# US 2025/0084229 A1 · Aramid Aerogel and A Preparation Method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0084229 A1
- Document ID: US20250084229A1
- Status: Published application
- Kind: A1
- Application number: 18/244,322
- Filed: 2023-09-11
- Published: 2025-03-13
- Earliest claimed: 2023-09-11
- Assignees: Microvast Advanced Membranes Inc.
- Applicants: Microvast Advanced Membranes Inc.
- Inventors: Haipeng ZHANG; Jinbo HE; Qingjin SUN; Wenjuan Liu MATTIS
- Web page: https://patentgrep.com/patent/US20250084229A1

## CPC

- C08J 9/28: by elimination of a liquid phase from a macromolecular composition or article, e.g. drying of coagulum
- C08J 9/286: {the liquid phase being a solvent for the monomers but not for the resulting macromolecular composition, i.e. macroporous or macroreticular polymers}
- C08G 69/32: from aromatic diamines and aromatic dicarboxylic acids with both amino and carboxylic groups aromatically bound
- C08J 2201/0542: from an organic solvent-based polymer composition
- C08J 2205/026: Aerogel, i.e. a supercritically dried gel
- C08J 2205/042: Nanopores, i.e. the average diameter being smaller than 0,1 micrometer
- C08J 2377/06: Polyamides derived from polyamines and polycarboxylic acids (C08J2377/10 takes precedence)
- C08J 2377/10: Polyamides derived from aromatically bound amino and carboxyl groups of amino carboxylic acids or of polyamines and polycarboxylic acids
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

Provided in the present disclosure are an aramid aerogel and a preparation method thereof. The aramid aerogel is a porous material, and the porosity of the aramid aerogel is 65-99%. By means of the preparation method in the present disclosure, an aramid material having good high heat resistance may be prepared into the aramid aerogel, such that the aramid aerogel is suitable for industrial production. An application range of the aramid aerogel is expanded by owning the aramid aerogel with the above porosity. In addition, the aramid aerogel has good structure and mechanical properties and excellent thermal insulation performance, and in particular, has a very good application prospect in the field of high temperature thermal insulation.

## Claims

### Claim 1

An aramid aerogel, wherein the aramid aerogel is a porous material, and the porosity of the aramid aerogel is 65-99%.

### Claim 2 (depends on 1)

The aramid aerogel according to claim 1, wherein a specific surface area of the aramid aerogel is 50-1000 m2/g; and/or a pore volume of the aramid aerogel is 0.05-1.5 cm3/g.

### Claim 3 (depends on 1)

The aramid aerogel according to claim 1, wherein an average pore diameter of pores of the aramid aerogel is 1-50 nm; and/or the density of the aramid aerogel is 1-500 mg/cm3.

### Claim 4 (depends on 1)

A method for preparing the aramid aerogel according to claim 1, comprising:
step S1, in an oxygen-free atmosphere, performing a complex reaction on raw materials comprising aramid slurry and ferrous halide, so as to obtain a complex precipitate;
step S2, performing a gelation reaction on the complex precipitate and a gelation reagent, so as to obtain gel;
step S3, performing solvent displacement treatment on the gel, so as to obtain an aramid precipitate;
step S4, drying the aramid precipitate, so as to obtain the aramid aerogel.

### Claim 5 (depends on 4)

The method according to claim 4, wherein in the step S1, a mass ratio of aramid in the aramid slurry to the ferrous halide is 0.032-0.8:1.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the aramid in the aramid slurry is any one or more of poly(p-phenylene terephthamide), polymetaphenylene isophthalamide, poly(p-benzamide), and polyphenylsulfone terephthalamide.

### Claim 7 (depends on 4)

The method according to claim 4, wherein in the step S1, the temperature of the complex reaction is 5-60° C.; and/or time for the complex reaction is 0.3-33 h.

### Claim 8 (depends on 4)

The method according to claim 4, wherein the aramid slurry comprises a first solvent; and the first solvent is any one or more of dimethyl sulfoxide, N, N-dimethylformamide, N,N-dimethylacetamide, N,N-dimethylhexanamide, N-methylpyrrolidone, and triethyl phosphate.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the solid content of the aramid slurry is 1-10%, and/or the pH value of the aramid slurry is 2-7.

### Claim 10 (depends on 4)

The method according to claim 4, wherein in the step S1, the ferrous halide is a ferrous halide powder or a ferrous halide solution; the ferrous halide is selected from any one or more of ferrous chloride tetrahydrate, anhydrous ferrous chloride, ferrous bromide hydrate, and anhydrous ferrous bromide; and the ferrous halide solution comprises the ferrous halide and a second solvent.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the second solvent is any one or more of water, methanol, ethanol, and acetic acid.

### Claim 12 (depends on 10)

The method according to claim 10, wherein a mass ratio of the ferrous halide to the second solvent is 10-20:5-10.

### Claim 13 (depends on 4)

The method according to claim 4, wherein in the step S2, the temperature of the gelation reaction is 5-60° C.; and/or time for the gelation reaction is 3-30 h.

### Claim 14 (depends on 4)

The method according to claim 4, wherein in the step S2, the gelation reagent is selected from any one or more of water, an aqueous solution containing 20 wt. %-50 wt. % of N, N-dimethylacetamide, hydrochloric acid, sulfuric acid, ethanol, ethylene glycol, glycerol, acetone, tetrahydrofuran, chloroform, dichloromethane, glacial acetic acid, and nitric acid.

### Claim 15 (depends on 4)

The method according to claim 4, wherein in the step S3, a number of times for solvent displacement treatment is 3-10, and/or time for solvent displacement treatment is 2-4 h/time.

### Claim 16 (depends on 4)

The method according to claim 4, wherein in the step S4, drying treatment comprises performing a vacuum freeze-drying process and/or a vacuum drying process on the aramid precipitate; and the vacuum freeze-drying process comprises: holding the aramid precipitate at −40° C. to −20° C. for 4-10 h, then under a vacuum condition, successively holding the aramid precipitate at −20° C. to −10° C. for 4-10 h, at −10° C. to 0° C. for 4-10 h, and at 0° C. to 10° C. for 4-10 h.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the vacuum drying process comprises: the aramid precipitate or the aramid precipitate obtained after vacuum drying is held at 100° C. to 150° C. for 6-10 h.

### Claim 18 (depends on 4)

The method according to claim 4, further comprising a process of preparing the aramid slurry; and the preparation process comprises:
performing an amidation reaction on raw materials comprising aromatic diacyl chloride, aromatic diamine, and a third solvent, so as to obtain an amidation product;
neutralizing the amidation product by using an alkaline reagent, so as to obtain a neutralized product;
diluting the neutralized product by using a fourth solvent, so as to obtain the aramid slurry; or
dissolving aramid into the fourth solvent, so as to obtain the aramid slurry.

### Claim 19 (depends on 18)

The method according to claim 18, wherein a mass ratio of the aromatic diacyl chloride to the third solvent is 10-30:45-135, and/or a mass ratio of the aromatic diamine to the third solvent is 5-15:45-135; and/or the third solvent and the fourth solvent are respectively independently selected from any one or more of dimethyl sulfoxide, N,N-dimethylformamide, N,N-dimethylacetamide, N,N-dimethylhexanamide, N-methylpyrrolidone, and triethyl phosphate.

### Claim 20 (depends on 18)

The method according to claim 18, wherein the solid content of the neutralized product is 10-30%, and/or the using amount of the alkaline reagent is 1-5% of a total mass of the amidation product.