# US 2025/0066238 A1 · Method for producing glass sheets and glass sheets produced by such method and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0066238 A1
- Document ID: US20250066238A1
- Status: Published application
- Kind: A1
- Application number: 18/945,655
- Filed: 2024-11-13
- Published: 2025-02-27
- Earliest claimed: 2019-10-28
- Assignees: Schott AG
- Applicants: Schott AG
- Inventors: Klaus-Peter Kurek; Martin Kurz; Andreas Ortner; Olaf Claussen
- Web page: https://patentgrep.com/patent/US20250066238A1

## CPC

- C03B 17/067: {combined with thermal conditioning of the sheets}
- C03B 33/0222: {Scoring using a focussed radiation beam, e.g. laser}
- B23K 26/0624: {using ultrashort pulses, i.e. pulses of 1 ns or less}
- B23K 26/073: Shaping the laser spot
- B23K 26/382: by boring
- B23K 26/53: for modifying or reforming the material inside the workpiece, e.g. for producing break initiation cracks
- B23K 26/703: {Cooling arrangements (by using a fluid stream B23K26/14)}
- C03B 25/025: {Glass sheets}
- C03B 33/0235: {Ribbons}
- C03B 33/033: Apparatus for opening score lines in glass sheets
- C03C 3/095: containing rare earths
- B23K 2103/54: {Glass}
- C03B 17/064: {by the overflow downdraw fusion process; Isopipes therefor}
- Y02P 40/57: Improving the yield, e-g- reduction of reject rates
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for producing ultra-thin glass sheets is provided that results in glass sheets with high edge strength. The method includes: hot forming a continuous glass ribbon with a glass thickness from molten glass; annealing the glass ribbon with an annealing rate chosen based on the glass thickness; producing a laser beam focus area that is longer than the glass thickness; introducing filamentary defects into the glass ribbon using the laser beam so that the filamentary defects extend from one face to the opposite face and are spaced apart from one another along the breaking lines to produce transverse breaking lines and longitudinal breaking lines with margins each comprising a thickened bead; separating the beads along the longitudinal breaking lines and separating glass sheets by severing along the transverse breaking lines.

## Claims

### Claim 1

A glass sheet, comprising:
a glass thickness between 15 μm and 2 mm between a first surface and a second surface;
a Weibull modulus according to DIN EN 843-5 of more than 7;
a characteristic stress at break of more than 130 MPa; and
at least one edge along the thickness, the at least one edge having a plurality of rough surface areas of filamentary defects spaced apart from a plurality of flat surface areas without the filamentary defects.

### Claim 2 (depends on 1)

The glass sheet of claim 1, wherein the characteristic stress at break is more than 150 MPa.

### Claim 3 (depends on 1)

The glass sheet of claim 1, further comprising a coefficient of thermal expansion of greater than 6 ppm/Kelvin.

### Claim 4 (depends on 1)

The glass sheet of claim 1, wherein the glass thickness is equal to or less than 100 μm.

### Claim 5 (depends on 1)

The glass sheet of claim 1, further comprising an area ratio of the flat surface areas to the rough surface areas between 3:10 and 2:1.

### Claim 6 (depends on 1)

The glass sheet of claim 1, wherein the glass sheets is configured for a use selected from a group consisting of an insulating intermediate substrate, a spacer for an electronic component, an encapsulating optoelectronic component, a substrate for a thin-film cell, a substrate for a thin-film batteries, a substrate for a thin-film solar cell, a composite substrates for a display, and a microfluidic cell.

### Claim 7 (depends on 1)

The glass sheet of claim 1, wherein the at least one edge exhibits an annealing-dependent edge strength (KGK) which satisfies KGK=KG/K, wherein KG denotes a strength value in MPa, and K denotes the annealing rate in Kelvin/s, and
wherein the annealing-dependent edge strength KGK is selected from a group consisting of: greater than 0.2 MPa·s/Kelvin for the glass thickness of at least 30 μm; greater than 0.5 MPa·s/Kelvin for the glass thickness of at least 30 μm; greater than 0.5 MPa·s/Kelvin for the glass thickness of at least 50 m; greater than 0.9 MPa·s/Kelvin for the glass thickness of at least 50 μm; greater than 1.5 MPa·s/Kelvin for the glass thickness of at least 100 μm; greater than 2 MPa·s/Kelvin for the glass thickness of at least 100 μm; and any combinations thereof.

### Claim 8 (depends on 1)

The glass sheet of claim 1, wherein the filamentary defect have a mean spacing to one another ranging from 1 μm to 10 μm.

### Claim 9 (depends on 1)

The glass sheet of claim 1, wherein the glass comprises the following components, in wt %:
SiO2 58 to 65
B2O3 6 to 10.5
Al2O3 14 to 25
MgO 0 to 3
CaO 0 to 9
BaO 3 to 8
ZnO 0 to 2,
with the total of the contents of MgO, CaO, and BaO ranging from 8 to 18 wt %.

### Claim 10 (depends on 1)

The glass sheet of claim 1, wherein the glass comprises the following components, in wt %:
SiO2 50-70
Al2O3 10-20
B2O3 5-15
CaO 4-8
BaO 0.5-5
SrO 4-8.

### Claim 11 (depends on 1)

The glass sheet of claim 1, wherein the glass comprises the following components, in wt %:
SiO2 30 to 85
B2O3 3 to 20
Al2O3 0 to 15
Na2O 3 to 15
K2O 3 to 15
ZnO 0 to 12
TiO2 0.5 to 10
CaO 0 to 0.1.

### Claim 12 (depends on 1)

The glass sheet of claim 1, wherein the glass comprises the following components, in wt %:
SiO2 50 to 65
Al2O3 15 to 20
B2O3 0 to 6
Li2O 0 to 6
Na2O 8 to 15
K2O 0 to 5
MgO 0 to 5
CaO 0 to 7
ZnO 0 to 4
ZrO2 0 to 4
TiO2 0 to 1.

### Claim 13

A glass ribbon, comprising:
a glass thickness in a range from 15 μm to 2 mm between a first face and a second face; and
filamentary defects extending from the first face to the second face, the filamentary defects being spaced apart from one another to define longitudinal breaking lines and transverse breaking lines, the longitudinal breaking lines being inward of margins having thickened beads, the transverse breaking lines being transverse to the longitudinal breaking lines.

### Claim 14 (depends on 13)

The glass ribbon of claim 13, wherein the filamentary defects are at most as deep as the glass thickness and have a mean spacing between adjacent defects in a range from 1 μm to 10 μm.

### Claim 15 (depends on 13)

A glass sheet separated from the glass ribbon of claim 13, where the glass sheet comprises:
at least one edge along the thickness, the at least one edge having a plurality of rough surface areas having the filamentary defects spaced apart from a plurality of flat surface areas without the filamentary defects;
a Weibull modulus according to DIN EN 843-5 of more than 7; and
a characteristic stress at break of more than 130 MPa.

### Claim 16 (depends on 15)

The glass sheet of claim 15, further comprising a coefficient of thermal expansion of greater than 6 ppm/Kelvin.

### Claim 17 (depends on 15)

The glass sheet of claim 15, wherein the glass thickness is equal to or less than 100 μm.

### Claim 18 (depends on 15)

The glass sheet of claim 15, further comprising an area ratio of the flat surface areas to the rough surface areas between 3:10 and 2:1.