# US 2025/0084557 A1 · Growth of strontium tetraborate crystals

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0084557 A1
- Document ID: US20250084557A1
- Status: Published application
- Kind: A1
- Application number: 18/752,650
- Filed: 2024-06-24
- Published: 2025-03-13
- Earliest claimed: 2023-09-11
- Applicants: Kla Corporation
- Inventors: Yung-Ho Alex CHUANG; John FIELDEN; Kelly MAUSER; Edgardo GARCIA BERRIOS
- Web page: https://patentgrep.com/patent/US20250084557A1

## CPC

- C30B 9/12: Salt solvents, e.g. flux growth
- C30B 9/06: using as solvent a component of the crystal composition
- C30B 29/22: Complex oxides
- G02F 1/3548: {Quasi phase matching [QPM], e.g. using a periodic domain inverted structure}
- G02F 1/3551: {Crystals}
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS

## Abstract

A method for growing a strontium tetraborate (SrB4O7) crystal is provided. The method includes lowering a seed crystal into a melt having a mixture comprising a source of Sr, B, O, and Cl. The method also includes heating and melting the mixture to a temperature sufficient to form a strontium tetraborate crystal.

## Claims

### Claim 1

A method for growing a strontium tetraborate (SrB4O7) crystal comprising:
lowering a seed crystal into a melt, wherein the melt comprises:
forming a mixture comprising a source of Sr, B, O, and Cl; and
heating and melting the mixture to a temperature sufficient to form a strontium tetraborate crystal.

### Claim 2 (depends on 1)

The method for growing a SrB4O7 crystal according to claim 1, wherein the mixture of Sr, B, O, and Cl is heated and melted to a temperature of approximately 960-1030° C., and then cooled to a temperature of approximately 950° C. to form the strontium tetraborate crystal.

### Claim 3 (depends on 1)

The method for growing a SrB4O7 crystal according to claim 1, wherein a source of the Cl is SrCl2.

### Claim 4 (depends on 1)

The method for growing a SrB4O7 crystal according to claim 1, wherein a source of Sr, B, O, and Cl comprises at least one of B2O3, SrCO3, and SrCl2.

### Claim 5 (depends on 3)

The method for growing a SrB4O7 crystal according to claim 3, wherein the melt comprises approximately between 0.5-34 mol % SrCl2.

### Claim 6 (depends on 4)

The method for growing a SrB4O7 crystal according to claim 4, wherein the melt comprises approximately between 0.5-34 mol % SrCO3.

### Claim 7 (depends on 4)

The method for growing a SrB4O7 crystal according to claim 4, wherein the melt comprises approximately between 66-90 mol % B2O3.

### Claim 8 (depends on 3)

The method for growing a SrB4O7 crystal according to claim 3, wherein the melt comprises approximately between 2-15 mol % SrCl2.

### Claim 9 (depends on 1)

The method for growing a SrB4O7 crystal according to claim 1, wherein the mixture additionally comprises a source of H2O.

### Claim 10 (depends on 1)

The method for growing a SrB4O7 crystal according to claim 1, further comprising growing the strontium tetraborate crystal by a top-seeded solution method.

### Claim 11 (depends on 1)

The method for growing a SrB4O7 crystal according to claim 1, further comprising growing the strontium tetraborate crystal by a flux method.

### Claim 12 (depends on 1)

The method for growing a SrB4O7 crystal according to claim 1, further comprising growing the strontium tetraborate crystal by a melt method.

### Claim 13 (depends on 1)

The method for growing a SrB4O7 crystal according to claim 1, which comprises a seed crystal of alternating crystal plates to enable quasi-phase matching.

### Claim 14

(canceled)

### Claim 15

(canceled)

### Claim 16 (depends on 1)

The method for growing a SrB4O7 crystal according to claim 1, wherein the mixture of Sr, B, O, and Cl is heated and melted to a temperature of approximately 960-1030° C., and then cooled to a temperature of approximately 900° C. to form the strontium tetraborate crystal.

### Claim 17 (depends on 1)

The method for growing a SrB4O7 crystal according to claim 1, wherein the mixture of Sr, B, O, and Cl is heated and melted to a temperature of approximately 960-1030° C., and then cooled to a temperature of approximately 875° C. to form the strontium tetraborate crystal.

### Claim 18 (depends on 1)

The method for growing a SrB4O7 crystal according to claim 1, wherein the mixture of Sr, B, O, and Cl is heated and melted to a temperature of approximately 1001-1030° C., and then cooled to a temperature of approximately 1000° C. to form the strontium tetraborate crystal.

### Claim 19 (depends on 1)

The method for growing a SrB4O7 crystal according to claim 1, wherein the mixture of Sr, B, O, and Cl is heated and melted to a temperature of approximately 1016-1030° C., and then cooled to a temperature of approximately 1015° C. to form the strontium tetraborate crystal.

### Claim 20 (depends on 1)

The method for growing a SrB4O7 crystal according to claim 1, wherein the mixture of Sr, B, O, and Cl is heated and melted to a temperature of approximately 960-1030° C., and then cooled to a temperature of approximately between 875-1015° C. to form the strontium tetraborate crystal.

### Claim 21 (depends on 1)

A frequency converting apparatus which contains a crystal grown in the method of claim 1.

### Claim 22 (depends on 1)

A linear optical apparatus which contains a crystal grown in the method of claim 1.