# US 2025/0081970 A1 · Polymer nanocomposites with sub 5nm nanoparticles for improved antimicrobial effectiveness

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0081970 A1
- Document ID: US20250081970A1
- Status: Published application
- Kind: A1
- Application number: 18/292,950
- Filed: 2022-05-23
- Published: 2025-03-13
- Earliest claimed: 2021-07-28
- Assignees: Sabanci Universitesi Nanoteknoloji Arastirma Ve Uygulama Merkezi
- Applicants: Sabanci Universitesi Nanoteknoloji Arastirma Ve Uygulama Merkezi
- Inventors: Mustafa Kemal BAYAZIT; Meral YUCE
- Web page: https://patentgrep.com/patent/US20250081970A1

## CPC

- A01N 59/16: Heavy metals; Compounds thereof
- A01N 25/10: Macromolecular compounds
- A01N 25/28: Microcapsules {or nanocapsules}
- A01N 59/20: Copper
- A01N: PRESERVATION OF BODIES OF HUMANS OR ANIMALS OR PLANTS OR PARTS THEREOF (preservation of food or foodstuff A23); BIOCIDES, e.g. AS DISINFECTANTS, AS PESTICIDES OR AS HERBICIDES (preparations for medical, dental or toiletry purposes which kill or prevent the growth or proliferation of unwanted organisms A61K); PEST REPELLANTS OR ATTRACTANTS; PLANT GROWTH REGULATORS

## Abstract

A method for producing a metal nanoparticle-polymer composite that includes uniformly shaped metal nanoparticles uniformly dispersed in a polymer matrix is provided. The method may be used to produce a silver nanoparticle-polymer composite that includes nanoparticles having a size smaller than 5 nm by a double-syringe microwave-flow system.

## Claims

### Claim 1

A method for production of an antimicrobial polymer nanocomposite structure comprising the steps of:
a) dissolving a polymer in an aqueous or organic solvent at room temperature;
b) preparing a solution of a metal salt precursor by dissolving the metal salt precursor in a solvent that does not act as a reducing agent at ambient conditions and is miscible with the aqueous or organic solvent the polymer is dissolved in;
c) transferring the solutions prepared in steps a and b into a coiled-flow reactor by two syringes controlled by syringe pumps or by peristaltic pumps to obtain pre-defined reaction concentrations for scalable productions or by a single syringe if no reducing agent is used at room temperature in the solvents from steps a and b by closing one valve;
d) pre-mixing the solutions prepared in steps a and b in a three-way connector for homogeneous mixture formation before reaching the coiled-flow reactor;
e) dispensing the solutions prepared in steps a and b to the coiled-flow reactor at known concentrations and flow rates under constant microwave power; and
f) producing homogeneously distributed nanoparticles (NPS) with <5 nm in size in a polymer matrix under controlled pressure provided by a pressure regulator and pressurized gas.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the polymer is a polyamide, a polyester, a polyurethane or a cellulose acetate.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the polyamide is nylon-6.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the polyester is polycaprolactone.

### Claim 5 (depends on 2)

The method according to claim 2, wherein the polyurethane is thermoplastic polyurethane.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the metal salt precursor comprises inorganic/organic silver, inorganic/organic copper, inorganic/organic zinc, or inorganic/organic iron.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the organic solvent is DMF, NMP, DMAc, DMSO or formic acid.

### Claim 8 (depends on 1)

An antimicrobial polymer nanocomposite structure comprising inorganic nanoparticles dispersed in a polymer matrix having particle size less than 5 nm produced according the method of claim 1.

### Claim 9 (depends on 6)

The method according to claim 6, wherein the metal salt precursor comprises inorganic/organic silver.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the inorganic/organic silver is AgNO3, CH3COOAg.

### Claim 11 (depends on 6)

The method according to claim 6, wherein the metal salt precursor comprises inorganic/organic copper.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the inorganic/organic copper is Cu(NO3)2, CuCO2CH3.

### Claim 13 (depends on 6)

The method according to claim 6, wherein the metal salt precursor comprises inorganic/organic zinc.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the inorganic/organic zinc is Zn(NO3)2, Zn(CH3COO)2.

### Claim 15 (depends on 6)

The method according to claim 6, wherein the metal salt precursor comprises inorganic/organic iron.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the inorganic/organic iron is Fe(NO3)3, Fe(CO2CH3)2.