# US 2025/0083132 A1 · Fischer-tropsch catalysts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0083132 A1
- Document ID: US20250083132A1
- Status: Published application
- Kind: A1
- Application number: 18/672,684
- Filed: 2024-05-23
- Published: 2025-03-13
- Earliest claimed: 2023-09-13
- Assignees: Dimensional Energy, Inc.
- Applicants: Dimensional Energy, Inc.
- Inventors: Rafael Luis Espinoza
- Web page: https://patentgrep.com/patent/US20250083132A1

## CPC

- B01J 23/75: Cobalt
- B01J 23/8913: {Cobalt and noble metals}
- B01J 35/30: characterised by their physical properties
- B01J 35/37: Crush or impact strength
- B01J 35/613: {10-100 m2/g}
- B01J 35/633: {less than 0.5 ml/g}
- B01J 35/635: {0.5-1.0 ml/g}
- B01J 35/647: {2-50 nm}
- B01J 37/0205: {in several steps}
- B01J 37/0242: {Coating followed by impregnation}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 21/04: Alumina
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

A Fischer-Tropsch catalyst includes a substantially homogeneous blend of cobalt and alumina, wherein the catalyst includes a pore volume (PV) ranging from 0.3 cc/g to 0.5 cc/g and an average pore diameter (PD) ranging from 18 nm to 30 nm. Methods of preparing the Fischer-Tropsch catalyst are also included in the present disclosure.

## Claims

### Claim 1

A method for preparing a Fischer-Tropsch catalyst, the method comprising:
forming a mixture using a cobalt salt, a liquid, and boehmite;
shaping the mixture subsequent to forming the mixture, sufficient to form a structure;
drying the structure to form a dried structure;
calcining the dried structure sufficient to form a catalyst;
optionally adding one or more metals to the catalyst by impregnation, wherein the one or more metals include cobalt; and
optionally reducing the catalyst.

### Claim 2 (depends on 1)

The method of claim 1, wherein the cobalt salt includes cobalt nitrate, the liquid includes water, and the cobalt salt is mixed with the liquid to form a cobalt-containing solution prior to mixing with boehmite.

### Claim 3 (depends on 1)

The method of claim 1, wherein the mixture includes a silver salt.

### Claim 4 (depends on 3)

The method of claim 3, wherein the silver salt includes silver nitrate.

### Claim 5 (depends on 1)

The method of claim 1, wherein the mixture includes an additional aluminum-containing compound.

### Claim 6 (depends on 1)

The method of claim 1, wherein the mixture includes one or more of platinum salt, palladium salt, ruthenium salt, silver salt, silicon, titanium, and zirconium.

### Claim 7

(canceled)

### Claim 8 (depends on 1)

The method of claim 1, wherein the mixture is in the form of a paste, and wherein shaping the mixture includes extruding the paste.

### Claim 9 (depends on 1)

The method of claim 1, wherein the one or more metals further include at least one of ruthenium and iron.

### Claim 10 (depends on 1)

The method of claim 1, wherein the catalyst includes cobalt oxide and between 25 wt. % to 75 wt. % of the cobalt oxide in the catalyst before reduction is present from the mixture.

### Claim 11 (depends on 1)

The method of claim 1, wherein the catalyst includes a blend of cobalt and alumina, and wherein the catalyst includes a pore volume (PV) ranging from 0.3 cc/g to 0.5 cc/g and an average pore diameter (PD) ranging from 18 nm to 30 nm.

### Claim 12

A method for preparing a Fischer-Tropsch catalyst, the method comprising:
mixing a first precursor and a second precursor sufficient to form a paste, wherein the first precursor includes a solution including at least cobalt nitrate and silver nitrate, and wherein the second precursor includes boehmite;
extruding the paste sufficient to form a structure;
calcining the structure sufficient to form a catalyst;
optionally adding one or more metals to the catalyst by impregnation, wherein the one or more metals include cobalt; and
optionally reducing the catalyst.

### Claim 13 (depends on 12)

The method of claim 12, wherein the first precursor further includes one or more of platinum, palladium, and ruthenium, and wherein the second precursor further includes one or more of an additional aluminum-containing compound, silicon, titanium, and zirconium.

### Claim 14 (depends on 12)

The method of claim 12, wherein the paste has a modified loss on ignition (MLOI) value between 30 and 60.

### Claim 15 (depends on 12)

The method of claim 12 further including drying the structure prior to calcining the structure, wherein drying the structure includes heating the structure at a temperature ranging from about 70° C. to about 180° C.

### Claim 16 (depends on 12)

The method of claim 12, wherein calcining the structure includes heating the structure at a temperature below about 725° C.

### Claim 17 (depends on 12)

The method of claim 12, wherein the one or more metals further include ruthenium.

### Claim 18 (depends on 12)

The method of claim 12, wherein the one or more metals further include iron.

### Claim 19

(canceled)

### Claim 20 (depends on 12)

The method of claim 12, wherein the catalyst includes a blend of cobalt and alumina, and wherein the catalyst includes a pore volume (PV) ranging from 0.3 cc/g to 0.5 cc/g and an average pore diameter (PD) ranging from 18 nm to 30 nm.

### Claim 21

A method for preparing a catalyst, the method comprising:
forming a first mixture including a cobalt salt and water;
forming a second mixture by adding boehmite to the first mixture;
shaping the second mixture sufficient to form a structure;
optionally drying the structure;
calcining the structure sufficient to form a catalyst;
optionally adding one or more metals to the catalyst by impregnation, wherein the one or more metals include cobalt; and
optionally reducing the catalyst.

### Claim 22 (depends on 21)

The method of claim 21, wherein the cobalt salt includes cobalt nitrate, and the first mixture further includes at least one of silver nitrate, silicic acid hydrate, and nitric acid.