# US 2025/0091938 A1 · Silica-free tungsten bronze glass ceramics and methods of making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0091938 A1
- Document ID: US20250091938A1
- Status: Published application
- Kind: A1
- Application number: 18/886,355
- Filed: 2024-09-16
- Published: 2025-03-20
- Earliest claimed: 2023-09-20
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Jesse Kohl
- Web page: https://patentgrep.com/patent/US20250091938A1

## CPC

- C03C 3/145: containing aluminium or beryllium
- C03C 10/0054: {containing PbO, SnO2, B2O3}
- C03C 2214/20: Glass-ceramics matrix
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A glass-ceramic that includes: 5 mol %≤Al2O3≤40 mol %; 30 mol %≤B2O3≤60 mol %; 10 mol %≤WO3≤50 mol %; 0 mol %≤SnO2≤5 mol %; and 1 mol %≤R2O≤30 mol %, wherein R2O is one or more of Li2O, Na2O, K2O, Rb2O, and Cs2O. Further, the glass-ceramic can be silica-free and, in some cases, can have a thickness from about 0.05 mm to about 0.5 mm and one or more of: (a) a total transmittance of less than or equal to 4% at ultraviolet (UV) wavelengths below 400 nm and (b) a total transmittance from about 0.5% to about 4% in the near-infrared (NIR) spectrum from 700 nm to 1500 nm.

## Claims

### Claim 1

A glass-ceramic, comprising:
5 mol %≤Al2O3≤40 mol %;
30 mol %≤B2O3≤60 mol %;
10 mol %≤WO3≤50 mol %;
0 mol %≤SnO2≤5 mol %; and
1 mol %≤R2O≤30 mol %,
wherein R2O is at least one of Li2O, Na2O, K2O, Rb2O, or Cs2O.

### Claim 2 (depends on 1)

The glass-ceramic of claim 1, wherein R2O is at least one of Li2O or Na2O.

### Claim 3 (depends on 1)

The glass-ceramic of claim 1, wherein the glass-ceramic is silica-free.

### Claim 4 (depends on 1)

The glass-ceramic of claim 1, wherein the glass-ceramic comprises a glassy phase and at least one crystalline phase, and further wherein the at least one crystalline phase comprises crystallites that range in size from 5 nm to 100 nm, as observed in transmission electron microscopy.

### Claim 5 (depends on 4)

The glass-ceramic of claim 4, wherein the at least one crystalline phase is uniformly distributed throughout a thickness of the glass-ceramic.

### Claim 6 (depends on 1)

The glass-ceramic of claim 1, wherein the glass-ceramic comprises a thickness from about 0.05 mm to about 0.5 mm and at least one of: (a) a total transmittance of less than or equal to 4% at ultraviolet wavelengths below 400 nm, or (b) a total transmittance from about 0.5% to about 4% in the near-infrared spectrum from 700 nm to 1500 nm.

### Claim 7 (depends on 6)

The glass-ceramic of claim 6, wherein the glass-ceramic further comprises a total transmittance of at least 0.5% in the visible spectrum from 400 nm to 700 nm.

### Claim 8 (depends on 1)

A solar shield comprising the glass-ceramic of claim 1.

### Claim 9

A glass-ceramic, comprising:
7 mol %≤Al2O3≤30 mol %;
35 mol %≤B2O3≤55 mol %;
15 mol %≤WO3≤40 mol %;
0 mol %≤SnO2≤2.5 mol %; and
5 mol %≤R2O≤25 mol %,
wherein R2O is at least one of Li2O, Na2O, K2O, Rb2O, or Cs2O.

### Claim 10 (depends on 9)

The glass-ceramic of claim 9, wherein R2O is at least one of Li2O or Na2O.

### Claim 11 (depends on 9)

The glass-ceramic of claim 9, wherein the glass-ceramic is silica-free.

### Claim 12 (depends on 9)

The glass-ceramic of claim 9, wherein the glass-ceramic comprises a glassy phase and at least one crystalline phase, and further wherein the at least one crystalline phase comprises crystallites that range in size from 5 nm to 100 nm, as observed in transmission electron microscopy.

### Claim 13 (depends on 12)

The glass-ceramic of claim 12, wherein the at least one crystalline phase is uniformly distributed throughout a thickness of the glass-ceramic.

### Claim 14 (depends on 9)

The glass-ceramic of claim 9, further comprising:
11.5 mol %≤Al2O3≤24.5 mol %;
44 mol %≤B2O3≤49 mol %;
20 mol %≤WO3≤25 mol %;
0 mol %≤SnO2≤0.25 mol %; and
13 mol %≤R2O≤19.5 mol %,
wherein R2O is at least one of Li2O, Na2O, K2O, Rb2O, or Cs2O.

### Claim 15 (depends on 9)

The glass-ceramic of claim 9, wherein the glass-ceramic comprises a thickness from about 0.05 mm to about 0.5 mm and at least one of: (a) a total transmittance of less than or equal to 4% at ultraviolet wavelengths below 400 nm, or (b) a total transmittance from about 0.5% to about 4% in the near-infrared spectrum from 700 nm to 1500 nm.

### Claim 16 (depends on 9)

The glass-ceramic of claim 9, wherein the glass-ceramic comprises a thickness from about 0.05 mm to about 0.5 mm and at least one of: (a) a total transmittance of less than or equal to 3.5% at ultraviolet wavelengths below 400 nm, or (b) a total transmittance from about 0.5% to about 2.5% in the near-infrared spectrum from 700 nm to 1500 nm.

### Claim 17 (depends on 9)

The glass-ceramic of claim 9, wherein the glass-ceramic comprises a thickness from about 0.05 mm to about 0.5 mm and at least one of: (a) a total transmittance of less than or equal to 3.5% at ultraviolet wavelengths below 400 nm, or (b) a total transmittance from about 0.5% to about 9% in the near-infrared spectrum from 700 nm to 2400 nm.

### Claim 18 (depends on 9)

The glass-ceramic of claim 9, wherein the glass-ceramic further comprises a total transmittance of at least 0.5% in the visible spectrum from 400 nm to 700 nm.

### Claim 19 (depends on 9)

A solar shield comprising the glass-ceramic of claim 9.

### Claim 20

A method of making a glass-ceramic, comprising:
mixing a batch comprising:
5 mol %≤Al2O3≤40 mol %;
30 mol %≤B2O3≤60 mol %;
10 mol %≤WO3≤50 mol %;
0 mol %≤SnO2≤5 mol %; and
1 mol %≤R2O≤30 mol %,
wherein R2O is at least one of Li2O, Na2O, K2O, Rb2O, or Cs2O;
melting the batch between about 1100° C. and about 1450° C. to form a melt;
annealing the melt between about 380° C. and about 500° C. to define an annealed melt; and
heat treating the annealed melt between about 500° C. and about 1000° C. from about 5 minutes to about 48 hours to form the glass-ceramic.

### Claim 21 (depends on 20)

The method of claim 20, wherein the glass-ceramic is silica-free.

### Claim 22 (depends on 20)

The method of claim 20, wherein the glass-ceramic comprises a glassy phase and at least one crystalline phase, and further wherein the at least one crystalline phase comprises crystallites that range in size from 5 nm to 100 nm, as observed in transmission electron microscopy.

### Claim 23 (depends on 20)

The method of claim 20, wherein the at least one crystalline phase is uniformly distributed throughout a thickness of the glass-ceramic.

### Claim 24 (depends on 20)

The method of claim 20, wherein the heat treating is conducted in a reducing atmosphere.

### Claim 25 (depends on 20)

The method of claim 20, wherein the glass-ceramic comprises a thickness from about 0.05 mm to about 0.5 mm and at least one of: (a) a total transmittance of less than or equal to 4% at ultraviolet wavelengths below 400 nm, or (b) a total transmittance from about 0.5% to about 4% in the near-infrared spectrum from 700 nm to 1500 nm.