# US 2025/0085622 A1 · Extreme Ultraviolet (EUV) Mask and Method of Fabrication Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0085622 A1
- Document ID: US20250085622A1
- Status: Published application
- Kind: A1
- Application number: 18/415,986
- Filed: 2024-01-18
- Published: 2025-03-13
- Earliest claimed: 2023-09-08
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Chun-Lang CHEN; Chung-Yang HUANG; Shih-Hao YANG; Chien-Yun HUANG; Wei-Ting CHEN
- Web page: https://patentgrep.com/patent/US20250085622A1

## CPC

- G03F 1/24: Reflection masks; Preparation thereof
- G03F 1/80: Etching
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

EUV masks and methods of fabrication thereof are described herein. An exemplary method includes receiving an EUV mask having a multilayer structure, a capping layer disposed over the multilayer structure, a patterned absorber layer disposed over the capping layer, and a patterned hard mask disposed over the patterned absorber layer. The method further includes removing the patterned hard mask by performing a first etching process to partially remove the patterned hard mask and performing a second etching process to remove a remainder of the patterned hard mask. The first etching process uses a first etchant, and the second etching process uses a second etchant. The second etchant is different than the first etchant. In some embodiments, the first etchant is a halogen-based plasma (e.g., a Cl2 plasma), and the second etchant is a halogen-and-oxygen-based plasma (e.g., a Cl2+O2 plasma).

## Claims

### Claim 1

A method comprising:
receiving an EUV mask having a multilayer structure, a capping layer disposed over the multilayer structure, a patterned absorber layer disposed over the capping layer, and a patterned hard mask disposed over the patterned absorber layer; and
removing the patterned hard mask by:
performing a first etching process to partially remove the patterned hard mask, wherein the first etching process uses a first etchant, and
performing a second etching process to remove a remainder of the patterned hard mask, wherein the second etching process uses a second etchant that is different than the first etchant.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first etchant is a halogen-based plasma, and the second etchant is a halogen-and-oxygen-based plasma.

### Claim 3 (depends on 2)

The method of claim 2, wherein the halogen-based plasma is a Cl2 plasma, and the halogen-and-oxygen-based plasma is a Cl2+O2 plasma.

### Claim 4 (depends on 1)

The method of claim 1, further comprising performing the second etching process after the first etching process has reduced the patterned hard mask from a first thickness to a second thickness, wherein the second thickness is about 30% to about 50% of the first thickness.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first etching process removes the patterned hard mask at a first etch rate, the second etching process removes the patterned hard mask at a second etch rate, and the second etch rate is greater than the first etch rate.

### Claim 6 (depends on 1)

The method of claim 1, wherein the patterned absorber layer exposes a portion of the capping layer, and the method further includes tuning parameters of the first etching process and the second etching process to control oxygen diffusion into the exposed portion of the capping layer, wherein an atomic ratio of oxygen in the exposed portion of the capping layer is limited to less than about 10%.

### Claim 7 (depends on 1)

The method of claim 1, wherein an oxide layer is formed on the patterned absorber layer after the second etching process.

### Claim 8 (depends on 7)

The method of claim 7, wherein the patterned absorber layer exposes a portion of the capping layer, and the method further includes tuning parameters of the second etching process to prevent formation of the oxide layer on the exposed portion of the capping layer.

### Claim 9 (depends on 7)

The method of claim 7, wherein:
the oxide layer has a first portion disposed on a top of the patterned absorber layer and a second portion disposed on sidewalls of the patterned absorber layer;
the first portion of the oxide layer has a first thickness, the second portion of the oxide layer has a second thickness, and the second portion of the oxide layer has a tip having a third thickness that is less than the second thickness; and
the method further includes tuning parameters of the first etching process and the second etching process to limit the third thickness of the tip to less than 5% of the first thickness.

### Claim 10 (depends on 9)

The method of claim 9, wherein:
the tip physically contacts a bottom corner of the patterned absorber layer; and
the third thickness is a minimum thickness of the oxide layer.

### Claim 11

A method for fabricating an extreme ultraviolet (EUV) mask comprising:
forming a capping layer over a multilayer structure;
forming an absorber layer over the capping layer;
forming a patterning layer over the absorber layer;
selectively etching the absorber layer with respect to the capping layer using the patterning layer as an etch mask; and
selectively etching the patterning layer with respect to the capping layer and the absorber layer, wherein the selectively etching of the patterning layer includes a first etch step that uses a non-oxygen etchant to partially remove the patterning layer and a second etch step that uses an oxygen etchant to remove a remainder of the patterning layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein:
the non-oxygen etchant is a chlorine-containing plasma; and
the oxygen etchant is an oxygen-containing plasma.

### Claim 13 (depends on 11)

The method of claim 11, wherein:
the patterning layer formed over the absorber layer has a first thickness; and
the selectively etching of the patterning layer includes switching from the first etch step to the second etch step when a thickness of the patterning layer is reduced by the first etch step from the first thickness to a second thickness, wherein the second thickness is equal to a predetermined percentage of the first thickness of the patterning layer.

### Claim 14 (depends on 13)

The method of claim 13, wherein the predetermined percentage of the first thickness is less than or equal to 50%.

### Claim 15 (depends on 11)

The method of claim 11, further comprising:
tuning parameters of the first etch step and the second etch step to control oxygen diffusion into the capping layer, wherein the parameters of the first etch step and the second etch step are tuned to limit an atomic ratio of oxygen in the capping layer to less than about 10%.

### Claim 16 (depends on 11)

The method of claim 11, further comprising:
tuning parameters of the first etch step and the second etch step to control forming of an oxide layer over the absorber layer, wherein the oxide layer has a first portion disposed over a top of the absorber layer and a second portion disposed over sidewalls of the absorber layer; and
wherein the parameters of the first etch step and the second etch step are tuned to limit a first thickness of a tip of the second portion of the oxide layer disposed on the capping layer to less than 5% of a second thickness of the first portion of the oxide layer.

### Claim 17

An extreme ultraviolet (EUV) mask comprising:
a multilayer structure;
a capping layer disposed over the multilayer structure;
a patterned absorber layer disposed over the capping layer, wherein the patterned absorber layer has an opening therein that exposes a portion of the capping layer; and
an oxide layer disposed over the patterned absorber layer, wherein the oxide layer is disposed along sidewalls of the patterned absorber layer that form the opening therein and the exposed portion of the capping layer is free of the oxide layer.

### Claim 18 (depends on 17)

The EUV mask of claim 17, wherein:
an oxygen region is along a top of the exposed portion of the capping layer; and
an atomic ratio of oxygen in the oxygen region is less than about 10%.

### Claim 19 (depends on 17)

The EUV mask of claim 17, wherein the oxide layer disposed along the sidewalls of the patterned absorber layer extends to the capping layer and a first thickness of a first portion of the oxide layer that physically contacts the capping layer is less than 5% of a second thickness of a second portion of the oxide layer that is disposed on a top of the patterned absorber layer.

### Claim 20 (depends on 17)

The EUV mask of claim 17, wherein the oxide layer disposed along the sidewalls of the patterned absorber layer does not physically contact the capping layer.