# US 2025/0083413 A1 · Stainless steel polymer adhesion layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0083413 A1
- Document ID: US20250083413A1
- Status: Published application
- Kind: A1
- Application number: 18/588,511
- Filed: 2024-02-27
- Published: 2025-03-13
- Earliest claimed: 2023-09-07
- Assignees: Apple Inc.
- Applicants: Apple Inc.
- Inventors: Todd S. Mintz; Kar-Wai Hon; James A. Curran; Daniel T. McDonald
- Web page: https://patentgrep.com/patent/US20250083413A1

## CPC

- B32B 15/09: comprising polyesters
- C25D 11/34: of metals or alloys not provided for in groups C25D11/04 - C25D11/32
- B32B 15/08: of synthetic resin
- B32B 15/18: comprising iron or steel {(B32B15/011, B32B15/012 and B32B15/013 take precedence)}
- B32B 27/36: comprising polyesters
- C23F 1/40: for etching other metallic material
- C25F 3/06: of iron or steel
- B32B 2255/06: on metal layer
- B32B 2255/28: Multiple coating on one surface
- B32B 2262/101: Glass fibres
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- C25F: PROCESSES FOR THE ELECTROLYTIC REMOVAL OF MATERIALS FROM OBJECTS; APPARATUS THEREFOR

## Abstract

A chemical treatment process has been identified as a simple and effective means of improving the bonding of injection-molded polymer to stainless steel surfaces. This process forms an oxide layer on a stainless steel surface that includes a layered double hydroxide. The layered double hydroxide both raises the bond strength and minimizes air or water leakage. The process enables the use of stainless steel alloys with injection molded polymer structural bonds in strong, lightweight, and water-resistant enclosures for consumer electronics.

## Claims

### Claim 1

An oxide layer on a stainless steel substrate comprising a layered double hydroxide;
wherein the oxide layer comprises an iron-rich precipitate deposited on a porous iron-nickel layer.

### Claim 2 (depends on 1)

The oxide layer of claim 1, wherein the oxide layer comprises a surface roughness of between about 500 nm and about 1000 nm Sz.

### Claim 3 (depends on 1)

The oxide layer of claim 1, wherein the oxide layer comprises a thickness of about 100 nm to about 300 nm.

### Claim 4 (depends on 1)

The oxide layer of claim 1, wherein the oxide layer comprises a porosity between about 30% and about 80%.

### Claim 5 (depends on 1)

The oxide layer of claim 1, wherein the iron-rich precipitate comprises a microstructure including a spheroidal structure having a diameter between about 20 nm and about 100 nm.

### Claim 6 (depends on 1)

The oxide layer of claim 1, wherein the oxide layer comprises a first layer including an iron-nickel hydroxide layer having a thickness between about 80 nm and about 150 nm; and
further comprising a second layer comprising an iron-rich oxide disposed over the first layer, the second layer comprising spheroidal structures having a diameter between about 20 nm and about 100 nm.

### Claim 7 (depends on 1)

The oxide layer of claim 1, wherein the oxide layer further comprises a porous structure defining a pore having a diameter between about 20 nm and about 50 nm.

### Claim 8

A stainless steel-polymer interface, comprising:
an oxide layer on a stainless steel substrate; and
a polymer extended into the oxide layer;
wherein the polymer extended into the oxide layer forms a bond comprising a bond strength of about 25 MPa or greater.

### Claim 9 (depends on 8)

The stainless steel-polymer interface of claim 8, wherein the oxide layer comprises a layered double hydroxide.

### Claim 10 (depends on 8)

The stainless steel-polymer interface of claim 8, wherein the polymer comprises a glass-filled PBT resin, a polyamide, or an epoxy.

### Claim 11 (depends on 8)

The stainless steel-polymer interface of claim 8, wherein the oxide layer comprises a surface roughness greater than about 500 nm Sz.

### Claim 12 (depends on 8)

The stainless steel-polymer interface of claim 8, the oxide layer comprising an iron-rich precipitate deposited on a porous iron-nickel layer.

### Claim 13 (depends on 8)

The stainless steel-polymer interface of claim 8, wherein the polymer comprises an injection-molded polymer.

### Claim 14 (depends on 8)

The stainless steel-polymer interface of claim 8, wherein the polymer comprises a dynamic viscosity from about 800 Pa·s to about 200 Pa·s.

### Claim 15

A method of forming an oxide layer on a stainless steel substrate comprising:
etching the stainless steel substrate by immersing the substrate in a caustic solution; and
applying a cathodic potential between the stainless steel substrate and an anode.

### Claim 16 (depends on 15)

The method of claim 15, wherein the caustic solution comprises a solution between about 1 molar and about 10 molar sodium hydroxide or potassium hydroxide.

### Claim 17 (depends on 15)

The method of claim 15, wherein the cathodic potential comprises a pulsed potential comprising a voltage between about 2V and about 5V and a pulse rate of between about 1 minute and about 4 minutes energized, and about 1 minute and about 4 minutes de-energized, the pulse repeated between about 2 and about 20 times.

### Claim 18 (depends on 15)

The method of claim 15, wherein the caustic solution is between about 50° C. and about 90° C.

### Claim 19 (depends on 15)

The method of claim 15, wherein a ratio between the anode and the stainless steel substrate is between about 2:1 and about 10:1.

### Claim 20 (depends on 15)

The method of claim 15, wherein the oxide layer comprises a surface roughness between about 500 nm and about 1000 nm Sz.