# US 2025/0083227 A1 · Copper alloy powder for lamination shaping, lamination shaped product production method, and lamination shaped product

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0083227 A1
- Document ID: US20250083227A1
- Status: Published application
- Kind: A1
- Application number: 18/951,748
- Filed: 2024-11-19
- Published: 2025-03-13
- Earliest claimed: 2017-08-21
- Assignees: JX Nippon Mining & Metals Corporation
- Applicants: JX Nippon Mining & Metals Corporation
- Inventors: Kenji SATO; Yoshitaka SHIBUYA
- Web page: https://patentgrep.com/patent/US20250083227A1

## CPC

- B22F 3/105: by using electric current {other than for infrared radiant energy}, laser radiation or plasma (B22F3/11 takes precedence){; by ultrasonic bonding (B22F3/115 takes precedence)}
- B22F 1/00: Metallic powder; Treatment of metallic powder, e.g. to facilitate working or to improve properties
- B22F 1/05: Metallic powder characterised by the size or surface area of the particles
- B22F 3/16: in successive or repeated steps
- B22F 10/28: Powder bed fusion, e.g. selective laser melting [SLM] or electron beam melting [EBM]
- B33Y 10/00: Processes of additive manufacturing
- B33Y 70/00: Materials specially adapted for additive manufacturing
- C22C 9/00: Alloys based on copper
- B22F 10/38: to achieve specific product aspects, e.g. surface smoothness, density, porosity or hollow structures
- B22F 2009/0804: {Dispersion in or on liquid, other than with sieves}
- B22F 2009/0824: {with a specific atomising fluid}
- B22F 2202/11: Use of irradiation
- B22F 2301/10: Copper
- B22F 2998/10: Processes characterised by the sequence of their steps
- B33Y 80/00: Products made by additive manufacturing
- Y02P 10/25: Process efficiency
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

An object of the present invention is to provide a copper alloy powder for lamination shaping comprising a copper alloy, a method for producing a lamination shaped product and a lamination shaped product, which can achieve coexistence of mechanical strength and conductivity. One aspect of the present invention relates to a copper alloy powder for lamination shaping, including at least one additive element having a solid solution amount to copper of less than 0.2 at %.

## Claims

### Claim 1

A method for producing a lamination shaped product using a copper alloy powder for lamination shaping comprising at least one additive element having a solid solution amount to copper of less than 0.2 at %, the method comprising the steps of:
spreading the copper alloy powder on a shaping stage to form a thin layer thereon; and
irradiating a portion of the thin layer to be shaped with an electron beam to melt the copper alloy powder and then solidifying the molten copper alloy powder by natural cooling;
wherein the steps are repeated several times to produce a lamination shaped product.

### Claim 2

A method for producing a lamination shaped product using a copper alloy powder for lamination shaping comprising at least one additive element having a solid solution amount to copper of less than 0.2 at %, the method comprising the steps of:
spreading the copper alloy powder on a shaping stage to form a thin layer thereon; and
irradiating a portion of the thin layer to be shaped with a laser beam to melt the copper alloy powder and then solidifying the molten copper alloy powder by natural cooling;
wherein the steps are repeated several times to produce a lamination shaped product.

### Claim 3

A lamination shaped product comprising a copper alloy, wherein the copper alloy contains at least one additive element having a solid solution amount of less than 0.2 at %, and the copper alloy has a relative density of 98% or more relative to theoretical density; a conductivity of 50% IACS or more, and a 0.2% yield strength of 700 MPa or more.

### Claim 4 (depends on 3)

The lamination shaped product according to claim 3, wherein the additive element is at least one selected from the group consisting of W, Zr, Nb, Nd, Y, Mo, Os or Ru.

### Claim 5 (depends on 3)