# US 2025/0084562 A1 · Porous silicon structure manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0084562 A1
- Document ID: US20250084562A1
- Status: Published application
- Kind: A1
- Application number: 18/765,914
- Filed: 2024-07-08
- Published: 2025-03-13
- Earliest claimed: 2023-09-13
- Assignees: Taiwan-Asia Semiconductor Corporation
- Applicants: Taiwan-Asia Semiconductor Corporation
- Inventors: Hou-Jun Wu
- Web page: https://patentgrep.com/patent/US20250084562A1

## CPC

- C30B 33/10: in solutions or melts
- C25F 3/12: of semiconducting materials
- C30B 29/06: Silicon
- H10P 50/00: Etching of wafers, substrates or parts of devices
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C25F: PROCESSES FOR THE ELECTROLYTIC REMOVAL OF MATERIALS FROM OBJECTS; APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A porous silicon structure manufacturing method is provided. The porous silicon structure manufacturing method involves forming an epitaxial layer on a substrate and forming a protective layer on the epitaxial layer. The protective layer includes an opening region. An electrochemical etching is performed within the opening region to create a porous silicon structure on the epitaxial layer. After removing the protective layer, a wafer with a porous silicon structure is obtained.

## Claims

### Claim 1

A porous silicon structure manufacturing method, comprising:
forming an epitaxial layer on a substrate;
forming a protective layer on the epitaxial layer, wherein the protective layer includes an opening region;
performing an electrochemical etching within the opening region to create a porous silicon structure on the epitaxial layer; and
removing the protective layer.

### Claim 2 (depends on 1)

The porous silicon structure manufacturing method of claim 1, wherein when the electrochemical etching is performed, an etching rate of the epitaxial layer is greater than or equal to 10 times an etching rate of the substrate.

### Claim 3 (depends on 1)

The porous silicon structure manufacturing method of claim 1, wherein a resistance value of the epitaxial layer is greater than or equal to 10 times a resistance value of the substrate.

### Claim 4 (depends on 1)

The porous silicon structure manufacturing method of claim 1, wherein a thickness of the epitaxial layer ranges from 20 micrometers (μm) to 80 micrometers (μm).

### Claim 5 (depends on 1)

The porous silicon structure manufacturing method of claim 1, wherein the substrate is a silicon substrate.

### Claim 6 (depends on 1)

The porous silicon structure manufacturing method of claim 1, wherein the epitaxial layer is a P-type doped epitaxial layer.

### Claim 7 (depends on 1)

The porous silicon structure manufacturing method of claim 1, wherein a thickness of the protection layer ranges from 200 nanometers (nm) to 500 nanometers (nm).

### Claim 8 (depends on 1)

The porous silicon structure manufacturing method of claim 1, wherein the electrochemical etching is conducted to perform an anodic etching to the epitaxial layer by using an etching solution made of hydrofluoric acid (HF) and ethanol (C2H5OH).

### Claim 9 (depends on 1)

The porous silicon structure manufacturing method of claim 1, wherein the epitaxial layer includes a porous silicon region and a non-porous silicon region, and a thickness of the porous silicon region is the same as a thickness of the epitaxial layer.