# US 2025/0084210 A1 · Polyester resin

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0084210 A1
- Document ID: US20250084210A1
- Status: Published application
- Kind: A1
- Application number: 18/284,668
- Filed: 2022-03-22
- Published: 2025-03-13
- Earliest claimed: 2021-03-30
- Assignees: Bell Polyester Products, Inc.; Daiwa Can Company; FUJIFILM Corporation
- Applicants: Bell Polyester Products, Inc.; Daiwa Can Company; Fujifilm Corporation
- Inventors: Ryota MISAKA; Keita KATSUMA; Masaya OKIMOTO; Yuta UMEDA; Akane NOZAKI; Rei MIYASAKA; Yukiharu NAGAO; Yasuhiro HAMADA
- Web page: https://patentgrep.com/patent/US20250084210A1

## CPC

- C08G 63/189: containing a naphthalene ring
- C08G 63/199: Acids or hydroxy compounds containing cycloaliphatic rings
- C08G 2250/00: Compositions for preparing crystalline polymers
- C08J 5/18: Manufacture of films or sheets
- C08J 2367/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds; (C08J2367/06 takes precedence)
- C08J 2367/06: Unsaturated polyesters
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

A polyester resin contains a polymer of an acid component (A) and an alcohol component (B). The component (A) contains 80 mol % or more of a 2,6-naphthalenedicarboxylic acid component with respect to a total amount of the component (A). The component (B) contains at least two types selected from the group consisting of 1,4-butanediol, 1,4-cyclohexanedimethanol, and ethylene glycol. The content of the at least one type of the component (B) is 80 mol % or more with respect to a total amount of the component (B).

## Claims

### Claim 1

A polyester resin comprising a polymer of an acid component (A) and an alcohol component (B), wherein:
the component (A) comprises 80 mol % or more of a 2,6-naphthalenedicarboxylic acid component with respect to a total amount of the component (A);
the component (B) comprises at least two types selected from the group consisting of 1,4-butanediol, 1,4-cyclohexanedimethanol, and ethylene glycol; and
a total amount of the at least two types of components is 80 mol % or more with respect to a total amount of the component (B).

### Claim 2 (depends on 1)

The polyester resin according to claim 1, wherein the polyester resin has a degree of polymerization of from 100 to 5000.

### Claim 3 (depends on 1)

The polyester resin according to claim 1, wherein the polyester resin has an intrinsic birefringence of 0.15 or greater.

### Claim 4 (depends on 1)

The polyester resin according to claim 1, wherein the component (B) consists of from 35 to 75 mol % of butanediol and from 25 to 65 mol % of 1,4-cyclohexanedimethanol with respect to the total amount of the component (B).

### Claim 5 (depends on 4)

The polyester resin according to claim 4, wherein the polyester resin has a film shape having a thickness of from 20 to 100 μm, and has an in-plane retardation of from 4,000 to 20,000 nm.

### Claim 6 (depends on 1)

The polyester resin according to claim 1, wherein the component (B) consists of from 5 to 80 mol % of ethylene glycol and from 20 to 95 mol % of butanediol with respect to the total amount of the component (B).

### Claim 7 (depends on 6)

The polyester resin according to claim 6, wherein the polyester resin has a film shape having a thickness of from 20 to 120 μm, and has an in-plane retardation of from 4,000 to 22,000 nm.

### Claim 8 (depends on 1)

The polyester resin according to claim 1, wherein the component (B) consists of from 82 to 95 mol % of ethylene glycol and from 5 to 18 mol % of 1,4-cyclohexanedimethanol with respect to the total amount of the component (B).

### Claim 9 (depends on 8)

The polyester resin according to claim 8, wherein the polyester resin has a film shape having a thickness of from 20 to 130 μm, and has an in-plane retardation of from 4,000 to 15,000 nm.

### Claim 10 (depends on 5)

The polyester resin according to claim 5, wherein a change in film turbidity after being heated at 150° C. for 100 hours is 1.5% or less.

### Claim 11 (depends on 5)

The polyester resin according to claim 5, wherein a thermal shrinkage rate, in both a machine stretching direction and a crosswise stretching direction of film stretching, when heated at 150° C. for 30 minutes is 2% or less with respect to a length before being heated.

### Claim 12 (depends on 5)

The polyester resin according to claim 5, wherein a minor endothermic peak temperature is 150° C. or higher.

### Claim 13 (depends on 5)

The polyester resin according to claim 5, wherein, when the film-shaped polyester resin is heated at 150° C. for 100 hours, the number of oligomers is 400 or less per 1 mm2 of the film surface.

### Claim 14 (depends on 7)

The polyester resin according to claim 7, wherein a change in film turbidity after being heated at 150° C. for 100 hours is 1.5% or less.

### Claim 15 (depends on 7)

The polyester resin according to claim 7, wherein a thermal shrinkage rate, in both a machine stretching direction and a crosswise stretching direction of film stretching, when heated at 150° C. for 30 minutes is 2% or less with respect to a length before being heated.

### Claim 16 (depends on 7)

The polyester resin according to claim 7, wherein a minor endothermic peak temperature is 150° C. or higher.

### Claim 17 (depends on 7)

The polyester resin according to claim 7, wherein, when the film-shaped polyester resin is heated at 150° C. for 100 hours, the number of oligomers is 400 or less per 1 mm2 of the film surface.

### Claim 18 (depends on 9)

The polyester resin according to claim 9, wherein a change in film turbidity after being heated at 150° C. for 100 hours is 1.5% or less.

### Claim 19 (depends on 9)

The polyester resin according to claim 9, wherein a thermal shrinkage rate, in both a machine stretching direction and a crosswise stretching direction of film stretching, when heated at 150° C. for 30 minutes is 2% or less with respect to a length before being heated.

### Claim 20 (depends on 9)

The polyester resin according to claim 9, wherein a minor endothermic peak temperature is 150° C. or higher.