# US 2025/0083961 A1 · Ammonium manganese iron phosphate precursor, lithium manganese iron phosphate positive electrode active material, preparation method thereof, and secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0083961 A1
- Document ID: US20250083961A1
- Status: Published application
- Kind: A1
- Application number: 18/957,026
- Filed: 2024-11-22
- Published: 2025-03-13
- Earliest claimed: 2022-09-02
- Assignees: Contemporary Amperex Technology (Hong Kong) Limited
- Applicants: Contemporary Amperex Technology (Hong Kong) Limited
- Inventors: Shaojun LIU; Wenwei ZHAN; Xinxin ZHANG; Chuying OUYANG; Qingzheng LI
- Web page: https://patentgrep.com/patent/US20250083961A1

## CPC

- C01B 25/451: {containing metal and ammonium}
- C01B 25/45: containing plural metal, or metal and ammonium
- H01M 4/1397: of electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/366: {as layered products}
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- C01P 2002/54: one element only
- C01P 2004/03: obtained by SEM
- C01P 2004/24: Nanoplates, i.e. plate-like particles with a thickness from 1-100 nanometer
- C01P 2006/40: Electric properties
- C01P 2006/80: Compositional purity
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for preparing the ammonium manganese iron phosphate precursor includes mixing and grinding metal source powder and phosphorus source powder to enable a low-heating-temperature solid-state reaction of each component, and then washing and drying the obtained product to obtain the ammonium manganese iron phosphate precursor, where the metal source includes an iron source, a manganese source and an optional source of a doping element M which represents doping elements at manganese and iron sites, and the phosphorus source includes triammonium phosphate.

## Claims

### Claim 1

A method for preparing an ammonium manganese iron phosphate precursor, comprising:
mixing and grinding metal source powder and phosphorus source powder to enable a low-heating-temperature solid-state reaction of the components; and
washing and drying the obtained product to obtain the ammonium manganese iron phosphate precursor;
wherein the metal source comprises an iron source, a manganese source and an optional source of a doping element M, M represents doping elements at manganese and iron sites, and the phosphorus source comprises triammonium phosphate.

### Claim 2 (depends on 1)

The method according to claim 1, wherein
mixing and grinding time is from 0.25 h to 6 h; and/or
a temperature for the low-heating-temperature solid-state reaction is from 20° C. to 100° C.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the mixing and grinding time is greater than or equal to 1.5 h.

### Claim 4 (depends on 1)

The method according to claim 1, further comprising, after mixing and grinding:
standing for standing time from 0.5 h to 12 h;
wherein a sum of the mixing and grinding time and the standing time is greater than or equal to 1.5 h.

### Claim 5 (depends on 1)

The method according to claim 1, wherein a surfactant is further added to mix and grind with the metal source powder and the phosphorus source powder.

### Claim 6 (depends on 5)

The method according to claim 5, wherein:
the surfactant comprises polyethylene glycol; and/or
an addition amount of the surfactant is 15 wt % or less, based on a total weight of the metal source powder and the phosphorus source powder.

### Claim 7 (depends on 1)

The method according to claim 1, further comprising, before mixing and grinding:
grinding the metal source powder and/or the phosphorus source powder separately.

### Claim 8 (depends on 1)

The method according to claim 1, wherein a molar ratio of the metal source powder to the phosphorus source powder is 1:(1-3).

### Claim 9 (depends on 1)

The method according to claim 1, wherein:
the washing comprises washing with water and/or washing with alcohol; and/or
the drying is vacuum drying; and/or
a drying temperature is from 60° C. to 100° C.; and/or
drying time is from 8 h to 20 h.

### Claim 10 (depends on 1)

The method according to claim 1, wherein:
the iron source is a divalent iron salt; and/or
the manganese source is a divalent manganese salt; and/or
the source of the doping element M is a divalent salt of the doping element M.

### Claim 11 (depends on 1)

An ammonium manganese iron phosphate precursor prepared by the method according to claim 1, having a chemical formula NH4FexMnyM1−x−yPO4, wherein 0<x<1, 0<y<1, 0≤1−x−y<1, M represents doping elements at manganese and iron sites, and the ammonium manganese iron phosphate precursor is electrically neutral.

### Claim 12 (depends on 11)

The ammonium manganese iron phosphate precursor according to claim 11, wherein the ammonium manganese iron phosphate precursor has a nano-sheet morphology, with an average length of 50 nm-800 nm and an average thickness of ≤100 nm.

### Claim 13 (depends on 1)

A method for preparing a lithium manganese iron phosphate positive electrode active material, comprising:
S1, mixing and grinding the ammonium manganese iron phosphate precursor prepared by the method according to claim 1 with a lithium source, in a predetermined ratio, and then performing spray drying granulation to obtain powder; and
S2, sintering the powder obtained in S1 to obtain the lithium manganese iron phosphate positive electrode active material.

### Claim 14 (depends on 13)

The method according to claim 13, wherein mixing and grinding in S1 includes mixing and grinding the ammonium manganese iron phosphate precursor with the lithium source, a source of a doping element N, a source of a doping element Q, and a source of a doping element R in a predetermined ratio, wherein N represents a doping element at a lithium site, Q represents a doping element at a phosphorus site, and R represents a doping element at an oxygen site.

### Claim 15 (depends on 13)

The method according to claim 13, wherein in S1, a carbon source is further added for mixing and grinding, and the carbon source comprises one or more of organic carbon sources and inorganic carbon sources.

### Claim 16 (depends on 13)

The method according to claim 13, wherein:
in S1, grinding time is from 1 h to 6 h; and/or
in S1, a spray drying temperature is from 200° C. to 250° C.

### Claim 17 (depends on 13)

The method according to claim 13, wherein in S2, the sintering comprises: pre-sintering the powder obtained in S1 at a low temperature of 350° C.-500° C. in an air atmosphere or a protective gas atmosphere, and then sintering the powder at a high temperature of 650° C.-750° C. in the protective gas atmosphere to obtain the lithium manganese iron phosphate positive electrode active material.

### Claim 18 (depends on 17)

The method according to claim 17, further comprising, after the low-temperature pre-sintering and before the high-temperature sintering, grinding and spray drying granulation.

### Claim 19 (depends on 13)

A lithium manganese iron phosphate positive electrode active material prepared by the method according to claim 13, having a chemical formula LiaNbFexMnyM1−x−yP1−mQmO4−nRn, wherein:
M represents doping elements at manganese and iron sites, N represents a doping element at a lithium site, Q represents a doping element at a phosphorus site, and R represents a doping element at an oxygen site;
0.9≤a≤1.1;
0≤b≤0.1;
0<x<1;
0<y<1;
0
≤
1
-
x
-
y
<
1
;
0≤m<1;
0≤n<4; and
the lithium manganese iron phosphate positive electrode active material is electrically neutral.

### Claim 20 (depends on 19)

A secondary battery, comprising the lithium manganese iron phosphate positive electrode active material according to claim 19.