# US 2025/0084204 A1 · Polymer with uv-responsive self-healing function and manufacturing method of the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0084204 A1
- Document ID: US20250084204A1
- Status: Published application
- Kind: A1
- Application number: 18/610,294
- Filed: 2024-03-20
- Published: 2025-03-13
- Earliest claimed: 2023-09-12
- Assignees: Pusan National University Industry-University Cooperation Foundation
- Applicants: Pusan National University Industry-University Cooperation Foundation
- Inventors: Chae Bin KIM; Yeomyung Yoon; Dupyo Jeon; Gyeong Hwan Choi
- Web page: https://patentgrep.com/patent/US20250084204A1

## CPC

- C08G 59/4064: {sulfur containing compounds (C08G59/4021, C08G59/4028 take precedence)}
- C08G 59/22: Di-epoxy compounds
- C08J 3/246: {Intercrosslinking of at least two polymers}
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

A polymer having a UV-responsive self-healing function at room temperature and its manufacturing method are disclosed herein. More specifically, the solid dynamic crosslinked polymer with a UV-responsive self-healing function is capable of being repaired and reprocessed through a dynamic exchange reaction of disulfide induced under exposure to UV radiation at ambient temperature when damaged after curing. The novel polymer with a UV-responsive self-healing function is capable of self-healing simply through UV exposure at ambient temperature. Therefore, it can be utilized in the recycling of thermosetting resins that are environmentally challenging to recycle in the plastic industry, and furthermore, serve as an alternative to address various environmental issues.

## Claims

### Claim 1

A polymer with a UV-responsive self-healing function, comprising:
a first monomer containing at least two epoxy groups; and
a second monomer serving as a curing agent,
wherein the first and second monomers are combined to enable a dynamic disulfide exchange reaction, allowing for self-healing.

### Claim 2 (depends on 1)

The polymer according to claim 1, wherein the first monomer comprises at least one selected from the group consisting of bisphenol-based, aminophenol-based, siloxane-based, and alicyclic epoxy resins.

### Claim 3 (depends on 1)

The polymer according to claim 1, wherein the second monomer serves as a curing agent containing sulfur and comprises at least one selected from the group consisting of 4-aminophenyl disulfide, 3,3′-dihydroxydiphenyl disulfide, and 4-(2-hydroxyethoxy)phenyl disulfide.

### Claim 4 (depends on 1)

The polymer according to claim 1, wherein the second monomer is represented by the following Chemical Formula 1, 2 or 3,

### Claim 5 (depends on 1)

The polymer according to claim 1, wherein the polymer is capable of self-healing through a dynamic disulfide exchange reaction induced by exposure to UV radiation when damaged even after curing.

### Claim 6 (depends on 5)

The polymer according to claim 5, wherein the UV radiation has a wavelength of 250 to 260 nm.

### Claim 7 (depends on 5)

The polymer according to claim 5, wherein the exposure to UV radiation is conducted by irradiating UV radiation with an intensity of 20 to 40 mW/cm2 for 5 to 15 minutes at ambient temperature.

### Claim 8

A method for manufacturing a polymer with a UV-responsive self-healing function, comprising:
mixing a first monomer and a second monomer and heating the mixture;
placing the heated mixture into a preheated mold;
degassing the mixture placed in the mold through vacuum substitution; and
heating the degassed mixture at an elevated temperature to obtain a cured polymer.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the first monomer is a monomer containing at least two epoxy groups and comprises at least one selected from the group consisting of bisphenol-based, aminophenol-based, siloxane-based, and alicyclic epoxy resins.

### Claim 10 (depends on 8)

The method according to claim 8, wherein the second monomer serves as a curing agent containing sulfur and comprises at least one selected from the group consisting of 4-aminophenyl disulfide, 3,3′-dihydroxydiphenyl disulfide, and 4-(2-hydroxyethoxy)phenyl disulfide.

### Claim 11 (depends on 8)

The method according to claim 8, wherein the second monomer is represented by the following chemical formula 1, 2, or 3,

### Claim 12 (depends on 8)

The method according to claim 8, wherein the step of mixing the first and second monomers and heating the mixture is performed at a temperature of 95 to 105° C. for 5 to 15 minutes.

### Claim 13 (depends on 8)

The method according to claim 8, wherein the step of degassing the mixture placed in the mold through vacuum substitution is degassing through vacuum substitution for 10 to 20 minutes.

### Claim 14 (depends on 8)

The method according to claim 8, wherein the step of heating the degassed mixture at an elevated temperature to obtain a cured polymer is heating the mixture at an elevated temperature of 140 to 160° C. for 9 to 11 hours to obtain a cured polymer.