# US 2025/0073694 A1 · Plasma-treated single atom catalyst, production method thereof and use of the catalyst

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0073694 A1
- Document ID: US20250073694A1
- Status: Published application
- Kind: A1
- Application number: 18/725,020
- Filed: 2022-12-22
- Published: 2025-03-06
- Earliest claimed: 2021-12-30
- Applicants: Max-Planck-Gesellschaft Zur FöRderung Der Wissenschaften E.V.
- Inventors: Beatriz ROLDAN CUENYA; Shamil SHAIKHUTDINOV; Weiming WAN
- Web page: https://patentgrep.com/patent/US20250073694A1

## CPC

- B01J 37/0215: {Coating}
- B01J 37/349: {making use of flames, plasmas or lasers}
- B01J 21/063: {Titanium; Oxides or hydroxides thereof}
- B01J 23/10: of rare earths
- B01J 23/40: of the platinum group metals
- B01J 23/42: Platinum
- B01J 23/63: with rare earths or actinides
- B01J 35/394: {Metal dispersion value, e.g. percentage or fraction}
- B01J 35/45: Nanoparticles
- B01J 37/009: {Preparation by separation, e.g. by filtration, decantation, screening}
- B01J 37/0217: {Pretreatment of the substrate before coating}
- B01J 37/0225: {of metal substrates}
- B01J 37/0226: {Oxidation of the substrate, e.g. anodisation}
- B01J 37/0238: {via the gaseous phase-sublimation}
- B01J 37/03: Precipitation; Co-precipitation
- B01J 37/031: {Precipitation}
- B01J 37/035: {Precipitation on carriers}
- B01J 37/06: Washing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/088: {Decomposition of a metal salt}
- B01J 37/347: {Ionic or cathodic spraying; Electric discharge}
- C01B 32/50: Carbon dioxide
- C07C 5/08: of carbon-to-carbon triple bonds
- B01J 35/40: characterised by dimensions, e.g. grain size (in a colloidal state B01J35/23; crystallite size B01J35/77)
- B01J 2235/00: Indexing scheme associated with group B01J35/00, related to the analysis techniques used to determine the catalysts form or properties
- B01J 2235/10: Infrared [IR]
- B01J 2235/30: Scanning electron microscopy; Transmission electron microscopy
- C07C 2523/10: of rare earths
- C07C 2523/60: with zinc, cadmium or mercury
- C07C 2523/62: with gallium, indium, thallium, germanium, tin or lead
- C07C 2523/63: with rare earths or actinides
- C07C 2523/66: Silver or gold
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

The present invention relates to a catalytically active material, the preparation thereof, and the use of the catalytically active material, e.g. in the catalytic oxidation of CO to CO2 or in the catalytic hydrogenation of alkyne. The catalytically active material comprises a support5 comprising a metal oxide, and atomically dispersed noble metal on the surface of the support, wherein the metal oxide is selected from TiO2, CeO2, ZnO, SnO2, Ga2O3, In2O3, ZrO2, and Fe2O3, the noble metal is selected from Pt, Pd, Rh, and Au, and the catalytically active material is obtainable by a method comprising a step of non-thermal plasma treatment in the presence of O2.

## Claims

### Claim 1

A catalytically active material comprising
a support comprising a metal oxide, and
atomically dispersed noble metal on the surface of the support, wherein
the metal oxide is selected from TiO2, CeO2, ZnO, SnO2, Ga2O3, In2O3, ZrO2, and Fe2O3,
the noble metal is selected from Pt, Pd, Rh, and Au, and
the catalytically active material is obtainable by a method comprising a step of non-thermal plasma treatment in the presence of O2.

### Claim 2 (depends on 1)

The catalytically active material according to claim 1, wherein
the number of the noble metal atoms normalized to the surface area of the catalytically active material is from 3.0×1012 at/cm2 to 8.0×1014 at/cm2.

### Claim 3 (depends on 1)

The catalytically active material according to claim 1, wherein
the relative intensity of the noble metal in oxidation state X with respect to the total intensity of the noble metal of all oxidation states in the catalytically active material is 50% or more, as measured by X-ray photoelectron spectroscopy, wherein
X is 2+ for Pt and Pd, and X is 3+ for Rh and Au.

### Claim 4 (depends on 1)

The catalytically active material according to claim 1, wherein
an infrared absorption spectrum measured on the catalytically active material shows an absorption band within the range of 2085 cm−1 to 2120 cm−1 that does not change upon heating the material from 300 K to 500 K, when measured under the following condition:
(1) exposing the catalytically active material in a reaction cell to a reaction mixture consisting of 1% CO and 5% O2 balanced by Ar at 1 bar,
(2) heating the catalytically active material to 500 K at a rate of 60 K/min and reacting the mixture for 5 min at 1 bar at 500 K,
(3) cooling down the reaction mixture and the catalytically active material to 300 K,
(4) removing the reaction mixture from the reaction cell and applying ultrahigh vacuum conditions of 10−9 mbar or less,
(5) recording a spectrum in ultrahigh vacuum at 300 K without additional exposure to CO,
(6) increasing the temperature to 500 K at a rate of 60 K/min and recording spectra at 320 K, 360 K, 400 K, 440 K, 480 K and 500 K, and
(7) comparing the absorption maxima in the spectra recorded at the respective temperatures.

### Claim 5 (depends on 1)

The catalytically active material according to claim 1, wherein the metal oxide and the noble metal are selected from the following material combinations:
the metal oxide is selected from TiO2 and CeO2 and
the noble metal from Pt and Pd, wherein
the metal oxide is CeO2 and the noble metal is Pt.

### Claim 6 (depends on 1)

The catalytically active material according to claim 1, wherein
the support is in the form of particles or powder.

### Claim 7 (depends on 6)

The catalytically active material according to claim 6, wherein the support consists of the metal oxide.

### Claim 8 (depends on 6)

The catalytically active material according to claim 6, wherein
the powder support has an average particle diameter of 10 nm to 50 nm, as measured by scanning transmission electron microscopy, and is CeO2 powder support.

### Claim 9

(canceled)

### Claim 10 (depends on 1)

The catalytically active material according to claim 1, wherein
the support is in the form of a film.

### Claim 11 (depends on 10)

The catalytically active material according to claim 10, wherein
the support consists of a substrate and clusters supported on the substrate,
the substrate and the clusters comprise the same metal oxide, and
the average diameter of the clusters is 2.0 nm or less as determined by scanning tunneling microscopy.

### Claim 12 (depends on 11)

The catalytically active material according to claim 11, wherein the substrate and the clusters consist of the same metal oxide.

### Claim 13 (depends on 1)

A method for a catalytic oxidation of CO to CO2, comprising using the catalytically active material according to claim 1, wherein the catalytically active material is used as follows:
a gas mixture comprising CO and O2 is reacted in the presence of the catalytically active material at a pressure of 0.8 to 2.0 bar, and at reaction temperatures of 323 K to 573 K, wherein
the content of CO in the gas mixture is 5 vol % or less,
the content of O2 in the gas mixture is 2 vol % or more and 25 vol % or less, and
the CO/O2 molar ratio is 2.0 or less.

### Claim 14 (depends on 1)

A method for a catalytic hydrogenation of alkyne,
comprising using the catalytically active material according to claim 1, wherein the catalytically active material is used as follows:
a gas mixture comprising an alkyne and H2 is reacted in the presence of the catalytically active material at a pressure of 0.8 to 2.0 bar, at a temperature of 323 K to 573 K, wherein
the content of the alkyne in the gas mixture is 10 vol % or less,
the alkyne to H2 molar ratio in the gas mixture is 1 or less, and
the alkyne is a C2-C5 alkyne, and more C2-C3 alkyne.

### Claim 15 (depends on 6)

A method for producing the catalytically active material according to claim 6, comprising the steps of
(1) providing a precursor for the catalytically active material comprising a support in the form of particles comprising a metal oxide and noble metal on the surface of the support,
(2) calcining the precursor for the catalytically active material in the presence of O2, and
(3) carrying out a non-thermal plasma treatment of the calcined precursor for the catalytically active material in the presence of O2.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the step (1) is selected from the following steps (1a) and (1b):
(1a) depositing the noble metal onto the support from an aqueous solution of a salt of the noble metal, wherein the support consists of the metal oxide, and
(1b) co-precipitating the noble metal and the metal oxide from an aqueous solution containing salts of the noble metal and the metal oxide.

### Claim 17 (depends on 15)

The method according to claim 15, wherein the non-thermal plasma treatment is carried out at a pressure of 20 mbar or less and at an O2 content of 5 vol % or more.

### Claim 18 (depends on 10)

A method for producing the catalytically active material according to claim 10 selected from Methods A and B,
Method A comprising steps of:
(1) providing a metal oxide film support,
(2) carrying out a non-thermal plasma treatment in the presence of O2 to obtain a plasma-treated metal oxide film support, and
(3) depositing noble metal onto the plasma-treated metal oxide film support in gas phase by physical vapor deposition of noble metal atoms;
Method B comprising steps of:
(1) providing a metal oxide film support,
(2) depositing noble metal onto the metal oxide film support from a solution containing the noble metal, and
(3) carrying out a non-thermal plasma treatment in the presence of O2;
wherein the non-thermal plasma treatment is carried out at a pressure of 1×10−6 mbar to 1×10−5 mbar of O2.

### Claim 19 (depends on 2)

The catalytically active material according to claim 2, wherein
the number of the noble metal atoms normalized to the surface area of the catalytically active material is from 3.0×1012 at/cm2 to 4.0×1014 at/cm2 or from 6.0×1012 at/cm2 to 2.0×1014 at/cm2.

### Claim 20 (depends on 3)

The catalytically active material according to claim 3, wherein
the relative intensity of the noble metal in oxidation state X with respect to the total intensity of the noble metal of all oxidation states in the catalytically active material is 75% or more, as measured by X-ray photoelectron spectroscopy, wherein
X is 2+ for Pt and Pd, and X is 3+ for Rh and Au.

### Claim 21 (depends on 11)

The catalytically active material according to claim 11, wherein
the average diameter of the clusters is 1.5 nm or less as determined by scanning tunneling microscopy.