# US 2025/0085365 A1 · Magnetoresistive element having thermally robust performances after high-field exposure and sensor comprising the magnetoresistive element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0085365 A1
- Document ID: US20250085365A1
- Status: Published application
- Kind: A1
- Application number: 18/727,425
- Filed: 2023-02-22
- Published: 2025-03-13
- Earliest claimed: 2022-02-22
- Assignees: Allegro MicroSystems, LLC
- Applicants: Allegro MicroSystems, LLC
- Inventors: Salim DOUNIA; Léa CUCHET; Nikita STRELKOV; Clarisse DUCRUET; Andrey TIMOPHEEV; Jeffrey CHILDRESS
- Web page: https://patentgrep.com/patent/US20250085365A1

## CPC

- G01R 33/098: {comprising tunnel junctions, e.g. tunnel magnetoresistance sensors}
- G01R 33/0052: {Manufacturing aspects; Manufacturing of single devices, i.e. of semiconductor magnetic sensor chips (devices based on galvano-magnetic effect or the like H10N50/85)}
- H01F 10/3254: {the spacer being semiconducting or insulating, e.g. for spin tunnel junction [STJ]}
- H01F 10/3268: {the exchange coupling being asymmetric, e.g. by use of additional pinning, by using antiferromagnetic or ferromagnetic coupling interface, i.e. so-called spin-valve [SV] structure, e.g. NiFe/Cu/NiFe/FeMn}
- H10N 50/01: Manufacture or treatment
- H10N 50/10: Magnetoresistive devices
- H10N 50/85: Materials of the active region
- G01R: MEASURING ELECTRIC VARIABLES; MEASURING MAGNETIC VARIABLES (indicating correct tuning of resonant circuits H03J3/12)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

Magnetoresistive element comprising a reference layer having a fixed reference magnetization; a ferromagnetic sense layer having a free sense magnetization having a stable vortex configuration that is orientable relative to the fixed reference magnetization in the presence of an external magnetic field; and a tunnel barrier layer between the reference layer and the sense layer and contacting a first side of the sense layer. The magnetoresistive element further comprises a hard magnetic layer arranged on a second side (212) of the sense layer opposed to the first side, the hard magnetic layer being configured to generate an interfacial magnetic coupling between the hard magnetic layer and the sense layer on the second side, such as to prevent chirality switching of the sense magnetization after the magnetoresistive element has been submitted to a heat treatment and an external magnetic field above vortex expulsion field.

## Claims

### Claim 1

Magnetoresistive element, comprising a reference layer having a fixed reference magnetization (230); a ferromagnetic sense layer having a free sense magnetization having a stable vortex configuration that is orientable relative to the fixed reference magnetization in the presence of an external magnetic field; and a tunnel barrier layer between the reference layer and the sense layer and contacting a first side of the sense layer;
the magnetoresistive element further comprises a hard magnetic layer arranged on a second side of the sense layer opposed to the first side, the hard magnetic layer being configured to generate an interfacial magnetic coupling between the hard magnetic layer and the sense layer on the second side, such as to prevent chirality switching of the sense magnetization after the magnetoresistive element has been submitted to a heat treatment and an external magnetic field above vortex expulsion field.

### Claim 2 (depends on 1)

The magnetoresistive element according to claim 1,
wherein the hard magnetic layer comprises a material having a magnetic coercivity greater than 1000 A/m.

### Claim 3 (depends on 2)

The magnetoresistive element according to claim 2,
wherein the material comprises any one, alone or in combination, of: CoCrPt, FePt—TiO2, FePt—SiO2, FePt—C, CoPt, NdFeB, or SmCo.

### Claim 4 (depends on 2)

The magnetoresistive element according to claim 2,
wherein the high magnetic coercivity material comprises any one of: a perpendicular ferrimagnetic alloy comprising a rare earth and a transition metal; a perpendicular ordered alloy, multilayers of 3d-4d metals having perpendicular magnetic anisotropy, a permanent magnet based on one or a plurality of rare earth metals.

### Claim 5 (depends on 3)

The magnetoresistive element according to claim 3,
wherein the high magnetic coercivity material further comprises Cr, C, Cu, V, or an oxide.

### Claim 6 (depends on 1)

The magnetoresistive element according to claim 1,
wherein the hard magnetic layer comprises an antiferromagnetic material.

### Claim 7 (depends on 6)

The magnetoresistive element according to claim 6,
wherein the antiferromagnetic material comprises any one, alone or in combination, of: IrMn, FeMn, PtMn, PdMn, CrPdMn, NiMn, CuMnAs, Mn3Sn, Mn2Au, or Cr2O.

### Claim 8 (depends on 1)

The magnetoresistive element according to claim 1,
wherein the thickness of the hard magnetic layer is between 2 nm and to 30 nm.

### Claim 9 (depends on 1)

The magnetoresistive element according to claim 1,
further comprising a mediating layer between the sense layer and the hard magnetic layer, the strength of the interfacial magnetic coupling being adjustable by adjusting the thickness of the mediating layer.

### Claim 10 (depends on 9)

The magnetoresistive element according to claim 9,
wherein the mediating layer comprises a transition metal, particularly Ru, W, Ir, or Ta.

### Claim 11 (depends on 9)

The magnetoresistive element according to claim 9,
wherein the thickness of the mediating layer is configured such that the strength of the interfacial magnetic coupling has a value between −1 mJ/m2 and +1 mJ/m2.

### Claim 12 (depends on 11)

The magnetoresistive element according to claim 11,
further comprising a ferromagnetic coupling layer between the mediating layer (26) and the hard magnetic layer;
the strength of the interfacial magnetic coupling being further adjustable by adjusting the thickness of the coupling layer.

### Claim 13 (depends on 1)

The magnetoresistive element according to claim 1,
wherein the magnetically soft material of the sense layer comprises a combination of Ni, Fe, Co and transition metals.

### Claim 14 (depends on 13)

The magnetoresistive element according to claim 13,
wherein the sense layer has a thickness greater than 15 nm.

### Claim 15 (depends on 1)

The magnetoresistive element according to claim 1,
wherein the sense layer has a net exchange bias that is lower 40 A/m in any direction in the plane (P) of the sense layer.

### Claim 16

A magnetic sensor comprising a plurality of the magnetoresistive element.

### Claim 17

Method for manufacturing the magnetoresistive element can thus comprises the steps of:
forming the reference layer, the tunnel barrier layer, the sense layer, and the hard magnetic layer;
measuring the net exchange bias of the magnetoresistive elements; and
heating the magnetoresistive element to a heating temperature between 150° C. and 400° C. until the measured net exchange bias of the magnetoresistive elements is below 40 A/m.

### Claim 18 (depends on 17)

Method according to claim 17,
wherein heating the magnetoresistive elements is performed during a heating time that is between 1 s and 24 h.

### Claim 19 (depends on 17)

Method according to claim 17,
wherein said measuring the net exchange bias is performed by using a magnetometry technique.