# US 2025/0084516 A1 · Steel reinforcement and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0084516 A1
- Document ID: US20250084516A1
- Status: Published application
- Kind: A1
- Application number: 18/958,505
- Filed: 2024-11-25
- Published: 2025-03-13
- Earliest claimed: 2021-11-08
- Assignees: Hyundai Steel Company; Korea University Research and Business Foundation; Korea Institute of Science and Technology
- Applicants: Hyundai Steel Company; Korea University Research and Business Foundation; Korea Institute of Science and Technology
- Inventors: Jun Ho Chung; Tae Hyung Kim
- Web page: https://patentgrep.com/patent/US20250084516A1

## CPC

- C22C 38/32: with boron
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0263: {following hot rolling}
- C21D 8/06: during manufacturing of rods or wires
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/20: with copper
- C22C 38/24: with vanadium
- C22C 38/26: with niobium or tantalum
- C22C 38/28: with titanium or zirconium
- C22C 38/40: with nickel
- C22C 38/42: with copper
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/58: with more than 1.5% by weight of manganese
- C21D 2211/001: Austenite
- C21D 2211/002: Bainite
- C21D 2211/005: Ferrite
- C21D 2211/009: Pearlite
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

Provided is a steel reinforcement including an amount of 0.07 to 0.43 wt % of carbon (C), an amount of 0.5 to 2.0 wt % of manganese (Mn), an amount of 0.05 to 0.5 wt % of silicon (Si), an amount greater than 0 and less than or equal to 0.5 wt % of chromium (Cr), an amount greater than 0 and less than or equal to 4.5 wt % of copper (Cu), an amount greater than 0 and less than or equal to 0.003 wt % of boron (B), an amount greater than 0 and less than or equal to 0.25 wt % of vanadium (V), an amount greater than 0 and less than or equal to 0.012 wt % of nitrogen (N), an amount greater than 0 and less than or equal to 0.03 wt % of phosphorus (P), an amount greater than 0 and less than or equal to 0.03 wt % of sulfur(S), an amount of 0.01 to 0.5 wt % of the sum of one or more of nickel (Ni), niobium (Nb) and titanium (Ti), the balance of iron (Fe), and other inevitable impurities. A final microstructure includes ferrite, bainite, pearlite, retained austenite, and precipitates comprising copper.

## Claims

### Claim at position 1

-3. (canceled)

### Claim 4

A method for manufacturing a steel reinforcement, the method comprising:
(a) reheating a steel at a temperature of 1,050 to 1,230° C., wherein the steel comprises an amount of 0.07 to 0.43 wt % of carbon (C), an amount of 0.5 to 2.0 wt % of manganese (Mn), an amount of 0.05 to 0.5 wt % of silicon (Si), an amount greater than 0 and less than or equal to 0.5 wt % of chromium (Cr), an amount greater than 0 and less than or equal to 4.5 wt % of copper (Cu), an amount greater than 0 and less than or equal to 0.003 wt % of boron (B), an amount greater than 0 and less than or equal to 0.25 wt % of vanadium (V), an amount greater than 0 and less than or equal to 0.012 wt % of nitrogen (N), an amount greater than 0 and less than or equal to 0.03 wt % of phosphorus (P), an amount greater than 0 and less than or equal to 0.03 wt % of sulfur(S), an amount of 0.01 to 0.5 wt % of the sum of one or more of nickel (Ni), niobium (Nb) and titanium (Ti), the balance of iron (Fe), and other inevitable impurities;
(b) hot rolling the reheated steel under a condition of a finish rolling temperature of 950 to 1,020° C.; and
(c) performing an aging heat treatment on the hot-rolled steel at a temperature of 400 to 600° C. for 15 to 60 minutes.

### Claim 5 (depends on 4)

The method of claim 4, wherein the final microstructure after performing step (c) includes ferrite, bainite, pearlite, retained austenite, and precipitates comprising copper.

### Claim 6 (depends on 5)

The method of claim 5, wherein the final microstructure has a bainite fraction of 90% or more and a retained austenite fraction of 5% or less.

### Claim 7 (depends on 4)

The method of claim 4, wherein the steel reinforcement after performing the step (c) has a yield strength (YS) of 750 MPa or greater, a tensile strength (TS) of 1,000 MPa or greater, an elongation of 11% or greater, and a ratio of a tensile strength to a yield strength (TS/YS) of 1.25 or greater.