# US 2025/0085624 A1 · Pellicle, exposure original plate, exposure apparatus, method for producing pellicle, and method for testing adhesive layer for mask

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0085624 A1
- Document ID: US20250085624A1
- Status: Published application
- Kind: A1
- Application number: 18/726,479
- Filed: 2023-01-26
- Published: 2025-03-13
- Earliest claimed: 2022-02-04
- Assignees: Mitsui Chemicals, Inc.
- Applicants: Mitsui Chemicals, Inc.
- Inventors: Ryo TANAKA
- Web page: https://patentgrep.com/patent/US20250085624A1

## CPC

- G03F 1/64: characterised by the frames, e.g. structure or material, including bonding means therefor
- G03F 1/48: Protective coatings
- G03F 1/62: Pellicles, e.g. pellicle assemblies, e.g. having membrane on support frame; Preparation thereof
- G03F 1/82: Auxiliary processes, e.g. cleaning or inspecting
- G03F 1/84: Inspecting
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

Provided is a pellicle, including a frame on which a pellicle film is placed and a mask adhesive layer which is placed on the frame, wherein when a water washing test is performed on the adhesive layer, which contacts a quartz mask over a predetermined contact area, a removal ratio {(the contact area before the water washing test−contact area after the water washing test)/(contact area before the water washing test)} of the adhesive layer is 80% or more.

## Claims

### Claim 1

A pellicle, comprising a frame on which a pellicle film is placed, and a mask adhesive layer placed on the frame, wherein
when a water washing test is performed on the adhesive layer, which contacts a quartz mask over a predetermined contact area A1, a removal ratio {(the contact area A1 before the water washing test−contact area A2 after the water washing test)/(the contact area A1 before the water washing test)} of the adhesive layer is 80% or more.

### Claim 2 (depends on 1)

The pellicle according to claim 1, wherein the adhesive layer contains a reaction product of a (meth)acrylic copolymer and a curing agent.

### Claim 3 (depends on 2)

The pellicle according to claim 2, wherein the curing agent is an isocyanate compound.

### Claim 4 (depends on 2)

The pellicle according to claim 2, wherein a ratio of the curing agent to the total amount of the (meth)acrylic copolymer is 0.10 to 3.00% by mass.

### Claim 5 (depends on 1)

The pellicle according to claim 1, wherein the water washing test is performed by immersing the mask in a water tank for 10 minutes and then extracting the mask from the water tank.

### Claim 6 (depends on 1)

The pellicle according to claim 1, wherein the contact area A1 before the water washing test is a residual area of the adhesive layer on the mask when an attachment portion of the adhesive layer to the mask is irradiated with VUV (Vacuum UltraViolet) light from a back side of the mask for 1 minute and the pellicle is then peeled off.

### Claim 7 (depends on 6)

The pellicle according to claim 6, wherein the contact area A1 before the water washing test is the residual area when the attachment portion is irradiated with the VUV light for 1 minute and the pellicle is then peeled off.

### Claim 8 (depends on 6)

The pellicle according to claim 6, wherein the contact area A1 before the water washing test is the residual area of the adhesive layer on the mask when the attachment portion of the adhesive layer to the mask is irradiated with VUV (Vacuum UltraViolet) light from a back surface of the mask at a cumulative radiation dose of 3.0 J/cm2 and the pellicle is then peeled off.

### Claim 9 (depends on 1)

The pellicle according to claim 1, wherein the removal ratio of the adhesive layer is 90% or more.

### Claim 10 (depends on 1)

The pellicle according to claim 1, wherein the water washing test is performed based on the following steps (A) to (D):
(A) immersing the quartz mask and the adhesive layer in contact with the quartz mask in water;
(B) rubbing the adhesive layer with a finger when the adhesive layer is in contact with the quartz mask in the water tank after 5 minutes from the start of immersion;
(C) extracting the quartz mask into the atmosphere after 10 minutes from the start of immersion; and
(D) rubbing the adhesive layer with a finger when the adhesive layer is in contact with the quartz mask in the atmosphere.

### Claim 11 (depends on 1)

An exposure master comprising the quartz mask and the pellicle according to claim 1 mounted to the mask.

### Claim 12 (depends on 11)

An exposure device, comprising:
a light source for emitting VUV (Vacuum UltraViolet) light, and
the exposure master according to claim 11, which is irradiated with the VUV light.

### Claim 13

A method for the production of a pellicle comprising a frame on which a pellicle film is placed, and a mask adhesive layer placed on the frame, wherein
when a water washing test is performed on the adhesive layer, which contacts a quartz mask over a predetermined contact area A1, a removal ratio {(the contact area A1 before the water washing test−contact area A2 after the water washing test)/(the contact area A1 before the water washing test)} of the adhesive layer is 80% or more.

### Claim 14

A test method for a mask adhesive layer of a pellicle comprising a frame on which a pellicle film is placed, and a mask adhesive layer placed on the frame, wherein
when a water washing test is performed on the adhesive layer, which contacts a quartz mask over a predetermined contact area A1, a value based on a removal ratio {(the contact area A1 before the water washing test−contact area A2 after the water washing test)/(the contact area A1 before the water washing test)} of the adhesive layer is compared with a predetermined threshold.

### Claim 15

A method for peeling a mask adhesive layer of a pellicle comprising a frame on which a pellicle film is placed, and a mask adhesive layer which is placed on the frame, from a quartz mask, the method comprising:
a step of irradiating an attachment portion of the adhesive layer to the mask with VUV (Vacuum Ultra Violet) light, and thereafter, a step of washing with water.

### Claim 16 (depends on 15)

The method for peeling a mask adhesive layer according to claim 15, wherein in the VUV light irradiation step, the attachment portion of the adhesive layer to the mask is irradiated with the VUV light from a back surface of the mask for 1 minute, and the pellicle is then peeled off.

### Claim 17 (depends on 15)

The method for peeling a mask adhesive layer according to claim 15, wherein in the VUV light irradiation step:
the attachment portion of the adhesive layer to the mask is irradiated with the VUV light from a back surface of the mask at a cumulative radiation dose of 3.0 J/cm2 and the pellicle is then peeled off.