# US 2025/0084248 A1 · Polyethylene glycol-based polymer processing aids

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0084248 A1
- Document ID: US20250084248A1
- Status: Published application
- Kind: A1
- Application number: 18/728,367
- Filed: 2023-02-08
- Published: 2025-03-13
- Earliest claimed: 2022-02-14
- Assignees: ExxonMobil Chemical Patents Inc.
- Applicants: Exxonmobil Chemical Patents Inc.
- Inventors: Nino RUOCCO; Michael A. LEAF; Danny VAN HOYWEGHEN; Stephen E. DEHLINGER
- Web page: https://patentgrep.com/patent/US20250084248A1

## CPC

- C08L 71/02: Polyalkylene oxides
- C08L 23/08: Copolymers of ethene (C08L23/16 takes precedence)
- C08L 2207/066: LDPE (radical process)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

Methods and compositions for processing polymers with fluorine-free polymer processing aids (PPAs) are described. The methods can include continuously extruding a polymer composition through an extruder to form a polymer product, and during at least a portion of the extruding, continually feeding a polyethylene glycol (PEG) composite to the extruder so that the PEG composite and polymer composition are coextruded through the extruder at conditions sufficient to melt blend the PEG composite and the polymer composition. The PEG composite can comprise or consist essentially of PEG (preferably PEG having weight average molecular weight less than 10,000 g/mol) and one or polymers having melting point at 1 atm greater than that of the PEG.

## Claims

### Claim 1

A process for making a polymer product using a polyethylene glycol (PEG) composite, the process comprising:
a. continuously extruding a polymer composition through an extruder to form the polymer product; and
b. during at least a portion of the extruding, continually feeding the PEG composite to the extruder so that the PEG composite and polymer composition are coextruded through the extruder at conditions sufficient to melt blend the PEG composite and the polymer composition;
wherein the PEG composite comprises solid particles of (i) PEG having weight average molecular weight (Mw) less than 10,000 g/mol, and (ii) one or more polymers having melting point at 1 atm greater than that of the PEG.

### Claim 2 (depends on 1)

The process of claim 1, wherein the PEG has Mw within the range from 6,500 to 9,500 g/mol.

### Claim 3 (depends on 1)

The process of claim 1, wherein the one or more polymers of the PEG composite each have melting point at 1 atm of 100° C. or greater.

### Claim 4 (depends on 3)

The process of claim 3, wherein the one or more polymers of the PEG composite each have melting point at 1 atm of 120° C. or greater.

### Claim 5 (depends on 1)

The process of claim 1, wherein the one or more polymers of the PEG composite comprise polyethylene.

### Claim 6 (depends on 5)

The process of claim 5, wherein the polyethylene of the PEG composite is selected from the group consisting of: metallocene-catalyzed linear low density polyethylene (mLLDPE); Ziegler-Natta-catalyzed linear low density polyethylene (ZN-LLDPE), and low density polyethylene (LDPE) produced using free radical polymerization.

### Claim 7 (depends on 1)

The process of claim 1, wherein the PEG composite consists essentially of the PEG and a polyethylene selected from mLLDPE, ZN-LLDPE, and LDPE.

### Claim 8 (depends on 6)

The process of claim 6, wherein the polyethylene is mLLDPE.

### Claim 9 (depends on 6)

The process of claim 6, wherein the polyethylene is ZN-LLDPE.

### Claim 10 (depends on 6)

The process of claim 6, wherein the polyethylene of the PEG composite has melt index (MI, measured at 190° C. and 2.16 kg loading) of 0.8 g/10 min or greater and ratio of weight-average molecular weight to number-average molecular weight (Mw/Mn) greater than 3.0.

### Claim 11 (depends on 10)

The process of claim 10, wherein the polyethylene of the PEG composite has MI within the range from 0.8 to 5.0 g/10 min and Mw/Mn within the range from 3.5 to 4.5.

### Claim 12 (depends on 1)

The process of claim 1, wherein the PEG composite comprises from 30 to 70 wt % PEG and the balance the one or more polymers, said wt % on the basis of total mass of the PEG composite.

### Claim 13 (depends on 12)

The process of claim 12, wherein the PEG composite comprises from 40 to 60 wt % PEG and the balance the one or more polymers.

### Claim 14 (depends on 13)

The process of claim 13, wherein the PEG composite has a weight ratio of PEG:polymer(s) of about 50:50.

### Claim 15 (depends on 1)

The process of claim 1, wherein the polymer composition is a linear low density polyethylene (LLDPE).

### Claim 16 (depends on 15)

The process of claim 15, wherein the LLDPE is a metallocene-catalyzed LLDPE.

### Claim 17 (depends on 15)

The process of claim 15, wherein the LLDPE is a copolymer of ethylene and a C3 to C12 comonomer, and has one or more of the following properties: melt index (12, determined at 190° C., 2.16 kg loading) within the range from 0.1 to 1.5 g/10 min; density within the range from 0.905 to 0.945 g/cm3; and melt index ratio (MIR) within the range from 10 to 85.