# US 2025/0084511 A1 · Enhanced magnetic performance of manganese aluminum alloy via titanium addition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0084511 A1
- Document ID: US20250084511A1
- Status: Published application
- Kind: A1
- Application number: 18/883,022
- Filed: 2024-09-12
- Published: 2025-03-13
- Earliest claimed: 2023-09-12
- Applicants: The Trustees of Dartmouth College
- Inventors: Thomas Keller; Dylan Barbagallo; Geoffroy Hautier; Ian Baker; Tushar Kanti Ghosh; Natalya Sheremetyeva
- Web page: https://patentgrep.com/patent/US20250084511A1

## CPC

- C22C 22/00: Alloys based on manganese
- H01F 1/047: Alloys characterised by their composition
- C22C 2202/02: Magnetic
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

A Mn—Al—Ti permanent magnet includes a body composed of an alloy consisting essentially of manganese in an amount of 50 to 56 atomic percent, aluminum in an amount of 44 to 50 atomic percent, and titanium in an amount of 0.5 to 1.5 atomic percent with a total amount of manganese, aluminum, and titanium not exceeding 100 atomic percent. In one preferred embodiment, a composition for the Mn—Al—Ti permanent magnet is Mn54Al45Ti1 with substantially no other elemental additions being present. The addition of titanium in amounts of approximately 1 atomic percent to the Mn—Al system is believed to result in the titanium sitting on the anti-phase boundary (APB) sites with atoms coupling ferromagnetically across the APB in the presence of titanium, resulting in suppression of the negative effects of the APB and improving the remanence over a titanium-less Mn—Al permanent magnet. This system also exhibits sustained coercivity at high temperatures.

## Claims

### Claim 1

A Mn—Al—Ti permanent magnet comprising:
a body composed of an alloy consisting essentially of manganese in an amount of 50 to 56 atomic percent of the alloy, aluminum in an amount of 44 to 50 atomic percent of the alloy, and titanium in an amount of 0.5 to 1.5 atomic percent of the alloy with a total amount of manganese, aluminum and titanium not exceeding 100 atomic percent.

### Claim 2 (depends on 1)

The Mn—Al—Ti permanent magnet of claim 1, wherein the alloy is a ternary alloy consisting of manganese in an amount of 50 to 56 atomic percent, aluminum in an amount of 44 to 50 atomic percent, and titanium in an amount of 0.5 to 1.5 atomic percent.

### Claim 3 (depends on 1)

The Mn—Al—Ti permanent magnet of claim 1, wherein, in the alloy, the amount of manganese is between 53 and 55 atomic percent of the alloy, the amount of aluminum is between 44 and 46 atomic percent of the alloy, and the amount of titanium is between 0.5 to 1.5 atomic percent of the alloy.

### Claim 4 (depends on 1)

The Mn—Al—Ti permanent magnet of claim 1, wherein in the alloy the amount of manganese is 54 atomic percent of the alloy, the amount of aluminum is 45 atomic percent of the alloy, and the amount of titanium is 1 atomic percent of the alloy with substantially no other elements present in the alloy.

### Claim 5 (depends on 4)

The Mn—Al—Ti permanent magnet of claim 4, wherein the Mn—Al—Ti permanent magnet consisting essentially of manganese, aluminum, and titanium has a (BH)max exceeding 33% of a titanium-less Mn—Al permanent magnet having 54 atomic percent manganese and 46 atomic percent aluminum.

### Claim 6 (depends on 1)

The Mn—Al—Ti permanent magnet of claim 1, wherein in the alloy the amount of manganese is 53 atomic percent of the alloy, the amount of aluminum is 46 atomic percent of the alloy, and the amount of titanium is 1 atomic percent of the alloy with substantially no other elements present in the alloy.

### Claim 7 (depends on 1)

The Mn—Al—Ti permanent magnet of claim 1, wherein the amount of titanium is between 0.75 to 1.25 atomic percent of the alloy.

### Claim 8 (depends on 1)

The Mn—Al—Ti permanent magnet of claim 1, wherein the titanium preferentially sits on anti-phase boundaries (APBs) of the microstructure, resulting in ferromagnetic coupling across the APBs, thereby suppressing negative effects usually associated with APBs in a titanium-less Mn—Al permanent magnet and improving remanence of the Mn—Al—Ti permanent magnet.

### Claim 9 (depends on 1)

The Mn—Al—Ti permanent magnet of claim 1, wherein the titanium stabilizes a coercivity of the Mn—Al—Ti permanent magnet at elevated temperatures in excess of 550° C. in comparison to a titanium-less Mn—Al permanent magnet with Mn to Al ratios to that of the Mn—Al—Ti permanent magnet.

### Claim 10 (depends on 1)

The Mn—Al—Ti permanent magnet of claim 1, wherein the addition of titanium relative to a titanium-less Mn—Al permanent magnet with Mn to Al ratios to that of the Mn—Al—Ti permanent magnet stabilizes the τ/ε phase to allow processing of the Mn—Al—Ti permanent magnet at elevated temperatures and stabilizing coercivity.

### Claim 11 (depends on 1)

The Mn—Al—Ti permanent magnet of claim 1, wherein, regardless of direction of measurement, Mr, Hci, and (BH)max are greater in the Mn—Al—Ti permanent magnet in comparison to a titanium-less Mn—Al permanent magnet with Mn to Al ratios of the Mn—Al—Ti permanent magnet.

### Claim 12 (depends on 1)

The Mn—Al—Ti permanent magnet of claim 1, wherein, in comparison to a titanium-less Mn—Al permanent magnet with Mn to Al ratios of the Mn—Al—Ti permanent magnet, the Mn—Al—Ti permanent magnet has a decreased density of anti-phase boundaries and an increased anti-phase boundary domain size resulting in less antiferromagnetic coupling and fewer magnetic domain reversal sites.

### Claim 13

A method of making a Mn—Al—Ti permanent magnet comprising:
forming an alloy consisting essentially of manganese in an amount of 50 to 56 atomic percent of the alloy, aluminum in an amount of 44 to 50 atomic percent of the alloy, and titanium in an amount of 0.5 to 1.5 atomic percent of the alloy with a total amount of manganese, aluminum and titanium not exceeding 100 atomic percent into a body of a Mn—Al—Ti permanent magnet.

### Claim 14 (depends on 13)

The method of making the Mn—Al—Ti permanent magnet of claim 13, wherein the step of forming the alloy into the body of a Mn—Al—Ti permanent magnet occurs as part of a casting operation in which the manganese, aluminum, and titanium are melted and then cast.

### Claim 15 (depends on 13)

The method of making the Mn—Al—Ti permanent magnet of claim 13, wherein the step of forming the alloy into the body of a Mn—Al—Ti permanent magnet comprises sintering powder metal containing the manganese, aluminum, and titanium.