Sintered metal friction material and production method for same
AssigneeTokai Carbon Co., Ltd.
InventorsMakoto Yasuda, Yusuke Okamura
Life of this patent
Estimating the term…
Loading patent…
AssigneeTokai Carbon Co., Ltd.
InventorsMakoto Yasuda, Yusuke Okamura
Estimating the term…
The present invention intends to provide a technique for obtaining a sintered metal friction material with a reduced copper content such that agglomerates can be hardly generated during production, the strength of a compact can be maintained, and wear during use can be suppressed. The present invention provides a sintered metal friction material that is a sintered material of a friction material composition. The friction material composition comprises 42 to 95% by mass of a metal powder for matrix. The metal powder for matrix comprises 20 to 40% by mass of an iron powder based on the mass of the friction material composition and 20 to 40% by mass of a nickel powder based on the mass of the friction material composition. The friction material composition has a copper content of 0.5% by mass or less. The nickel powder comprises a spherical nickel powder and a chained nickel powder.
A sintered metal friction material that is a sintered material of a friction material composition, wherein
A method for producing a sintered metal friction material comprising the steps of: