# US 2025/0084225 A1 · Heat-shrinkable polyester film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0084225 A1
- Document ID: US20250084225A1
- Status: Published application
- Kind: A1
- Application number: 18/725,969
- Filed: 2022-09-28
- Published: 2025-03-13
- Earliest claimed: 2022-03-31
- Assignees: C.I. Takiron Corporation; Bonset America Corporation
- Applicants: C.I. TAKIRON Corporation; Bonset America Corporation
- Inventors: Takuma KANEKO; Yuichiro KANZAKA; Shuuta YUGE; Tatsuya IRIFUNE
- Web page: https://patentgrep.com/patent/US20250084225A1

## CPC

- C08J 5/00: Manufacture of articles or shaped materials containing macromolecular substances (manufacture of semi-permeable membranes B01D67/00 - B01D71/00)
- C08J 5/18: Manufacture of films or sheets
- C08J 3/226: {using a polymer as a carrier}
- C08J 2367/06: Unsaturated polyesters
- C08J 2467/06: Unsaturated polyesters
- C08K 3/36: Silica
- C08K 2201/005: Additives being defined by their particle size in general
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A heat-shrinkable polyester film is provided, which has excellent high humidity storage stability, and effectively suppresses a breakage phenomenon of the film at the time of thermal shrinkage. A heat-shrinkable polyester film derived from a polyester resin composition including a crystalline polyester resin of 10% to 70% by weight satisfies the following configurations (a) and (b): (a) when upper yield point stresses in a stress-strain curve in an MD direction that orthogonally intersects a main shrinkage direction as measured before and after storage for 30 days under high humidity conditions of 23° C. and 50% RH are designated as E1 (MPa) and E2 (MPa), respectively, the E2 and E1 satisfy the following relational expression (1): 0 ≤ E ⁢ 2 - E ⁢ 1 ≤ 10 ( 1 ) (b) a thermal shrinkage ratio A1 (main shrinkage direction at 98° C. for 10 seconds) has a value of 30 to 80%.

## Claims

### Claim 1

A heat-shrinkable polyester film derived from a polyester resin composition including a crystalline polyester resin in an amount in a range of 10% to 70% by weight with respect to the total resin amount,
wherein a main shrinkage direction is designated as TD direction, a direction orthogonally intersecting the TD direction is designated as MD direction, and the heat-shrinkable polyester film satisfies the following configurations (a) and (b):
(a) when upper yield point stresses in a stress-strain curve in the MD direction as measured before and after storage for 30 days under high humidity conditions at 23° C. and 50% RH are designated as E1 (MPa) and E2 (MPa), respectively, the E1 and E2 satisfy the following relational expression (1):
0
≤
E
⁢
2
-
E
⁢
1
≤
1
⁢
0
;
(
1
)
(b) when a thermal shrinkage ratio in the TD direction in a case where the heat-shrinkable polyester film is shrunk under the conditions of 10 seconds in hot water at 98° C. is designated as A1, the A1 has a value within a range of 30% to 80%.

### Claim 2 (depends on 1)

The heat-shrinkable polyester film according to claim 1, wherein as configuration (c), the upper yield point stress E1 has a value within a range of 45 to 65 MPa, and the upper yield point stress E2 has a value within a range of 50 to 70 MPa.

### Claim 3 (depends on 1)

The heat-shrinkable polyester film according to claim 1, wherein as configuration (d), when lower yield point stresses in a stress-strain curve in the MD direction as measured before and after storage for 30 days under high humidity conditions at 23° C. and 50% RH are designated as E3 (MPa) and E4 (MPa), respectively, the E3 and E4 satisfy the following relational expression (2):
0
≤
E
⁢
4
-
E
⁢
3
≤
8
.
(
2
)

### Claim 4 (depends on 3)

The heat-shrinkable polyester film according to claim 3, wherein as configuration (e), the lower yield point stress E3 has a value within a range of 20 to 35 MPa, and the lower yield point stress E4 has a value within a range of 20 to 35 MPa.

### Claim 5 (depends on 1)

The heat-shrinkable polyester film according to claim 1, wherein as configuration (f), when a thermal shrinkage ratio in the TD direction in a case where the heat-shrinkable polyester film is shrunk under the conditions of 10 seconds in hot water at 80° C. is designated as A2, the A2 has a value within a range of 15% to 60%.

### Claim 6 (depends on 1)

The heat-shrinkable polyester film according to claim 1, wherein as configuration (g), when a thermal shrinkage ratio in the TD direction in a case where the heat-shrinkable polyester film is shrunk under the conditions of 10 seconds in hot water at 70° C. is designated as A3, the A3 has a value of 20% or less.

### Claim 7 (depends on 1)

The heat-shrinkable polyester film according to claim 1, wherein as configuration (h), b* in the chromaticity coordinates of CIE 1976 L*a*b* as measured according to JIS Z 8781-4:2013 has a value within a range of 0.15 to 0.5.

### Claim 8 (depends on 1)

The heat-shrinkable polyester film according to claim 1, wherein as configuration (j), a haze value of the film before thermal shrinkage as measured according to JIS K 7136:2000 has a value of 8% or less.