# US 2025/0083133 A1 · Cobalt-Based Single-Atom Dehydrogenation Catalysts and Method for Producing Corresponding Olefins from Paraffins Using the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0083133 A1
- Document ID: US20250083133A1
- Status: Published application
- Kind: A1
- Application number: 18/960,341
- Filed: 2024-11-26
- Published: 2025-03-13
- Earliest claimed: 2018-10-31
- Assignees: SK Innovation Co., Ltd.; SK Geo Centric Co., Ltd.
- Applicants: SK Innovation Co., Ltd.; SK Geo Centric Co., Ltd.
- Inventors: Ho Won Lee; Je Mi Lim; Hee Soo Kim; Ju Hwan Im; Dae Hyun Choo; Ka Young Kim; Jae Suk Choi
- Web page: https://patentgrep.com/patent/US20250083133A1

## CPC

- B01J 23/75: Cobalt
- B01J 21/08: Silica
- B01J 35/615: {100-500 m2/g}
- B01J 35/633: {less than 0.5 ml/g}
- B01J 35/635: {0.5-1.0 ml/g}
- B01J 35/643: {less than 2 nm}
- B01J 35/647: {2-50 nm}
- B01J 35/651: {50-500 nm}
- B01J 37/02: Impregnation, coating or precipitation ({B01J37/0009 and B01J37/0018 take precedence } ; protection by coating B01J33/00)
- B01J 37/0205: {in several steps}
- B01J 37/0207: {Pretreatment of the support}
- B01J 37/0209: {involving a reaction between the support and a fluid}
- B01J 37/0213: {Preparation of the impregnating solution}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C07C 5/3335: {with metals}
- C07C 2521/08: Silica
- C07C 2523/75: Cobalt
- Y02P 20/52: using catalysts, e.g. selective catalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

In the present disclosure, a dehydrogenation catalyst in which cobalt in the form of single atom is supported on an inorganic oxide (specifically, silica) support in which an alkali metal in the form of single atom is fixed by alkali metal pretreatment and a method for producing the same, and a method for producing olefins by dehydrogenating corresponding paraffins, specifically light paraffins in the presence of the dehydrogenation catalyst are described.

## Claims

### Claim 1

A dehydrogenation catalyst that is a cobalt-based single-atom catalyst comprising:
silica having an alkali metal adsorbed thereon as a support; and
cobalt, as an active metal, loaded on the support,
wherein the cobalt having an oxidation number of 2+ and the alkali metal having an oxidation number of 1+, respectively, exist in an isolated form of single atom on the silica while the cobalt having an oxidation number of 2+ forms a tetrahedrally coordinated at the three-membered siloxane ring present on the surface of silica.

### Claim 2 (depends on 1)

The dehydrogenation catalyst according to claim 1, wherein a content of cobalt in the catalyst is in a range of 0.1% to 10% by weight.

### Claim 3 (depends on 2)

The dehydrogenation catalyst according to claim 2, wherein a content of an alkali metal in the catalyst is in a range of 0.00001% to 1% by weight.

### Claim 4 (depends on 3)

The dehydrogenation catalyst according to claim 3, wherein a weight ratio of cobalt (Co)/alkali metal in the catalyst is in a range of 1 to 2000.

### Claim 5 (depends on 1)

A method for producing an olefin from a paraffin, the method comprising:
providing a feedstock containing a light paraffin;
subjecting the feedstock to dehydrogenation at a temperature of 500° C. to 700° C. under a pressure of 0.3 to 2 bar in presence of the catalyst according to claim 1; and
recovering the olefin corresponding to the light paraffin from the dehydrogenation product.

### Claim 6 (depends on 5)

The method for producing an olefin from a paraffin according to claim 5, wherein the feedstock is provided as a gaseous phase.

### Claim 7 (depends on 6)

The method for producing an olefin from a paraffin according to claim 6, wherein the paraffin is a light paraffin having 2 to 5 carbon atoms.

### Claim 8 (depends on 7)

The method for producing an olefin from a paraffin according to claim 7, wherein a content of the light paraffin in the feedstock is at least 50% by volume.

### Claim 9 (depends on 5)

The method for producing an olefin from a paraffin according to claim 5, wherein a gas hourly space velocity (GHSV) is set in a range of 100 to 2000 hr−1 in a standard state of the dehydrogenation.