# US 2025/0093303 A1 · Semiconductor defect inspection method and apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0093303 A1
- Document ID: US20250093303A1
- Status: Published application
- Kind: A1
- Application number: 18/887,837
- Filed: 2024-09-17
- Published: 2025-03-20
- Earliest claimed: 2023-09-18
- Assignees: Hyundai Motor Company; Kia Corporation
- Applicants: Hyundai Motor Company; Kia Corporation
- Inventors: Jung Gi Han
- Web page: https://patentgrep.com/patent/US20250093303A1

## CPC

- G01N 29/04: Analysing solids (using acoustic emission techniques G01N29/14)
- G01N 1/34: Purifying; Cleaning {(processes or apparatus for extracting or separating nucleic acids from biological samples C12N15/1003)}
- G01N 1/44: Sample treatment involving radiation, e.g. heat
- G01N 2291/0231: Composite or layered materials
- G01N 2291/0289: Internal structure, e.g. defects, grain size, texture
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

A method and an apparatus for inspecting defects in semiconductors may be incorporated in a vehicle production process. The apparatus includes an exterior inspection unit for inspecting an exterior of a semiconductor, a function inspection unit for inspecting functions of the semiconductor, a first ultrasonic inspection unit for performing a first ultrasonic inspection on the semiconductor, a pretreatment tester for performing a pretreatment on the semiconductor when the first ultrasonic inspection has been completed, a second ultrasonic inspection unit for performing a second ultrasonic inspection on the semiconductor when the pretreatment has been completed, and a cross-sectional inspection unit for inspecting a cross-section of the semiconductor when the second ultrasonic inspection shows that delamination has increased after the pretreatment.

## Claims

### Claim 1

A method of inspecting defects in a semiconductor, the method comprising
inspecting, by an exterior inspection unit, an exterior of a semiconductor,
inspecting, by a function inspection unit, functions of the semiconductor,
performing, by a first ultrasonic inspection unit, a first ultrasonic inspection on the semiconductor,
performing, by a pretreatment tester, a pretreatment on the semiconductor,
performing, by a second ultrasonic inspection unit, a second ultrasonic inspection on the semiconductor for which the pretreatment has been completed, and
inspecting, by a cross-sectional inspection unit, a cross-section of the semiconductor when the second ultrasonic inspection shows that delamination has increased after the pretreatment.

### Claim 2 (depends on 1)

The method of claim 1, wherein during the inspecting of the cross-section, the cross-section of a lead portion of the semiconductor is inspected.

### Claim 3 (depends on 2)

The method of claim 2, wherein the inspection of the cross-section of the lead portion is carried out using ion milling equipment.

### Claim 4 (depends on 3)

The method of claim 3, further comprising performing a verification of reliability of the semiconductor when it is determined that delamination has occurred on the cross-section of the lead portion after inspecting the cross-section.

### Claim 5 (depends on 3)

The method of claim 3, further comprising determining that the semiconductor is defect-proof when it is determined that delamination has occurred under a preset delamination level on the cross-section of the lead portion after inspecting the cross-section.

### Claim 6 (depends on 3)

The method of claim 3, wherein the verification of the reliability includes a temperature and cycle test.

### Claim 7 (depends on 6)

The method of claim 6, wherein the temperature and cycle test includes a heat shock test.

### Claim 8 (depends on 7)

The method of claim 7, wherein the heat shock test is performed under conditions of 1,000 cycles to 2,000 cycles and a temperature of −55° C. to 125° C.

### Claim 9 (depends on 4)

The method of claim 4, further comprising performing a third ultrasonic inspection after performing the verification of the reliability.

### Claim 10 (depends on 1)

The method of claim 1, wherein the method of inspecting defects is incorporated into a vehicle production process.

### Claim 11

An apparatus for inspecting defects in a semiconductor, the apparatus comprising:
an exterior inspection unit configured to inspect an exterior of a semiconductor,
a function inspection unit configured to inspect functions of the semiconductor,
a first ultrasonic inspection unit configured to perform a first ultrasonic inspection on the semiconductor,
a pretreatment tester configured to perform a pretreatment on the semiconductor when the first ultrasonic inspection has been completed,
a second ultrasonic inspection unit configured to perform a second ultrasonic inspection on the semiconductor when the pretreatment has been completed, and
a cross-sectional inspection unit configured to inspect a cross-section of the semiconductor when the second ultrasonic inspection shows that delamination has increased after the pretreatment.

### Claim 12 (depends on 11)

The apparatus of claim 11, wherein the cross-sectional inspection unit inspects the cross-section of a lead portion of the semiconductor.

### Claim 13 (depends on 12)

The apparatus of claim 12, wherein the inspection of the cross-section of the lead portion is carried out using ion milling equipment.

### Claim 14 (depends on 13)

The apparatus of claim 13, further comprising a reliability verification unit configured to perform a verification of reliability of the semiconductor,
wherein when the cross-sectional inspection unit determines that delamination has occurred on the cross-section of the lead portion, the verification of the reliability of the semiconductor is carried out through the reliability verification unit.

### Claim 15 (depends on 13)

The apparatus of claim 13, wherein the cross-sectional inspection unit determines that the semiconductor is defect-proof when it is determined that delamination has occurred under a preset delamination level on the cross-section of the lead portion.

### Claim 16 (depends on 13)

The apparatus of claim 13, wherein the reliability verification unit performs a temperature and cycle test.

### Claim 17 (depends on 16)

The apparatus of claim 16, wherein the temperature and cycle test includes a heat shock test.

### Claim 18 (depends on 17)

The apparatus of claim 17, wherein the heat shock test is performed under conditions of 1,000 cycles to 2,000 cycles and a temperature of −55° C. to 125° C.

### Claim 19 (depends on 14)

The apparatus of claim 14, further comprising a third ultrasonic inspection unit configured to perform a third ultrasonic inspection on the semiconductor,
wherein the third ultrasonic inspection unit performs the third ultrasonic inspection when the verification of the reliability has been completed through the reliability verification unit.

### Claim 20 (depends on 11)

A vehicle production line comprising the apparatus of claim 11.