# US 2025/0083972 A1 · Titanium dioxide nanomaterial, method of manufacturing the same and solar steam generator

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0083972 A1
- Document ID: US20250083972A1
- Status: Published application
- Kind: A1
- Application number: 18/384,897
- Filed: 2023-10-30
- Published: 2025-03-13
- Earliest claimed: 2023-09-07
- Assignees: National Sun Yat-Sen University
- Applicants: National Sun Yat-Sen University
- Inventors: HUI-FEN WU; MAHESHIKA KUMARIHAMY
- Web page: https://patentgrep.com/patent/US20250083972A1

## CPC

- C01G 23/0536: {by hydrolysing chloride-containing salts}
- C01G 23/047: Titanium dioxide
- C01G 23/08: Drying; Calcining {; After treatment of titanium oxide}
- F22B 1/006: {using solar heat}
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- Y02W 10/37: using solar energy
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- F22B: METHODS OF STEAM GENERATION; STEAM BOILERS
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A method of manufacturing a titanium dioxide nanomaterial according to the present invention comprises: mixing a titanium (III) chloride solution, ethanol, and a sodium chloride solution to obtain a solution to be sonicated; performing probe ultrasonication to the solution to be sonicated with an opening time and a pulse closing time for a sonicating time at a power of 45 W to 55 W and under a temperature of 23° C. to 27° C. to obtain a reaction solution; adding deionized water dropwise into the reaction solution with a predetermined adding rate, and gradually increasing the temperature of the reaction solution to 80° C. with a predetermined ramping rate to obtain a solution to be centrifuged; and centrifuging the solution to be centrifuged to separate a precipitate, wherein the precipitate includes the titanium dioxide nanomaterial.

## Claims

### Claim 1

A method of manufacturing a titanium dioxide nanomaterial, comprising:
mixing a titanium (III) chloride solution, ethanol, and a sodium chloride solution to obtain a solution to be sonicated;
performing probe ultrasonication to the solution to be sonicated with an opening time and a pulse closing time for a sonicating time at a power of 45 W to 55 W and under a temperature of 23° C. to 27° C. to obtain a reaction solution;
adding deionized water dropwise into the reaction solution with a predetermined adding rate, and gradually increasing the temperature of the reaction solution to 80° C. with a predetermined ramping rate to obtain a solution to be centrifuged; and
centrifuging the solution to be centrifuged to separate a precipitate, wherein the precipitate includes the titanium dioxide nanomaterial.

### Claim 2 (depends on 1)

The method of claim 1, wherein the opening time is 5 seconds, the pulse closing time is 1 second, and the sonicating time is 10 minutes.

### Claim 3 (depends on 1)

The method of claim 1, wherein the predetermined adding rate is 1 ml deionized water per 5 minutes, and the predetermined ramping rate is 10° C. per 20 minutes.

### Claim 4 (depends on 1)

The method of claim 1, further comprising washing the precipitate with deionized water and ethanol and then drying the washed precipitate at 50° C. for 15 hours.

### Claim 5 (depends on 1)

A titanium dioxide nanomaterial manufactured by the method of claim 1, wherein the titanium dioxide nanomaterial has a two-dimensional layered sheet structure and includes titanium (III) oxide.

### Claim 6 (depends on 5)

The titanium dioxide nanomaterial of claim 5, wherein the absorption wavelength range of the titanium dioxide nanomaterial is between 300 to 400 nm.

### Claim 7 (depends on 5)

A solar steam generator, comprising:
a first container having an opening on a top end thereof;
a second container having an opening on a top end thereof, wherein the first container is located within the second container; and
a water purification component covering the opening of the second container, wherein the water purification component has a photothermal exchange part, a heat conduction part, and a water absorption part, the photothermal exchange part and the water absorption part are both adjacent to the heat conduction part, and a surface of the photothermal exchange part has the titanium dioxide nanomaterial of claim 5.

### Claim 8 (depends on 7)

The solar steam generator of claim 7, wherein the first container has a water inlet tube and a first water outlet tube, and one end of the water inlet tube and one end of the first water outlet tube are both connected to the inside of the first container.

### Claim 9 (depends on 8)

The solar steam generator of claim 8, wherein the second container has a sidewall, and the other end of the water inlet tube and the other end of the first water outlet tube each passes through at least one hole of the sidewall.

### Claim 10 (depends on 9)

The solar steam generator of claim 9, wherein the second container has a second water outlet tube connected to the inside of the second container.

### Claim 11 (depends on 7)

The solar steam generator of claim 7, wherein the cross-sectional area of the water purification component is equal to the cross-sectional area of the second container.

### Claim 12 (depends on 7)

The solar steam generator of claim 7, wherein the photothermal exchange part is a natural fiber layer, and the titanium dioxide nanomaterial is coated on a surface of the natural fiber layer.

### Claim 13 (depends on 7)

The solar steam generator of claim 7, wherein the heat conduction part is made of metal.

### Claim 14 (depends on 7)

The solar steam generator of claim 7, wherein the water absorption part has at least one extension part extending into the inside of the first container.