1, wherein the removal solution consists essentially of water or deionized water.

### Claim 11 (depends on 1)

The method of claim 1, wherein the one or more fabrication processes comprise exposing the second surface to a deposition process, an etch process, a cleaning process, a curing process, a thermal process, or any combination thereof.

### Claim 12

A method for protecting a photoresist on a workpiece, comprising:
depositing a photoresist layer on a substrate, wherein the photoresist layer comprises a poly(methyl methacrylate) (PMMA);
depositing a protective coating on the photoresist layer, wherein the protective coating comprises a water-soluble polymeric material comprising a polyvinyl pyrrolidone (PVP); then
exposing the workpiece to one or more fabrication processes; then
removing the protective coating by at least partially dissolving the water-soluble polymeric material with a removal solution comprising water.

### Claim 13 (depends on 12)

The method of claim 12, wherein the PVP has an average molecular weight (MW) from about 20 kDa to about 100 kDa.

### Claim 14 (depends on 12)

The method of claim 12, wherein the workpiece comprising at least the substrate, the photoresist layer, and the protective coating is heated to a temperature in a range from about 80° C. to about 150° C. for about 1 minute to about 30 minutes prior to removing the protective coating.

### Claim 15 (depends on 12)

The method of claim 12, wherein the substrate comprises at least a first surface and a second surface, wherein the protective coating is disposed on the photoresist layer which is disposed on the first surface of the substrate, and wherein the one or more fabrication processes comprise exposing the second surface to a deposition process, an etch process, a cleaning process, a curing process, a thermal process, or any combination thereof.

### Claim 16

A workpiece, comprising:
a photoresist layer disposed on a substrate, wherein the photoresist layer comprises a poly(methyl methacrylate) (PMMA); and
a protective coating disposed on the photoresist layer, wherein the protective coating comprises a water-soluble polymeric material, and wherein the water-soluble polymeric material comprises a poly(acrylamide) (PAM), a polyvinyl pyrrolidone (PVP), a polyvinyl alcohol (PVA), a poly(acrylic acid) (PAA), a polyethylene oxide (PEO), a polyvinyl acetate (PVAc), salts thereof, derivatives thereof, or any combination thereof.

### Claim 17 (depends on 16)

The workpiece of claim 16, wherein the water-soluble polymeric material has an average molecular weight (MW) from about 1 kDa to about 1,500 kDa.

### Claim 18 (depends on 16)

The workpiece of claim 16, wherein the water-soluble polymeric material comprises the polyvinyl pyrrolidone (PVP).

### Claim 19 (depends on 18)

The workpiece of claim 18, wherein the PVP has an average molecular weight (MW) from about 20 kDa to about 100 kDa.

### Claim 20 (depends on 18)

The workpiece of claim 18, wherein the photoresist layer has a thickness in a range from about 100 nm to about 800 nm and the protective coating has a thickness in a range from about 100 nm to about 1,000 nm.