# US 2025/0084266 A1 · Ink formulations and film constructions thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0084266 A1
- Document ID: US20250084266A1
- Status: Published application
- Kind: A1
- Application number: 18/885,686
- Filed: 2024-09-15
- Published: 2025-03-13
- Earliest claimed: 2013-09-11
- Assignees: Landa Corporation Ltd.
- Applicants: Landa Corporation Ltd.
- Inventors: Benzion LANDA; Gregory NAKHMANOVICH; Galia GOLODETZ; Sagi ABRAMOVICH
- Web page: https://patentgrep.com/patent/US20250084266A1

## CPC

- C09D 11/107: from unsaturated acids or derivatives thereof
- C09D 11/104: Polyesters
- C09D 11/106: containing macromolecular compounds obtained by reactions only involving carbon-to-carbon unsaturated bonds
- C09D 11/30: Inkjet printing inks
- C09D 11/38: characterised by non-macromolecular additives other than solvents, pigments or dyes
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

Ink formulations suitable for deposition upon the intermediate transfer member of an indirect printing system and for transfer therefrom to a substrate. The inks are aqueous inkjet inks comprising an organic polymeric resin and a colorant. Ink film constructions including a plurality of continuous ink films fixedly adhered to the printing substrate that can be obtained with these inks are also disclosed. The inks and the printed constructions are such that the ink films and the dried inks composing them have a first dynamic viscosity within a range of 106 cP to 5·107 cP at at least a first temperature within a first range of 60° C. to 87.5° C., and a second dynamic viscosity of at least 6·107 cP, for at least a second temperature within a second range of 50° C. to 55° C.

## Claims

### Claim 1

A water-based ink formulation comprising:
(a) a solvent containing water;
(b) at least one colorant dispersed or at least partly dissolved within the solvent; and
(c) at least one organic polymeric resin, dispersed within the solvent; and
(d) a softening agent selected to reduce a glass transition temperature (Tg) of said polymeric resin, the ink formulation forming, when dried, a substantially dry ink residue having:
(i) a first dynamic viscosity within a range of 106 cP to 3·108 cP over at least part of a first temperature range of 60° C. to 110° C.; and
(ii) a second dynamic viscosity of at least 6·107 cP, over at least a part of a second temperature range of 50° C. to 55° C.;
said second dynamic viscosity at 55° C. exceeding the first dynamic viscosity at 85° C.;
said softening agent having a pure vapor pressure of at most 0.40 kPa at 150° C.

### Claim 2 (depends on 1)

The formulation of claim 1, said softening agent having a vapor pressure of at most 0.35 kPa, at most 0.25 kPa, at most 0.20 kPa, at most 0.15 kPa, at most 0.12 kPa, at most 0.10 kPa, at most 0.08 kPa, at most 0.06 kPa, or at most 0.05 kPa, at 150° C.

### Claim 3 (depends on 1)

The formulation of claim 1, at least one particular resin of said organic polymeric resin having an elevated glass transition temperature (Tg) of at least 50° C., at least 52° C., at least 54° C., at least 56° C., at least 58° C., at least 60° C., at least 65° C., at least 70° C., at least 75° C., at least 80° C., at least 85° C., at least 90° C., or at least 95° C.

### Claim 4 (depends on 3)

The formulation of claim 3, said softening agent selected and/or added in an amount to reduce said elevated glass transition temperature by at least 5° C., at least 7° C., at least 10° C., at least 15° C., at least 20° C., at least 25° C., at least 30° C., at least 40° C., or at least 50° C.

### Claim 5 (depends on 1)

The formulation of claim 1, said substantially dry ink residue has, at at least one of 100° C., 90° C., 85° C., 80° C., 75° C., and 70° C., an overall transferability rating of at least 0.90, at least 0.95, or 1.0.

### Claim 6 (depends on 3)

The formulation of claim 3, said softening agent selected and added in an amount such that said substantially dry ink residue has, at at least one of 100° C., 90° C., 85° C., 80° C., 75° C., and 70° C., an overall transferability rating of at least 0.90, at least 0.95, or 1.0.

### Claim 7 (depends on 1)

The formulation of claim 1, at least one polymeric resin of said at least one organic polymeric resin having a minimum film-forming temperature (MFFT) of at least 48° C., at least 50° C., at least 52° C., at least 54° C., at least 56° C., at least 58° C., at least 60° C., at least 65° C., at least 70° C., or at least 75° C.

### Claim 8 (depends on 1)

The formulation of claim 1, said first temperature range being 60° C. to 100° C.

### Claim 9 (depends on 1)

The formulation of claim 1, said first temperature range being 60° C. to 87.5° C., said first dynamic viscosity being within a range of 106 cP to 5·107 cP over at least part of said first temperature range.

### Claim 10 (depends on 1)

The formulation of claim 1, a weight ratio of said softening agent to said substantially dry ink residue being within a range of 0.01 to 0.25, 0.025 to 0.25, 0.04 to 0.25, 0.06 to 0.25, 0.08 to 0.25, 0.10 to 0.25, 0.10 to 0.20, or 0.12 to 0.20.

### Claim 11 (depends on 1)

The ink formulation of claim 1, the formulation being an aqueous inkjet ink having at least one of
(i) a viscosity of 2 to 25 cP at at least one particular temperature in a jetting temperature range of 20-60° C.; and
(ii) a surface tension of at most 50 milliNewton/m at at least one particular temperature within said jetting temperature range.

### Claim 12 (depends on 1)

The ink formulation of claim 1, the formulation having a total solids content, and wherein a first weight ratio of said softening agent to said total solids content is at least 0.01, at least 0.02, at least 0.03, at least 0.04, at least 0.06, at least 0.08, or at least 0.10.

### Claim 13 (depends on 12)

The formulation of claim 12, said first weight ratio being at most 0.20, at most 0.15, at most 0.12, or at most 0.11.

### Claim 14 (depends on 1)

The ink formulation of claim 1, the formulation having a total resin content, and wherein a second weight ratio of said softening agent to said total resin content is at least 0.01, at least 0.02, at least 0.03, at least 0.04, at least 0.06, at least 0.08, at least 0.10, or at least 0.12.

### Claim 15 (depends on 14)

The formulation of claim 14, said second weight ratio being at most 0.25, at most 0.20, at most 0.15, or at most 0.13.

### Claim 16 (depends on 1)

The ink formulation of claim 1, the formulation having at least one high Tg resin having a Tg above 50° C., and wherein a third weight ratio of said softening agent to said at least one high Tg resin is at least 0.02, at least 0.04, at least 0.06, at least 0.08, at least 0.10, at least 0.12, at least 0.15, or at least 0.20.

### Claim 17 (depends on 16)

The formulation of claim 16, said third weight ratio being at most 1.0, at most 0.70, at most 0.50, at most 0.40, at most 0.30, at most 0.20, at most 0.17, at most 0.15, at most 0.12, or at most 0.10.

### Claim 18 (depends on 1)

The formulation of claim 1, wherein ΔT defines a temperature differential between a temperature (TF) at which said dried ink residue begins to exhibit a particular degree of flowability, and a baseline temperature (TB):
Δ
⁢
T
=
T
F
-
T
B
said degree of flowability being defined by a critical viscosity (μCR) at which said degree of flowability is achieved,
and wherein, when said baseline temperature equals 50° C., and said critical viscosity equals 108 cP, said temperature differential is at least 3° C., at least 4° C., at least 5° C., at least 7° C., at least 12° C., at least 15° C., at least 18° C., at least 20° C., or at least 25° C.

### Claim 19 (depends on 1)

The formulation of claim 1, said polymeric resin including, mainly including, or consisting essentially of an acrylic-based polymer selected from the group consisting of an acrylic polymer and an acrylic-styrene copolymer.

### Claim 20 (depends on 1)

The formulation of claim 1, the formulation adapted such that when diluted with water by at least 50%, at least 100%, at least 150%, at least 200%, at least 250%, at least 300%, at least 350%, or at least 400%, on a weight/weight basis by water, a resultant mixture is an aqueous inkjet ink having: (i) a viscosity of 2 to 25 cP at at least one particular temperature in a range of 20-60° C.; and (ii) a surface tension of at most 50 milliNewton/m at at least one particular temperature within said range.

### Claim 21

(canceled)