# US 2025/0093776 A1 · Method for preparing pixel defining layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0093776 A1
- Document ID: US20250093776A1
- Status: Published application
- Kind: A1
- Application number: 18/891,750
- Filed: 2024-09-20
- Published: 2025-03-20
- Earliest claimed: 2023-09-20
- Assignees: Duk San Neolux Co., Ltd.
- Applicants: Duk San Neolux Co., Ltd.
- Inventors: Seo Jeong JEON; Jun Ki KIM; Kyung Soo KIM; Changmin LEE; Yeon Soo LEE; Jun BAE; Hanwook SEO; Soung Yun MUN
- Web page: https://patentgrep.com/patent/US20250093776A1

## CPC

- G03F 7/032: with binders
- G03F 7/0007: {Filters, e.g. additive colour filters; Components for display devices}
- G03F 7/027: Non-macromolecular photopolymerisable compounds having carbon-to-carbon double bonds, e.g. ethylenic compounds (G03F7/075 takes precedence)
- G03F 7/168: {Finishing the coated layer, e.g. drying, baking, soaking}
- B05D 3/0272: {with ovens}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)

## Abstract

The present disclosure is not only to ensure vivid colors but also to increase display reliability and lifespan by implementing a colored pattern with low outgas amount and moisture content on an electrode substrate; in other words, since it may cause a decrease in luminance and a decrease in lifespan due to pixel shrinkage if the amount of outgas in the panel after post-heat treatment is 15 ppm or more, or the moisture content is 50 ppm or more, the present disclosure is to minimize the generation of outgas and the moisture content in the panel state by maintaining sufficient heat and time and generating sufficient fume in the post-heat treatment step in order to minimize the outgas amount and moisture content after completing the post-heat treatment process by including a colorant according to the present disclosure.

## Claims

### Claim 1

A method for preparing a pixel defining layer, the method comprising steps of:
applying and coating a photosensitive resin composition; performing prebaking; performing exposure; performing development; and performing post-heat treatment, wherein the post-heat treatment step is performed at an oven temperature of 210° C. to 300° C. for 30 to 120 minutes, the amount of fume generated in the post-heat treatment step is 86 ppm or more, the amount of outgas generated after the post-heat treatment step is 15 ppm or less, and the content of moisture generated after the post-heat treatment step is 50 ppm or less.

### Claim 2 (depends on 1)

The method of claim 1, wherein the oven temperature of the post-heat treatment step is 210 to 300° C.

### Claim 3 (depends on 1)

The method of claim 1, wherein the post-heat treatment step is performed for 30 to 120 minutes.

### Claim 4 (depends on 1)

The method of claim 1, wherein the oven temperature of the post-heat treatment step is 250 to 270° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein the post-heat treatment step is performed for 60 to 120 minutes.

### Claim 6 (depends on 1)

The method of claim 1, wherein the photosensitive resin composition contains a colorant.

### Claim 7 (depends on 6)

The method of claim 6, wherein the colorant includes one or more of an inorganic dye, an organic dye, an inorganic pigment, and an organic pigment.

### Claim 8 (depends on 6)

The method of claim 6, wherein the colorant is contained in an amount of 1 to 40% by weight based on the total amount of the photosensitive resin composition.

### Claim 9 (depends on 6)

The method of claim 6, wherein the colorant is pretreated using: a dispersant; or a water-soluble inorganic salt and a wetting agent.

### Claim 10 (depends on 6)

The method of claim 6, wherein the colorant has an average particle diameter of 20 nm to 110 nm.

### Claim 11 (depends on 1)

The method of claim 1, wherein the photosensitive resin composition contains a patterning resin which includes an acrylic binder resin, a cardo-based binder resin, or a combination thereof.

### Claim 12 (depends on 11)

The method of claim 11, wherein the acrylic binder resin has a weight average molecular weight of 3,000 g/mol to 150,000 g/mol.

### Claim 13 (depends on 11)

The method of claim 11, wherein the cardo-based binder resin includes a repeating structure of Formula 1 below:
in Formula 1,
1) R1 and R2 are each independently hydrogen; deuterium; a halogen; a C6-C30 aryl group; a C2-C30 heterocyclic group containing at least one heteroatom of O, N, S, Si, and P; a fused ring group of a C6-C30 aliphatic ring and a C6-C30 aromatic ring; a C1-C20 alkyl group; a C2-C20 alkenyl group; a C2-C20 alkynyl group; a C1-C20 alkoxy group; a C6-C30 aryloxy group; a fluorenyl group; a carbonyl group; an ether group; or a C1-C20 alkoxycarbonyl group,
2) R1 and R2 can form a ring between neighboring groups,
3) m and n are each independently an integer of 0 to 4,
4) A1 and A2 are each independently Formula 2 or Formula 3 below,
in Formula 2 and Formula 3,
4-1) * indicates a connection part,
4-2) R3 to R6 are each independently hydrogen; deuterium; a halogen; a C6-C30 aryl group; a C2-C30 heterocyclic group containing at least one heteroatom of O, N, S, Si, and P; a fused ring group of a C6-C30 aliphatic ring and a C6-C30 aromatic ring; a C1-C20 alkyl group; a C2-C20 alkenyl group; a C2-C20 alkynyl group; a C1-C20 alkoxy group; a C6-C30 aryloxy group; a fluorenyl group; a carbonyl group; an ether group; or a C1-C20 alkoxycarbonyl group,
4-3) R3 to R6 can form a ring between neighboring groups,
4-4) Y1 and Y2 are each independently Formula 6 or Formula 7 below,
in Formula 6 and Formula 7,
4-4-1) * indicates a binding position,
4-4-2) R9 is hydrogen or methyl,
4-4-3) R10 to R13 are each independently hydrogen; deuterium; a halogen; a C6-C30 aryl group; a C2-C30 heterocyclic group containing at least one heteroatom of O, N, S, Si, and P; a fused ring group of a C6-C30 aliphatic ring and a C6-C30 aromatic ring; a C1-C20 alkyl group; a C2-C20 alkenyl group; a C2-C20 alkynyl group; a C1-C20 alkoxy group; a C6-C30 aryloxy group; a fluorenyl group; a carbonyl group; an ether group; or a C1-C20 alkoxycarbonyl group,
4-4-4) L1 to L3 are each independently a single bond; a fluorenylene group; C2-C30 alkylene; C6-C30 arylene; C2-C30 heterocycle; C1-C30 alkoxylene; C2-C30 alkyleneoxy; a C6-C30 aryloxy group; or a C2-C30 polyethyleneoxy group,
4-4-5) q and r are each independently an integer of 0 to 3, with the proviso that q+r=3, and
5) the ratio of A1 and A2 in the polymer chain of the resin including a repeating unit represented by Formula 1 is 9:1 to 1:9,
6) X1 is a single bond; O; CO; SO2; CR′R″; SiR'R″; Formula 4 below; or Formula 5 below,
6-1) R′ and R″ are each independently hydrogen; deuterium; a halogen; a C6-C30 aryl group; a C2-C30 heterocyclic group containing at least one heteroatom of O, N, S, Si, and P; a fused ring group of a C6-C30 aliphatic ring and a C6-C30 aromatic ring; a C1-C20 alkyl group; a C2-C20 alkenyl group; a C2-C20 alkynyl group; a C1-C20 alkoxy group; a C6-C30 aryloxy group;
a fluorenyl group; a carbonyl group; an ether group; or a C1-C20 alkoxycarbonyl group,
6-2) R′and R″ can form a ring between adjacent groups,
in Formula 4 and Formula 5,
6-3) * indicates a binding position,
6-4) R7 and R8 are each independently hydrogen; deuterium; a halogen; a C6-C30 aryl group; a C2-C30 heterocyclic group containing at least one heteroatom of O, N, S, Si, and P; a fused ring group of a C6-C30 aliphatic ring and a C6-C30 aromatic ring; a C1-C20 alkyl group; a C2-C20 alkenyl group; a C2-C20 alkynyl group; a C1-C20 alkoxy group; a C6-C30 aryloxy group; a fluorenyl group; a carbonyl group; an ether group; or a C1-C20 alkoxycarbonyl group,
6-5) o and p are each independently an integer of 0 to 4,
7) X2 is a C6-C30 aryl group; a C2-C30 heterocyclic group containing at least one heteroatom of O, N, S, Si, and P; a fused ring group of a C6-C30 aliphatic ring and a C6-C30 aromatic ring; a C1-C20 alkyl group; a C2-C20 alkenyl group; a C2-C20 alkynyl group; a C1-C20 alkoxy group; a C6-C30 aryloxy group; a fluorenylene group; a carbonyl group; an ether group; or a C1-C20 alkoxycarbonyl group, and
8) R′, R″, X2, L1 to L3, R1 to R8, and R10 to R13 can each be further substituted with one or more substituents selected from the group consisting of deuterium; a halogen; a silane group substituted or unsubstituted with a C1-C30 alkyl group or C6-C30 aryl group; a siloxane group; a boron group; a germanium group; a cyano group; an amino group; a nitro group; a C1-C30 alkylthio group; a C1-C30 alkoxy group; a C6-C30 arylalkoxy group; a C1-C30 alkyl group; a C2-C30 alkenyl group; a C2-C30 alkynyl group; a C6-C30 aryl group; a C6-C30 aryl group substituted with deuterium; a fluorenyl group; a C2-C30 heterocyclic group containing at least one heteroatom selected from the group consisting of O, N, S, Si, and P; a C3-C30 alicyclic group; a C7-C30 arylalkyl group; a C8-C30 arylalkenyl group; and combinations thereof, and can form a ring between adjacent substituents.

### Claim 14 (depends on 11)

The method of claim 11, wherein the cardo-based resin has a weight average molecular weight of 1,000 to 100,000 g/mol.

### Claim 15 (depends on 11)

The method of claim 11, wherein the cardo-based resin is contained in an amount of 1 to 30% by weight based on the total amount of the photosensitive resin composition.

### Claim 16 (depends on 1)

The method of claim 1, wherein the photosensitive resin composition contains a reactive unsaturated compound in an amount of 1 to 40% by weight based on the total amount of the photosensitive resin composition.

### Claim 17 (depends on 1)

The method of claim 1, wherein the photosensitive resin composition contains a photoinitiator in an amount of 0.01 to 10% by weight based on the total amount of the photosensitive resin composition.

### Claim 18 (depends on 1)

A pixel defining layer prepared by the preparation method according to claim 1.

### Claim 19 (depends on 18)

An organic light emitting display device comprising the pixel defining layer according to claim 18.

### Claim 20 (depends on 19)

An electronic device comprising the display device of claim 19 and a control unit for driving the display device.