# US 2025/0084509 A1 · A 6xxx alloy for high strength extruded products with high processability

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0084509 A1
- Document ID: US20250084509A1
- Status: Published application
- Kind: A1
- Application number: 18/561,758
- Filed: 2022-05-24
- Published: 2025-03-13
- Earliest claimed: 2021-05-25
- Assignees: Constellium Singen GmbH; Constellium Extrusion Levice S.R.O.
- Applicants: CONSTELLIUM SINGEN GmbH; Constellium Extrusion Levice S.R.O.
- Inventors: Mehdi BEN TAHAR; Roland TIRARD-COLLET; Martin JARRETT
- Web page: https://patentgrep.com/patent/US20250084509A1

## CPC

- C22C 21/02: with silicon as the next major constituent
- B21C 23/002: {Extruding materials of special alloys so far as the composition of the alloy requires or permits special extruding methods of sequences}
- B21C 23/142: {Making profiles}
- C22C 21/04: Modified aluminium-silicon alloys
- C22C 21/08: with silicon
- C22C 21/14: with silicon
- C22C 21/16: with magnesium
- C22F 1/002: {by rapid cooling or quenching; cooling agents used therefor}
- C22F 1/043: of alloys with silicon as the next major constituent
- C22F 1/047: of alloys with magnesium as the next major constituent
- C22F 1/057: of alloys with copper as the next major constituent
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B21C: MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES, PROFILES OR LIKE SEMI-MANUFACTURED PRODUCTS OTHERWISE THAN BY ROLLING; AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

The invention concerns an improved alloy to obtain AA6xxx alloy extrusions with high strength, typically having an ultimate tensile strength higher than 390 MPa, and high processability, in particular with a high productivity, as well as high surface quality and high corrosion resistance. In particular, the alloy of the invention contains, in wt. %, Si 0.6-0.9, Mg 0.55-0.76, Cu 0.65-0.9, Mn 0.4-0.7, Cr 0.05-0.2, Zr 0.10-0.19, Fe 0.05-0.5, Zn≤1.0, V≤0.10, Ti≤0.10, other elements <0.05 each and <0.15 total, rest aluminium. The extruded profiles of the invention are advantageously used as automotive components such as crash boxes, a bumpers, a side impact beams or side sills.

## Claims

### Claim 1

An extruded profile comprising an Al—Mg—Si alloy containing, in wt. %,
Si 0.6-0.9,
Mg 0.55-0.76,
Cu 0.65-0.9,
Mn 0.4-0.7,
Cr 0.05-0.2,
Zr 0.10-0.19,
Fe 0.05-0.5,
Zn≤1.0,
V≤0.10,
Ti≤0.10,
other elements <0.05 each and <0.15 total, rest aluminium.

### Claim 2 (depends on 1)

An extruded profile according to claim 1 wherein the Cu content is from 0.75 to 0.85 wt. %.

### Claim 3 (depends on 1)

An extruded profile according to claim 1 wherein the microstructure is essentially unrecrystallized.

### Claim 4 (depends on 4)

An extruded profile according to claim 4 wherein peripheral coarse grain is at most 400 μm thick per wall side.

### Claim 5 (depends on 1)

An extruded profile according to claim 1 wherein solidus temperature of the alloy is from 580° C. to 610° C., optionally from 585° C. to 600° C. and more optionally from 588° C. to 595° C. and even more optionally from 589° C. to 594 C.

### Claim 6 (depends on 1)

An extruded profile according to claim 1 wherein the flow stress measured at 480° C. and a strain rate of 0.14 s−1 is at most 35 MPa and optionally at most 32 MPa.

### Claim 7 (depends on 1)

An extruded profile according to claim 1 wherein the extruded profile is in a T6 temper and has an ultimate tensile strength in a longitudinal direction of at least 390 MPa and optionally of at least 400 MPa.

### Claim 8 (depends on 1)

A method to make an extruded profile according to claim 1 comprising successively steps of
(a) Casting a billet containing, in wt. %,
Si 0.6-0.9,
Mg 0.55-0.76,
Cu 0.65-0.9,
Mn 0.4-0.7,
Cr 0.05-0.2,
Zr 0.10-0.19,
Fe 0.05-0.5,
Zn≤1.0,
V≤0.10,
Ti≤0.10,
other elements <0.05 each and <0.15 total, rest aluminium
(b) Homogenizing the billet,
(c) Cooling the homogenized billet to room temperature,
(d) Solution heat treating the homogenized billet at a temperature from 500° C. to 560° C. for a duration from 150 s to 500 s and quenching to a temperature from 300° C. to 500° C. or reheating the homogenized billet directly and without solutionising to a temperature from 300° C. to 500° C.,
(e) Extruding at an extrusion rate from 5 m/mn to 15 m/mn said heat treated and quenched or reheated billet to obtain an extruded profile,
(f) Quenching, stretching and aging said extruded profile.

### Claim 9 (depends on 8)

The method to make an extruded profile according to claim 8 wherein homogenization temperature is from 530° C. to 580° C. and wherein extrusion rate is at least 7 m/mn.

### Claim 10 (depends on 1)

A product comprising an extruded profile according to claim 1 as an automotive component optionally a crash box, a bumper, a side impact beam or a side sill.