# US 2025/0083283 A1 · Method for removing laminated material on surface of intermediately discharged silicon wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0083283 A1
- Document ID: US20250083283A1
- Status: Published application
- Kind: A1
- Application number: 18/705,010
- Filed: 2022-10-27
- Published: 2025-03-13
- Earliest claimed: 2021-10-28
- Assignees: Nanolub Co.,Ltd; Keitech Co., Ltd.
- Applicants: Nanolub Co.,Ltd; Keitech Co.,Ltd
- Inventors: Yongsheng SUN
- Web page: https://patentgrep.com/patent/US20250083283A1

## CPC

- B24C 11/00: Selection of abrasive materials {or additives} for abrasive blasts (polishing compositions C09G)
- B24C 1/00: Methods for use of abrasive blasting for producing particular effects; Use of auxiliary equipment in connection with such methods
- B24C 1/04: for treating only selected parts of a surface, e.g. for carving stone or glass
- B24C 5/02: Blast guns, e.g. for generating high velocity abrasive fluid jets for cutting materials {(perforating by fluid jet B26F1/26)}
- B24C 9/00: Appurtenances of abrasive blasting machines or devices, e.g. working chambers, arrangements for handling used abrasive material
- H10P 52/00: Grinding, lapping or polishing of wafers, substrates or parts of devices
- B24C: ABRASIVE OR RELATED BLASTING WITH PARTICULATE MATERIAL
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Provided is a method for removing a laminated material on a surface of a silicon wafer capable of considerably efficiently removing a laminated material on a surface of a silicon wafer at a low cost with a simple apparatus without a negative effect on environment or a serious damage on the silicon wafer as a substrate. A blasting process was performed by spraying boron carbide (B4C) having a particle size of #220 as an abrasive on a laminate surface of a laminated material of an intermediately discharged silicon wafer using a blasting machine (dry type that sprays a dry abrasive, and a gravity type that sprays the abrasive fallen from a tank of the abrasive due to gravity on a compressed air) under spray conditions of a spray distance=120 mm and a spray pressure=0.2 MPa for five seconds.

## Claims

### Claim 1

A method for removing a laminated material from a surface of an intermediately discharged silicon wafer discharged outside a system during manufacturing a semiconductor integrated circuit, the method comprising
spraying an abrasive having a density of 2.0 g/cm3 or more and less than 3.0 g/cm3 and a Mohs hardness of 9 or more and less than 11 to the surface of the intermediately discharged silicon wafer to forcibly peel off the laminated material on the surface of the intermediately discharged silicon wafer.

### Claim 2 (depends on 1)

The method for removing a laminated material on a surface of an intermediately discharged silicon wafer according to claim 1, wherein
the abrasive has a particle size of from #150 to #10,000.

### Claim 3 (depends on 1)

The method for removing a laminated material on a surface of an intermediately discharged silicon wafer according to claim 1, wherein
a spray pressure of the abrasive is from 0.15 MPa to 0.8 MPa.

### Claim 4 (depends on 1)

The method for removing a laminated material on a surface of an intermediately discharged silicon wafer according to according to claim 1, wherein
the abrasive is boron carbide (B4C).

### Claim 5 (depends on 1)

The method for removing a laminated material on a surface of an intermediately discharged silicon wafer according to according to claim 1, the method comprising
spraying the abrasive to the surface of the intermediately discharged silicon wafer placed on a base, wherein
a buffer is interposed between the base and the intermediately discharged silicon wafer.