- Number: US 2025/0084310 A1
- Document ID: US20250084310A1
- Status: Published application
- Kind: A1
- Application number: 18/458,348
- Filed: 2023-08-30
- Published: 2025-03-13
- Earliest claimed: 2023-08-30
- Assignees: King Fahd University of Petroleum and Minerals
- Applicants: King Fahd University of Petroleum and Minerals
- Inventors: Mohammad Abu Jafar MAZUMDER; Shaikh Asrof ALI; Lipiar Khan Mohammad Osman GONI
- Web page: https://patentgrep.com/patent/US20250084310A1

## CPC

- C09K 15/30: containing heterocyclic ring with at least one nitrogen atom as ring member
- C08F 126/04: Diallylamine
- C09D 5/08: Anti-corrosive paints
- C09D 139/02: Homopolymers or copolymers of vinylamine
- C23F 11/04: in markedly acid liquids
- C08F 2810/00: Chemical modification of a polymer
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25

## Abstract

A corrosion inhibitor composition is provided. The corrosion inhibitor composition includes a polycationic polymeric surfactant. The polycationic polymeric surfactant is a copolymer including polymerized units of cationic heterocyclic monomer units and dicationic heterocyclic comonomer units including a quaternary ammonium group. The cationic heterocyclic monomer units and the dicationic heterocyclic comonomer units are alkyl diallyl ammonium units. The quaternary ammonium group comprises a first C8-C16 alkyl group, a second C4-C8 alkyl group, a third C1-C2 alkyl group, and a fourth C1-C2 alkyl group. A method of corrosion inhibition is also provided.

## Claims

### Claim at position 1

1: A corrosion inhibitor composition, comprising:
a polycationic polymeric surfactant,
wherein the polycationic polymeric surfactant is a copolymer comprising polymerized units of cationic heterocyclic monomer units and dicationic heterocyclic comonomer units comprising a quaternary ammonium group,
wherein the cationic heterocyclic monomer and the dicationic heterocyclic comonomer are alkyl diallyl ammonium units;
wherein the quaternary ammonium group comprises a first C8-C16 alkyl group, a second C4-C8 alkyl group, a third C1-C2 alkyl group, and a fourth C1-C2 alkyl group.

### Claim at position 2 (depends on 1)

2: The corrosion inhibitor of claim 1, wherein the cationic heterocyclic monomer and the dicationic heterocyclic comonomer units are present in the polymer in a molar ratio in a range of 0.85:0.15 to 0.95:0.05.

### Claim at position 3 (depends on 1)

3: The corrosion inhibitor of claim 1, wherein the quaternary ammonium group is a dodecyl-dimethyl-hexyl ammonium chloride.

### Claim at position 4 (depends on 1)

4: The corrosion inhibitor of claim 1, wherein the polycationic polymeric surfactant has a repeating structure:
wherein R1 is a methyl group,
wherein R2 is a hydrogen atom or the quaternary ammonium group, and
wherein X is a chloride atom.

### Claim at position 5 (depends on 1)

5: A method of corrosion inhibition, comprising:
contacting a metal substrate with the corrosion inhibitor of claim 1,
wherein the corrosion inhibitor is in the form of a solution comprising the polycationic polymeric surfactant in an amount of 1 to 60 parts per million (ppm) and an acidic aqueous electrolyte to form a corrosion inhibitor coated metal substrate.

### Claim at position 6 (depends on 5)

6: The method of claim 5, wherein the polycationic polymeric surfactant is in an amount of 5 to 60 ppm and wherein the corrosion inhibitor coated metal substrate has an inhibition efficiency of 65 to 80% based on weight loss of the metal substrate.

### Claim at position 7 (depends on 5)

7: The method of claim 5, wherein the polycationic polymeric surfactant is in an amount of 5 to 60 ppm and wherein the corrosion inhibitor coated metal substrate has a corrosion rate of 4 to 6 mm yr−1 compared to a corrosion rate of 17 to 19 mm yr−1 of the metal substrate in the absence of the corrosion inhibitor.

### Claim at position 8 (depends on 5)

8: The method of claim 5, wherein the polycationic polymeric surfactant adsorbs on a surface of the metal substrate via chemisorption.

### Claim at position 9 (depends on 5)

9: The method of claim 5, wherein the polycation polymeric surfactant is in an amount of 40 to 60 ppm and wherein the corrosion inhibitor coated metal substrate has a corrosion current density of 350 to 450 microamperes per square centimeter (μA cm−2) compared to a corrosion current density of 2600 to 2800 A cm−2 of the metal substrate in the absence of the corrosion inhibitor.

### Claim at position 10 (depends on 5)

10: The method of claim 5, wherein the polycation polymeric surfactant is in an amount of 40 to 60 ppm and wherein the corrosion inhibitor coated metal substrate has an elemental composition of iron in the amount of 85 to 88% by weight, oxygen in the amount of 5 to 7% by weight, carbon in the amount of 4 to 6% by weight, chlorine in the amount of 1 to 3% by weight, and manganese 0.5 to 1.5% by weight based on a total weight of the corrosion inhibitor coated metal substrate.

### Claim at position 11 (depends on 5)

11: The method of claim 5, wherein the polycation polymeric surfactant is in an amount of 40 to 60 ppm and wherein the corrosion inhibitor coated metal substrate has an average surface roughness of 5 to 5.5 micrometers (μm).

### Claim at position 12 (depends on 5)

12: The method of claim 5, further comprising:
adding potassium iodide to the solution.

### Claim at position 13 (depends on 12)

13: The method of claim 12, wherein the polycationic polymeric surfactant is in an amount of 40 to 60 ppm, wherein a concentration of potassium iodide is 4 to 6 millimolar (mM), and wherein the corrosion inhibitor coated metal substrate has an inhibition efficiency of 92 to 97% based on weight loss of the metal substrate.

### Claim at position 14 (depends on 12)

14: The method of claim 12, wherein the polycationic polymeric surfactant is in an amount of 40 to 60 ppm, wherein a concentration of potassium iodide is 4 to 6 mM, and wherein the corrosion inhibitor coated metal substrate has a corrosion rate of 0.5 mm yr−1 to 1 mm yr−1 compared to a corrosion rate of 17 to 19 mm yr−1 of the metal substrate in the absence of the corrosion inhibitor and potassium iodide.

### Claim at position 15 (depends on 12)

15: The method of claim 12, wherein the polycationic polymeric surfactant adsorbs on a surface of the metal substrate using physisorption.

### Claim at position 16 (depends on 12)

16: The method of claim 12, wherein the polycation polymeric surfactant is in an amount of 40 to 60 ppm, wherein a concentration of potassium iodide is 4 to 6 mM, and wherein the corrosion inhibitor coated metal substrate has a corrosion current density of 15 to 25 μA cm−2 compared to a corrosion current density of 2600 to 2800 μA cm−2 of the metal substrate in the absence of the corrosion inhibitor and potassium iodide.

### Claim at position 17 (depends on 12)

17: The method of claim 12, wherein the polycation polymeric surfactant is in an amount of 40 to 60 ppm, wherein a concentration of potassium iodide is 4 to 6 mM, and wherein the corrosion inhibitor coated metal substrate has an elemental composition of iron in the amount of 88 to 91% by weight, oxygen in the amount of 1 to 3% by weight, carbon in the amount of 5 to 7% by weight, chlorine in the amount of 0.01 to 0.5% by weight, manganese 0.5 to 1.5% by weight, and nitrogen in the amount of 0.5 to 2% by weight based on a total weight of the corrosion inhibitor coated metal substrate.

### Claim at position 18 (depends on 12)

18: The method of claim 12, wherein the polycation polymeric surfactant is in an amount of 40 to 60 ppm, wherein a concentration of potassium iodide is 4 to 6 mM, and wherein the corrosion inhibitor coated metal substrate has an average surface roughness of 5.5 to 6 μm.

### Claim at position 19 (depends on 5)

19: The method of claim 5, wherein the metal substrate is C1018 carbon steel.

### Claim at position 20 (depends on 5)

20: The method of claim 5, wherein the acidic aqueous electrolyte is hydrochloric acid in a concentration of 10 to 20 percent by weight.