# US 2025/0084214 A1 · Fabrication of hydrophobic, mechanically flexible and optically transparent polyimide aerogels

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0084214 A1
- Document ID: US20250084214A1
- Status: Published application
- Kind: A1
- Application number: 18/243,824
- Filed: 2023-09-08
- Published: 2025-03-13
- Earliest claimed: 2023-09-08
- Assignees: The Governing Council of the University of Toronto
- Applicants: The Governing Council of the University of Toronto
- Inventors: Hani NAGUIB; Omid AGHABABAEI TAFRESHI; Shahriar GHAFFARI-MOSANENZADEH; Zia SAADATNIA
- Web page: https://patentgrep.com/patent/US20250084214A1

## CPC

- C08G 73/1032: {characterised by the solvent(s) used}
- C08G 73/101: {containing chain terminating or branching agents}
- C08G 73/1067: {Wholly aromatic polyimides, i.e. having both tetracarboxylic and diamino moieties aromatically bound}
- C08J 3/24: Crosslinking, e.g. vulcanising, of macromolecules (mechanical aspects B29C35/00; crosslinking agents C08K)
- C08J 5/18: Manufacture of films or sheets
- C08J 2379/08: Polyimides; Polyester-imides; Polyamide-imides; Polyamide acids or similar polyimide precursors
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

The present disclosure provides a method of fabrication of physically crosslinked polyimide (PCPI) aerogels with significantly improved properties using no chemical crosslinker. The fabricated PCPI aerogels present high moisture resistance, hydrophobic behavior, ultralow density, ultrahigh porosity, excellent thermal stability, increased mechanical strength, and high mechanical flexibility. Also, samples have been successfully fabricated in a thin-film geometry with high mechanical flexibility and controlled thickness. Furthermore, some fabricated aerogel films present improved optical transparency of over 80%, which is the highest transparency reported so far for organic PI aerogels.

## Claims

### Claim 1

A polyimide aerogel, comprising:
a polyimide-based polymer of the formula 1:
wherein n is an integer in a range between about 30 to about 50, and
wherein the polymer is physically crosslinked through polymer chain entanglement, and the aerogel is formed by a process including initial gelation for about 1-10 minutes; and
wherein the aerogel is free of polyamic amide polymer.

### Claim 2 (depends on 1)

The polyimide aerogel according to claim 1, wherein the aerogel has a pore size in a range from about 2 nanometers to about 100 nanometers.

### Claim 3 (depends on 1)

The polyimide aerogel according to claim 1, wherein the aerogel has pores with a pore size of less than about 2 nanometers.

### Claim 4 (depends on 1)

The polyimide aerogel according to claim 1, wherein the aerogel has a porosity in a range from about 85% to about 99%.

### Claim 5 (depends on 1)

The polyimide aerogel according to claim 1 is free of chemical crosslinkers.

### Claim 6 (depends on 1)

The polyimide aerogel according to claim 1, wherein the aerogel has a density in a range from about 0.07 g/cm3 to about 0.25 g/cm3.

### Claim 7 (depends on 1)

The polyimide aerogel according to claim 1, wherein the aerogel has a thermal conductivity in a range from about 15 to about 50 milliwatts/degrees Kelvin-meters.

### Claim 8 (depends on 1)

The polyimide aerogel according to claim 1, wherein the aerogel is characterized by a hydrophobicity in a range from about 90 degrees to about 140 degrees water contact angle.

### Claim 9 (depends on 1)

The polyimide aerogel according to claim 1, wherein the aerogel is characterized by a water uptake as low as about 1%.

### Claim 10 (depends on 1)

The polyimide aerogel according to claim 1, wherein the aerogel has an onset of thermal decomposition in a range from about 500 to about 700° C.

### Claim 11 (depends on 1)

The polyimide aerogel according to claim 1, wherein the aerogel has a dielectric constant in a range from about 1.5 to about 3.

### Claim 12 (depends on 1)

The polyimide aerogel according to claim 1, wherein the aerogel is in the form of a film having a thickness of at least about 80 microns, and wherein the aerogel has optical transparency in a range from about 60% to about 99%.

### Claim 13 (depends on 1)

The polyimide aerogel according to claim 1, wherein the aerogel is characterized by a compressive modulus in a range from about 17 to 25 Mega Pascal (MPa).

### Claim 14 (depends on 1)

The polyimide aerogel according to claim 1, wherein the aerogel is characterized by a tensile modulus in a range from about 1 to 5 Mega Pascal (MPa).

### Claim 15 (depends on 1)

A process of making a polyimide aerogel of claim 1, comprising the steps of
forming a wet gel by reacting a diamine monomer (DIAM) with a dianhydride monomer (DIAH) in a reaction solution comprising a dipolar aprotic solvent to form the polymer of Formula A; wherein n is between the range of 30 to 50
imidizing the formed polymer;
gelation of the formed polymer for about 1-10 minutes;
replacing the aprotic solvent with a drying solvent; and
removing the drying solvent from the formed wet gel.

### Claim 16 (depends on 15)

The process of claim 15, wherein the step of imidizing the formed polymer is performed through thermal imidization or chemical imidization.

### Claim 17 (depends on 15)

The process of claim 15, further comprising the step of aging the wet gel obtained by the initial gelation to increase the polymerization yield and to advance the degree of physical crosslinking.

### Claim 18 (depends on 15)

The process of claim 15, wherein the aprotic solvent is N-methylpyrrolidinone (NMP), dimethylformamide (DMF), dimethyl sulfoxide (DMSO), or a mixture of NMP and tetrahydrofuran (THF).

### Claim 19 (depends on 15)

The process of claim 15, wherein the step of reacting the DIAM monomer with the DIAH monomer is done without the use of a chemical crosslinker.

### Claim 20 (depends on 15)

The process of claim 15, wherein the DIAM monomer and DIAH monomer are first dissolved separately then the DIAM monomer solution is combined with the DIAH monomer solution.

### Claim 21 (depends on 15)

The process of claim 15, wherein DIAM monomer is first dissolved and DIAH monomer is added to the DIAM solution.

### Claim 22 (depends on 15)

The process of claim 15, wherein the diamine monomer (DIAM) is 2,2′-dimethylbenzidine (DMBZ).

### Claim 23 (depends on 15)

The process of claim 15, wherein the dianhydride monomer (DIAH) is biphenyl-tetracarboxylic acid dianhydride (BPDA).

### Claim 24 (depends on 15)

The process of claim 15, wherein the drying solvent is removed via supercritical drying, freeze drying, or ambient pressure drying.

### Claim 25 (depends on 15)

The process of claim 15, wherein the wet gel forming step occurs over a period of time ranging between about 1 minute to about 24 hours.