# US 2025/0082816 A1 · Wound dressing based on polymeric mixture of cellulose acetate and hyaluronic acid embedded with copper oxide and magnesium oxide nanoparticles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0082816 A1
- Document ID: US20250082816A1
- Status: Published application
- Kind: A1
- Application number: 18/533,052
- Filed: 2023-12-07
- Published: 2025-03-13
- Earliest claimed: 2023-09-08
- Assignees: King Faisal University
- Applicants: King Faisal University
- Inventors: MOHAMED GOUDA; HANY MOHAMED ABD EL-LATEEF AHMED
- Web page: https://patentgrep.com/patent/US20250082816A1

## CPC

- A61L 15/28: Polysaccharides or their derivatives {(A61L15/225 takes precedence)}
- A61L 15/18: containing inorganic materials
- A61L 2300/102: Metals or metal compounds, e.g. salts such as bicarbonates, carbonates, oxides, zeolites, silicates
- A61L 2400/12: Nanosized materials, e.g. nanofibres, nanoparticles, nanowires, nanotubes; Nanostructured surfaces
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)

## Abstract

Wound dressings fabricated from a polymeric mixture of cellulose acetate and hyaluronic acid embedded with copper oxide and/or magnesium oxide nanoparticles and a method of making the wound dressing. The method includes combining hyaluronic acid and deionized water to form a first mixture, combining cellulose acetate and acetone to form a second mixture, combining the first and second mixtures to form a third mixture of hyaluronic acid, cellulose acetate, deionized water and acetone, separately adding at least one of a copper acetate solution and a magnesium chloride solution to the third mixture to form a fourth mixture, adding sodium hydride to the fourth mixture to form a final mixture, and drying the final mixture to form a film used for the wound dressing. Different weights of copper oxide and magnesium oxide can be chosen to achieve a certain morphological appearance. The wound dressing is a promising option for wound healing.

## Claims

### Claim at position 1

1-6. (canceled)

### Claim 7

A method for making a wound dressing, the method comprising:
combining hyaluronic acid and deionized water to form a first mixture;
combining cellulose acetate and acetone to form a second mixture;
combining the first and second mixtures to form a third mixture of hyaluronic acid, cellulose acetate, deionized water, and acetone;
separately adding at least one of a copper acetate solution and a magnesium chloride solution to the third mixture to form a fourth mixture;
adding sodium hydride to the fourth mixture under an ultrasonic bath to form a final mixture; and
drying the final mixture to form a film used as the wound dressing;
wherein the ratio of hyaluronic acid to deionized water in the first mixture is about 1:10 (g/mL);
wherein the ratio of cellulose acetate to acetone in the second mixture is about 1:10 (g/mL).

### Claim at position 3

-9. (canceled)

### Claim 10 (depends on 7)

The method of making a wound dressing according to claim 7, wherein the ultrasonic bath lasts for a minimum of 30 minutes.

### Claim 11 (depends on 7)

The method of making a wound dressing according to claim 7, wherein the third mixture is stirred until a clear solution is obtained.

### Claim 12 (depends on 7)

The method of making a wound dressing according to claim 7, wherein both the copper acetate solution and the magnesium chloride solution are added to the third mixture to form the fourth mixture.

### Claim at position 7

13-18. (canceled)