# US 2025/0084560 A1 · Holder and vapor phase growth apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0084560 A1
- Document ID: US20250084560A1
- Status: Published application
- Kind: A1
- Application number: 18/958,833
- Filed: 2024-11-25
- Published: 2025-03-13
- Earliest claimed: 2022-05-30
- Assignees: NuFlare Technology, Inc.
- Applicants: NuFlare Technology, Inc.
- Inventors: Toru WATANABE; Yoshiaki DAIGO; Masayoshi YAJIMA
- Web page: https://patentgrep.com/patent/US20250084560A1

## CPC

- C23C 16/4581: {characterised by material of construction or surface finish of the means for supporting the substrate}
- C30B 25/12: Substrate holders or susceptors
- C23C 16/4583: {the substrate being supported substantially horizontally}
- H10P 14/29: {characterised by the substrates}
- H10P 72/70: for supporting or gripping
- C30B 29/36: Carbides
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A holder according to an embodiment includes a portion containing non-oriented polycrystalline 3C-SiC on its surface. A substrate can be placed on the holder. In the non-oriented polycrystalline 3C-SiC, when a diffraction peak intensity of a (111) face of the 3C-SiC obtained by Out-of-Plane XRD measurement is 100, the diffraction peak intensity of a (400) face of the 3C-SiC is greater than 0, the diffraction peak intensity of a (331) face of the 3C-SiC is greater than 0, the diffraction peak intensity of a (420) face of the 3C-SiC is greater than 0, and the diffraction peak intensity of a (422) face of the 3C-SiC is greater than 0.

## Claims

### Claim 1

A holder, comprising:
a portion containing non-oriented polycrystalline 3C-SiC on its surface,
wherein a substrate can be placed on the holder, and
in the non-oriented polycrystalline 3C-SiC, when a diffraction peak intensity of a (111) face of the 3C-SiC obtained by Out-of-Plane XRD measurement is 100, the diffraction peak intensity of a (400) face of the 3C-SiC is greater than 0, the diffraction peak intensity of a (331) face of the 3C-SiC is greater than 0, the diffraction peak intensity of a (420) face of the 3C-SiC is greater than 0, and the diffraction peak intensity of a (422) face of the 3C-SiC is greater than 0.

### Claim 2 (depends on 1)

The holder according to claim 1,
wherein, in the non-oriented polycrystalline 3C-SiC, when a diffraction peak intensity of a (111) face of the 3C-SiC obtained by the Out-of-Plane XRD measurement is 100, the diffraction peak intensity of a (200) face of the 3C-SiC is 10 or more and 40 or less, the diffraction peak intensity of a (220) face of the 3C-SiC is 25 or more and 50 or less, and the diffraction peak intensity of a (311) face of the 3C-SiC is 15 or more and 65 or less.

### Claim 3 (depends on 1)

The holder according to claim 1,
wherein the diffraction peak intensity of a (400) face of the 3C-SiC is 20 or less, the diffraction peak intensity of a (331) face of the 3C-SiC is 20 or less, the diffraction peak intensity of a (420) face of the 3C-SiC is 20 or less, and the diffraction peak intensity of a (422) face of the 3C-SiC is 20 or less.

### Claim 4 (depends on 1)

The holder according to claim 1, further comprising:
an inner region; and
an outer region with an annular shape surrounding the inner region and surrounding the substrate when the substrate is placed,
wherein the portion is provided in the outer region.

### Claim 5 (depends on 1)

The holder according to claim 1, further comprising:
a base member; and
an annular member placed on an outer periphery of the base member,
wherein the annular member includes the portion.

### Claim 6 (depends on 5)

The holder according to claim 5,
wherein the annular member includes a first member and a second member separable from the first member, and
at least one of the first member and the second member includes the portion.

### Claim 7 (depends on 6)

The holder according to claim 6,
wherein the first member has an annular shape,
the second member has an annular shape, and
the second member surrounds the first member.

### Claim 8 (depends on 7)

The holder according to claim 7,
wherein the first member includes the portion, and the second member does not include the portion.

### Claim 9 (depends on 1)

A vapor phase growth apparatus, comprising:
the holder according to claim 1.