# US 2025/0084565 A1 · Thermally insulating aerogel composite fiber

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0084565 A1
- Document ID: US20250084565A1
- Status: Published application
- Kind: A1
- Application number: 18/580,267
- Filed: 2023-04-27
- Published: 2025-03-13
- Earliest claimed: 2023-04-27
- Assignees: Textime Manufacturing Limited
- Applicants: Textime Manufacturing Limited
- Inventors: SAU PING WONG
- Web page: https://patentgrep.com/patent/US20250084565A1

## CPC

- D01F 1/10: Other agents for modifying properties
- D01D 1/02: Preparation of spinning solutions
- D01D 5/08: Melt spinning methods {(D01D5/0023 takes precedence)}
- D01D 5/088: Cooling filaments, threads or the like, leaving the spinnerettes
- D01D 5/247: Discontinuous hollow structure or microporous structure
- D01F 1/08: for forming hollow filaments
- D01F 6/60: from polyamides (from polyamino acids or polypeptides D01F6/68)
- D01F 6/605: {from aromatic polyamides}
- D01F 6/62: from polyesters
- D01F 6/74: from polycondensates of cyclic compounds, e.g. polyimides, polybenzimidazoles
- D01F 6/92: of polyesters
- D04H 3/009: Condensation or reaction polymers
- D10B 2401/10: porous
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- D04H: MAKING TEXTILE FABRICS, e.g. FROM FIBRES OR FILAMENTARY MATERIAL (weaving D03; knitting D04B; braiding D04C; net-making D04G; sewing D05B; tufting D05C; finishing non-woven fabrics D06); FABRICS MADE BY SUCH PROCESSES OR APPARATUS, e.g. FELTS, NON-WOVEN FABRICS; COTTON-WOOL; WADDING {; NON-WOVEN FABRICS FROM STAPLE FIBRES, FILAMENTS OR YARNS, BONDED WITH AT LEAST ONE WEB-LIKE MATERIAL DURING THEIR CONSOLIDATION}(non-woven fabrics having an intermediate or external layer of a different kind, e.g. of woven fabric, B32B)
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES

## Abstract

The present application provides a preparation method of an all-polymer aerogel composite fiber by compounding fiber material(s) with polymer-based micro-aerogel powder using a melting process, comprising of the following steps: (a) Weighing the materials to form the aerogel composite fibers, which should compose of 0.1-20% (w/w) polymer micro-aerogel powder and 80-99.9% (w/w) fiber material(s); (a) Mixing the polymer micro-aerogel powder and fiber material(s) to form a homogenized composite mixture; and (b) Heating the composite mixture up to the melting point of the fiber material(s) to disperse the polymer micro-aerogels throughout the molten fiber material(s), then extruded to form aerogel composite fibers.

## Claims

### Claim 1

A preparation method of an aerogel composite fiber, comprising of the following steps:
(a) Weighing the materials to form the aerogel composite fibers, which should compose of 0.1-20% (w/w) polymer micro-aerogel powder and 80-99.9% (w/w) fiber material(s);
(a) Mixing the polymer micro-aerogel powder and fiber material(s) to form a homogenized composite mixture; and
(b) Heating the composite mixture up to the melting point of the fiber material(s) to disperse the polymer micro-aerogels throughout the molten fiber material(s), then extruded to form aerogel composite fibers.

### Claim 2 (depends on 1)

The preparation method of an aerogel composite fiber according to claim 1, wherein the polymer micro-aerogel powder has an average particle size of 0.1-100 μm, a porous structure with an average pore size of 10-2000 nm, and a thermal conductivity of 20-100 mW/mK.

### Claim 3 (depends on 1)

The preparation method of an aerogel composite fiber according to claim 1, wherein the polymer micro-aerogel powder is prepared by dissolving 0.1-30% (w/w) of polymer in a suitable solvent at 40-80° C., then adding 0-30% (v/v) of a suitable non-solvent before the mixture is frozen, gelled in a non-solvent bath, ball-milled into microgels, washed, and lastly freeze-dried with tert-butanol.

### Claim 4 (depends on 3)

The preparation method of an aerogel composite fiber according to claim 3, wherein the polymer is a polyimide or an aramid.

### Claim 5 (depends on 3)

The preparation method of an aerogel composite fiber according to claim 3, wherein the solvent is a chemical that can dissolve 0-30% (w/w) of the polymer material and can accept up to 0-30% of non-solvent without the polymer material precipitating.

### Claim 6 (depends on 3)

The preparation method of an aerogel composite fiber according to claim 3, wherein the non-solvent is a chemical that causes the polymer material to precipitate when added in excess.

### Claim 7 (depends on 3)

The preparation method of an aerogel composite fiber according to claim 3, wherein the gelation occurs inside a refrigerator, freezer, or liquid nitrogen.

### Claim 8 (depends on 3)

The preparation method of an aerogel composite fiber according to claim 3, wherein the gels are ball-milled into microgels for 0.1-48 hours.

### Claim 9 (depends on 3)

The preparation method of an aerogel composite fiber according to claim 3, wherein the washing and freeze drying uses a suitable solvent that can be frozen and sublimated at a pressure below 600 Pa.

### Claim 10 (depends on 1)

The preparation method of an aerogel composite fiber according to claim 1, wherein the fiber material(s) are polyethylene terephthalate, polylactic acid, and/or nylon.

### Claim 11 (depends on 1)

The preparation method of an aerogel composite fiber according to claim 1, wherein the composite mixture is molten and formed into a fiber with melt spinning or melt extrusion.

### Claim 12 (depends on 1)

The preparation method of an aerogel composite fiber according to claim 1, wherein the fiber diameter is 10-200 μm.

### Claim 13 (depends on 1)

The preparation method of an aerogel composite fiber according to claim 1, wherein the fiber shows a 1-50% reduction in thermal conductivity and a change of ±30% in fiber tenacity strength when compared to fibers produced with only the fiber material.

### Claim 14 (depends on 1)

An textile product, comprising the aerogel composite fibers manufactured by the preparation methodin claim 1.