# US 2025/0062494 A1 · Electrode Assembly

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0062494 A1
- Document ID: US20250062494A1
- Status: Published application
- Kind: A1
- Application number: 18/935,093
- Filed: 2024-11-01
- Published: 2025-02-20
- Earliest claimed: 2021-07-09
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Se Hyun Yoon; Beomsu Kim; Yong Nam Kim; Heeyong Kim; Dong Hyeuk Park; Dong Myung Kim; Jae Han Jung
- Web page: https://patentgrep.com/patent/US20250062494A1

## CPC

- B32B 37/0084: {Point bonding}
- H01M 10/0459: {Cells or batteries with folded separator between plate-like electrodes}
- B32B 7/08: by mechanical means
- B32B 37/0076: {characterised in that the layers are not bonded on the totality of their surfaces}
- H01M 10/0404: {Machines for assembling batteries}
- H01M 10/0583: of accumulators with folded construction elements except wound ones, i.e. folded positive or negative electrodes or separators, e.g. with "Z"-shaped electrodes or separators
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 50/46: Separators, membranes or diaphragms characterised by their combination with electrodes
- H01M 50/466: U-shaped, bag-shaped or folded
- H01M 50/491: Porosity
- B30B 15/064: {with heating or cooling means}
- H01M 4/043: {involving compressing or compaction}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B30B: PRESSES IN GENERAL (producing ultra-high pressure or ultra-high pressure and high temperature to effect modifications of a substance, e.g. for making artificial diamonds B01J3/00 ){(compressing means for refuse receptacles B65F1/1405)}
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

An electrode assembly includes a plurality of electrodes arranged in a stack along a stacking axis with a respective separator portion of an elongated separator sheet positioned between and winding around each of the electrodes in the stack along a serpentine path. The plurality of electrodes include a top electrode positioned at a top of the stack along the stacking axis, and the plurality of electrodes include a bottom electrode positioned at a bottom of the stack. The separator portions in the stack include a top separator portion abutting the top electrode and a bottom separator portion abutting the bottom electrode. The bottom electrode may have a thickness along the stacking axis that is from 80% to 120% of a thickness of the top electrode along the stacking axis. Moreover, a maximum thickness of each of the electrodes in the stack may be less than 8.3 mm.

## Claims

### Claim 1

An electrode assembly, comprising:
a plurality of electrodes arranged in a stack along a stacking axis with a respective separator portion of a plurality of separator portions positioned between each of the electrodes in the stack, the plurality of electrodes including a top electrode of the plurality of electrodes positioned at a top of the stack along the stacking axis and including a bottom electrode of the plurality of electrodes positioned at a bottom of the stack along the stacking axis, and the plurality of separator portions including a top separator portion abutting the top electrode and including a bottom separator portion abutting the bottom electrode,
wherein a maximum thickness of each of the electrodes in the stack is less than 8.3 mm, and
wherein a value of air permeability of the bottom separator portion is smaller than a value of air permeability of the top separator portion.

### Claim 2 (depends on 1)

The electrode assembly of claim 1, further comprising an intermediate separator portion between the top and bottom separator portions along the stacking axis, wherein the value of air permeability of the top separator portion and the value of air permeability of the bottom separator portion are each independently in a range from 80 sec/100 ml to 120 sec/100 ml per square inch of the respective separator portion at a pressure of 0.05 MPa, and wherein a value of air permeability of the intermediate separator portion is in a range from 70 sec/100 ml to 85 sec/100 ml per square inch of the intermediate separator portion at a pressure of 0.05 MPa.

### Claim 3 (depends on 1)

The electrode assembly of claim 1, wherein each of the plurality of separator portions is a portion of an elongated separator sheet, the elongated separator sheet being folded between each of the plurality of separator portions such that the elongated separator sheet follows a serpentine path traversing back and forth along an orthogonal dimension orthogonal to the stacking axis to extend between each successive one of the plurality of electrodes in the stack.

### Claim 4 (depends on 1)

The electrode assembly of claim 1, wherein the thickness of each of the electrodes in the stack has a thickness along the stacking axis that is from 70% to 120% of a thickness of the top electrode along the stacking axis.

### Claim 5 (depends on 4)

The electrode assembly of claim 4, wherein a minimum thickness of each of the electrodes of the electrode assembly is 8.2 mm.

### Claim 6 (depends on 1)

The electrode assembly of claim 1, wherein the plurality of electrodes include an intermediate electrode of the plurality of electrodes between the top electrode and the bottom electrode along the stacking axis, wherein the plurality of separator portions include an intermediate separator portion abutting the intermediate electrode, and wherein the intermediate separator portion is adhered to the intermediate electrode to a degree that it would take a peel force in a range from 5 gf to 35 gf per 20 mm width of the intermediate separator portion applied to an edge of the intermediate separator portion in order to peel the intermediate separator portion away from the intermediate electrode at a speed of 100 mm/min along the stacking axis.

### Claim 7 (depends on 1)

The electrode assembly of claim 1, wherein the plurality of separator portions include a top separator portion abutting the top electrode, and wherein the top separator portion is adhered to the top electrode to a degree that it would take a peel force in a range from 5 gf to 70 gf per 20 mm width of the top separator portion applied to an edge of the top separator portion in order to peel the top separator portion away from the top electrode at a speed of 100 mm/min along the stacking axis.

### Claim 8 (depends on 1)

The electrode assembly of claim 1, wherein the plurality of separator portions include a top separator portion abutting the top electrode, and wherein the top separator portion has a value of air permeability from 80 sec/100 ml to 120 sec/100 ml per square inch of the top separator portion at a pressure of 0.05 MPa.

### Claim 9 (depends on 1)

The electrode assembly of claim 1, wherein the plurality of separator portions include a bottom separator portion abutting the bottom electrode, and wherein the bottom separator portion is adhered to the bottom electrode to a degree that it would take a peel force in a range from 5 gf to 75 gf per 20 mm width of the bottom separator portion applied to an edge of the bottom separator portion in order to peel the bottom separator portion away from the bottom electrode at a speed of 100 mm/min along the stacking axis.

### Claim 10 (depends on 1)

The electrode assembly of claim 1, wherein the plurality of separator portions include a bottom separator portion abutting the bottom electrode, and wherein the bottom separator portion has a value of air permeability from 80 sec/100 ml to 120 sec/100 ml per square inch of the bottom separator portion at a pressure of 0.05 MPa.

### Claim 11 (depends on 1)

The electrode assembly of claim 1, wherein the plurality of electrodes include an intermediate electrode of the plurality of electrodes positioned between the top electrode and the bottom electrode along the stacking axis, wherein the plurality of separator portions include: an intermediate separator portion abutting the intermediate electrode, a top separator portion abutting the top electrode, and a bottom separator portion abutting the bottom electrode,
wherein the intermediate separator portion is adhered to the intermediate electrode to a degree that it would take a first peel force per 20 mm width of the intermediate separator portion applied to an edge of the intermediate separator portion in order to peel the intermediate separator portion away from the intermediate electrode at a speed of 100 mm/min along the stacking axis, wherein the top and bottom separator portions are adhered to the respective top and bottom electrodes to a degree that it would take a second peel force per 20 mm width of the respective top and bottom separator portions applied to an edge of the respective top and bottom separator portion in order to peel the respective top and bottom separator portion away from the respective top and bottom electrode at a speed of 100 mm/min along the stacking axis, and wherein a difference between the first peel force and the second peel force is from 3 gf/20 mm to 15 gf/20 mm.

### Claim 12 (depends on 1)

The electrode assembly of claim 1, wherein the plurality of electrodes include an intermediate electrode of the plurality of electrodes positioned between the top electrode and the bottom electrode along the stacking axis, wherein the separator portions include: an intermediate separator portion abutting the intermediate electrode, a top separator portion abutting the top electrode, and a bottom separator portion abutting the bottom electrode, wherein the intermediate separator portion has a second value of air permeability per square inch at a pressure of 0.05 MPa and at room temperature, and wherein the difference between the second value of air permeability and the value of air permeability of the top separator portion and the bottom separator portion is from 10 sec/100 ml to 35 sec/100 ml per square inch at a pressure of 0.05 MPa and at room temperature.

### Claim 13 (depends on 1)

The electrode assembly of claim 1, wherein the bottom electrode has a thickness along the stacking axis that is from 80% to 120% of a thickness of the top electrode along the stacking axis.

### Claim 14 (depends on 1)

The electrode assembly of claim 1, further comprising an intermediate separator portion between the top and bottom separator portions along the stacking axis, wherein a value of air permeability of the intermediate separator portion is smaller than the value of air permeability of the bottom separator portion.