# US 2025/0091297 A1 · Method for producing bonded body

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0091297 A1
- Document ID: US20250091297A1
- Status: Published application
- Kind: A1
- Application number: 18/723,979
- Filed: 2022-12-21
- Published: 2025-03-20
- Earliest claimed: 2021-12-27
- Assignees: Resonac Corporation
- Applicants: Resonac Corporation
- Inventors: Nobuyuki TAKAHASHI; Masatoshi MORI
- Web page: https://patentgrep.com/patent/US20250091297A1

## CPC

- B29C 65/4815: {Hot melt adhesives, e.g. thermoplastic adhesives}
- C09J 171/12: Polyphenylene oxides
- B29C 65/02: by heating, with or without pressure
- B29C 65/08: using ultrasonic vibrations {(non-plastics element to plastics elements B29C65/645)}
- B29C 65/10: using hot gases {(e.g. combustion gases) or flames coming in contact with at least one of the parts to be joined}
- B29C 65/14: using wave energy {, i.e. electromagnetic radiation,} or particle radiation {(using mechanical waves B29C65/06; using ultrasonic waves B29C65/08; pressing means transparent to electromagnetic radiation B29C66/81267)}
- B29C 65/1412: {Infrared [IR] radiation}
- B29C 65/1432: {direct heating of the surfaces to be joined}
- B29C 65/36: heated by induction
- B29C 65/486: {characterised by their physical form being non-liquid, e.g. in the form of granules or powders (B29C65/50 takes precedence)}
- B29C 66/1122: {Single lap to lap joints, i.e. overlap joints (B29C66/45, B29C66/472, B29C66/52272 take precedence)}
- B29C 66/45: {Joining of substantially the whole surface of the articles (methods or apparatus for laminating B32B37/00)}
- B29C 66/7392: {characterised by the material of at least one of the parts being a thermoplastic}
- B29C 66/742: {to metals or their alloys}
- B29C 66/91933: {higher than said fusion temperature}
- B32B 15/092: comprising epoxy resins
- B32B 15/20: comprising aluminium or copper {(B32B15/016 and B32B15/017 take precedence)}
- B32B 27/08: of synthetic resin
- B32B 27/285: {comprising polyethers}
- B32B 27/36: comprising polyesters
- B32B 27/38: comprising epoxy resins
- C08J 5/121: {by heating}
- C09J 5/06: involving heating of the applied adhesive
- C09J 163/00: Adhesives based on epoxy resins; Adhesives based on derivatives of epoxy resins
- B29K 2101/12: Thermoplastic materials
- B29L 2009/003: {comprising a metal layer}
- B29L 2009/005: {coated}
- B32B 2250/02: 2 layers
- C08J 2463/00: Characterised by the use of epoxy resins; Derivatives of epoxy resins
- C09J 2400/163: in the substrate
- C09J 2463/00: Presence of epoxy resin
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

Disclosed is a method for producing a joined body obtained by joining a base material A, a solid joining agent containing an amorphous thermoplastic resin, which is at least one of a thermoplastic epoxy resin and a phenoxy resin, as a main component, and a base material B in this order, in which at least the base material A is a thermoplastic resin base material, an epoxy equivalent of the amorphous thermoplastic resin is 1,600 g/eq. or more or the amorphous thermoplastic resin does not contain an epoxy group, and a heat of fusion of the amorphous thermoplastic resin is 15 J/g or less, and the method has a step of superposing and a joining step (1), or has a joining step (2-1) and a joining step (2-2).

## Claims

### Claim 1

A method for producing a joined body obtained by joining a base material A, a solid joining agent containing an amorphous thermoplastic resin, which is at least one of a thermoplastic epoxy resin and a phenoxy resin, as a main component, and a base material B in this order,
wherein
at least the base material A is a thermoplastic resin base material,
an epoxy equivalent of the amorphous thermoplastic resin is 1,600 g/eq. or more or the amorphous thermoplastic resin does not contain an epoxy group, and a heat of fusion of the amorphous thermoplastic resin is 15 J/g or less, and
wherein the method comprises:
a step of superposing the base material A, the solid joining agent, and the base material B in this order; and
a joining step (1) of joining the base material A and the base material B by pressurizing the base material A and the base material B via the solid joining agent in a state in which a temperature of the joining surface of at least one of the base material A, the solid joining agent, and the base material B is raised to the melting point thereof or higher.

### Claim 2

A method for producing a joined body obtained by joining a base material A, a solid joining agent containing an amorphous thermoplastic resin, which is at least one of a thermoplastic epoxy resin and a phenoxy resin, as a main component, and a base material B in this order,
wherein
at least the base material A is a thermoplastic resin base material,
an epoxy equivalent of the amorphous thermoplastic resin is 1,600 g/eq. or more or the amorphous thermoplastic resin does not contain an epoxy group, and a heat of fusion of the amorphous thermoplastic resin is 15 J/g or less, and
wherein the method comprises:
a joining step (2-1) of joining at least one of the base material A and the base material B to the solid joining agent in a state in which a temperature of the joining surface of at least one of the base materials and the solid joining agent is raised to the melting point thereof or higher; and
a joining step (2-2) of joining the base material A and the base material B by pressurizing the base material A and the base material B via the solid joining agent in a state in which a temperature of the joining surface of at least one of the base material A and the base material B is raised to the softening point thereof or higher.

### Claim 3 (depends on 1)

The method for producing a joined body according to claim 1, wherein in the joining step (1), the temperature of the joining surface is raised by heating with radiant heat.

### Claim 4 (depends on 2)

The method for producing a joined body according to claim 2, wherein in the joining step (2-1), the temperature of the joining surface is raised by heating with radiant heat.

### Claim 5 (depends on 2)

The method for producing a joined body according to claim 2, wherein in the joining step (2-2), the temperature of the joining surface is raised by heating with radiant heat.

### Claim 6 (depends on 1)

The method for producing a joined body according to claim 1, wherein the solid joining agent before melting has any shape selected from the group consisting of a film, a rod, a pellet, and a powder.

### Claim 7 (depends on 1)

The method for producing a joined body according to claim 1, wherein the solid joining agent before melting is a film.

### Claim 8 (depends on 1)

The method for producing a joined body according to claim 1, wherein the base material B is made of at least one of a resin and a metal.

### Claim 9 (depends on 1)

The method for producing a joined body according to claim 1, wherein the base material B is made of a metal.

### Claim 10 (depends on 8)

The method for producing a joined body according to claim 8, further comprising a step of forming a primer layer made of a solid joining agent on the joining surface of the metal.

### Claim 11 (depends on 4)

The method for producing a joined body according to claim 4, wherein in the joining step (2-2), the temperature of the joining surface is raised by heating with radiant heat.

### Claim 12 (depends on 2)

The method for producing a joined body according to claim 2, wherein the solid joining agent before melting has any shape selected from the group consisting of a film, a rod, a pellet, and a powder.

### Claim 13 (depends on 2)

The method for producing a joined body according to claim 2, wherein the solid joining agent before melting is a film.

### Claim 14 (depends on 2)

The method for producing a joined body according to claim 2, wherein the base material B is made of at least one of a resin and a metal.

### Claim 15 (depends on 2)

The method for producing a joined body according to claim 2, wherein the base material B is made of a metal.

### Claim 16 (depends on 14)

The method for producing a joined body according to claim 14, further comprising a step of forming a primer layer made of a solid joining agent on the joining surface of the metal.