# US 2025/0084544 A1 · Solid oxide cell and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0084544 A1
- Document ID: US20250084544A1
- Status: Published application
- Kind: A1
- Application number: 18/287,815
- Filed: 2023-09-25
- Published: 2025-03-13
- Earliest claimed: 2022-12-06
- Assignees: Samsung Electro-Mechanics Co., Ltd.
- Applicants: Samsung Electro-Mechanics Co., Ltd.
- Inventors: Jungdeok Park; Jaeseok Yi; Hongryul Lee; Jaehyuk Jang
- Web page: https://patentgrep.com/patent/US20250084544A1

## CPC

- C25B 1/042: by electrolysis of steam
- C25B 11/031: Porous electrodes
- C25B 9/19: with diaphragms
- C25B 9/23: comprising ion-exchange membranes in or on which electrode material is embedded
- C25B 9/77: having diaphragms
- C25B 11/02: characterised by shape or form
- C25B 13/02: characterised by shape or form
- C25B 13/07: based on ceramics
- H01M 4/861: {with a gradient in the porosity}
- H01M 4/8621: {containing only metallic or ceramic material, e.g. made by sintering or sputtering}
- H01M 4/8626: {characterised by the form}
- H01M 4/8657: {layered}
- H01M 4/8885: {Sintering or firing}
- H01M 8/124: characterised by the process of manufacturing or by the material of the electrolyte
- H01M 8/2404: Processes or apparatus for grouping fuel cells
- H01M 8/2432: Grouping of unit cells of planar configuration
- H01M 2008/1293: {Fuel cells with solid oxide electrolytes}
- Y02E 60/50: Fuel cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- C25B: ELECTROLYTIC OR ELECTROPHORETIC PROCESSES FOR THE PRODUCTION OF COMPOUNDS OR NON-METALS; APPARATUS THEREFOR (anodic or cathodic protection C23F13/00; single-crystal growth C30B)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A solid oxide cell according to an embodiment includes: a fuel electrode and an air electrode that face each other; and an electrolyte electrode that is disposed between the fuel electrode and the air electrode. The fuel electrode has a plate shape, an edge of the fuel electrode is rounded along a thickness direction of the fuel electrode, the fuel electrode includes a central layer and an outer layer disposed on both sides of the central layer, and a first porosity, which is a porosity of the central layer of the fuel electrode, is smaller than a second porosity, which is a porosity of the outer layer of the fuel electrode.

## Claims

### Claim 1

A solid oxide cell comprising:
a fuel electrode and an air electrode that face each other; and
an electrolyte electrode that is disposed between the fuel electrode and the air electrode,
wherein the fuel electrode has a plate shape,
an edge of the fuel electrode is rounded along a thickness direction of the fuel electrode,
the fuel electrode includes a central layer and an outer layer disposed on both sides of the central layer, and
a first porosity, which is a porosity of the central layer of the fuel electrode, is smaller than a second porosity, which is a porosity of the outer layer of the fuel electrode.

### Claim 2 (depends on 1)

The solid oxide cell of claim 1, wherein:
a first corner, which is a corner connecting edges of the fuel electrode, is rounded along the thickness direction of the fuel electrode.

### Claim 3 (depends on 2)

The solid oxide cell of claim 2, wherein:
the first corner is rounded on a plane crossing the thickness direction of the fuel electrode.

### Claim 4 (depends on 3)

The solid oxide cell of claim 3, wherein:
the edge of the fuel electrode has a curvature radius which is a range of ¼ to 1 of the thickness of the fuel electrode.

### Claim 5 (depends on 3)

The solid oxide cell of claim 3, wherein:
a second corner, a corner of the electrolyte electrode, and a third corner, a corner of the air electrode, are rounded on a plane crossing the thickness direction of the fuel electrode.

### Claim 6 (depends on 5)

The solid oxide cell of claim 5, wherein:
a curvature radius of each of the first corner, the second corner, and the third corner on a plane crossing the thickness direction of the fuel electrode is a range of 0.1 mm to 2 mm.

### Claim 7 (depends on 1)

The solid oxide cell of claim 1, wherein:
the fuel electrode further comprises a middle layer disposed between the central layer and the outer layer and having a third porosity, and the third porosity is greater than the first porosity and less than the second porosity.

### Claim 8 (depends on 7)

The solid oxide cell of claim 7, wherein:
a length of the middle layer is longer than a length of the outer layer and shorter than a length of the central layer.

### Claim 9

A manufacturing method of a solid oxide cell, comprising:
preparing a plurality of fuel electrode members of plate shape including a central member and an outer member disposed on both sides of the central member;
stacking and compressing the plurality of fuel electrode members;
stacking an electrolyte member on the fuel electrode member;
sintering the plurality of fuel electrode members and the electrolyte member to form the fuel electrode and electrolyte electrode to round an edge of the fuel electrode along a thickness direction of the fuel electrode and to have a first porosity, which is a porosity of a central layer formed of the central member, being smaller than a second porosity, which is a porosity of the outer layer formed of the outer member; and
forming an air electrode on the electrolyte electrode.

### Claim 10 (depends on 9)

The manufacturing method of the solid oxide cell of claim 9, wherein:
by sintering the plurality of fuel electrode members,
the outer member shrinks more than the central member such that a length of the outer layer formed by sintering the outer member is shorter than a length of the central layer formed by sintering the central member.

### Claim 11 (depends on 10)

The manufacturing method of the solid oxide cell of claim 10, wherein:
the preparing the plurality of fuel electrode members comprises forming a first corner, which is a corner of the plurality of fuel electrode members, to be round on a plane crossing the thickness direction of the fuel electrode.

### Claim 12 (depends on 11)

The manufacturing method of the solid oxide cell of claim 11, wherein:
the stacking the electrolyte member comprises
forming a second corner, which is a corner of the electrolyte member, to be round on a plane crossing the thickness direction of the fuel electrode.

### Claim 13 (depends on 12)

The manufacturing method of the solid oxide cell of claim 12, wherein:
the forming the air electrode comprises
forming a third corner, which is a corner of the air electrode, to be round on a plane crossing the thickness direction of the fuel electrode.

### Claim 14

A solid oxide cell comprising:
a fuel electrode and an air electrode that face each other; and
an electrolyte electrode that is disposed between the fuel electrode and the air electrode,
wherein the fuel electrode has a plate shape, and
a central portion of the fuel electrode is longer than a portion of the fuel electrode which is closer to the electrolyte electrode than the central portion.

### Claim 15 (depends on 14)

The solid oxide cell of claim 14, wherein:
a first corner, which is a corner connecting edges of the fuel electrode, is rounded along a thickness direction of the fuel electrode.

### Claim 16 (depends on 15)

The solid oxide cell of claim 15, wherein:
wherein a curvature radius of the fuel electrode is a range of 0.1 mm to 2 mm.

### Claim 17 (depends on 15)

The solid oxide cell of claim 15, wherein:
a second corner, a corner of the electrolyte electrode, and a third corner,
a corner of the air electrode, are rounded on a plane crossing the thickness direction of the fuel electrode.

### Claim 18 (depends on 14)

The solid oxide cell of claim 14, wherein:
a length of the fuel electrode decreases in a direction from the central portion of the fuel electrode to the portion of the fuel electrode which is closer to the electrolyte electrode than the central portion.

### Claim 19 (depends on 14)

The solid oxide cell of claim 14, wherein:
a porosity of the fuel electrode increases in a direction from the central portion of the fuel electrode to the portion of the fuel electrode which is closer to the electrolyte electrode than the central portion.

### Claim 20 (depends on 14)

The solid oxide cell of claim 14, wherein:
a length of the electrolyte electrode is greater than a length of the air electrode and less than a length of the fuel electrode.