# US 2025/0062319 A1 · Method of pre-forming anode particles having tailored solid electrolyte interphase composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0062319 A1
- Document ID: US20250062319A1
- Status: Published application
- Kind: A1
- Application number: 18/449,261
- Filed: 2023-08-14
- Published: 2025-02-20
- Earliest claimed: 2023-08-14
- Applicants: GM Global Technology Operations LLC
- Inventors: Jeffrey David Cain; Nicholas Paul William Pieczonka; Sayed Youssef Sayed Nagy; Zachary Hood; Shiba Adhikari
- Web page: https://patentgrep.com/patent/US20250062319A1

## CPC

- H01M 4/366: {as layered products}
- C25D 7/006: {Nanoparticles}
- C25D 9/02: with organic materials
- C25D 9/04: with inorganic materials
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0452: {from solutions}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/139: Processes of manufacture
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/4235: {Safety or regulating additives or arrangements in electrodes, separators or electrolyte (H01M10/4242 takes precedence)}
- H01M 10/446: {Initial charging measures}
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method is provided for pre-forming anode particles for use in lithium ion batteries. The pre-formed anode particles bear a solid electrolyte of a composition that cannot be formed in situ in the battery. The method includes providing a dispersion of anode precursor particles and an additive not found in the battery in a liquid electrolyte solution. Applying a voltage or current across the dispersion forms the solid electrolyte interphase, on the particles. These particles can be used in an electrode of a lithium ion battery.

## Claims

### Claim 1

A method of pre-forming anode particles bearing a solid electrolyte interphase, the anode particles being for use in an anode of a lithium ion battery, where the lithium ion battery includes the anode, an anode current collector, a cathode, a cathode current collector, an optional separator, and a battery electrolyte, the method comprising:
providing a dispersion in a vessel configured for electrochemical reactions, wherein the dispersion comprises anode precursor particles and a first liquid electrolyte solution, and the dispersion includes an additive not found in the lithium ion battery,
applying a voltage across the dispersion or applying a current across the dispersion to form the anode particles bearing the solid electrolyte interphase, and
recovering the anode particles bearing the solid electrolyte interphase from the dispersion.

### Claim 2 (depends on 1)

The method of claim 1 wherein the additive is present in the dispersion before applying the voltage or the current.

### Claim 3 (depends on 1)

The method of claim 1 wherein the additive is added to the dispersion during the application of the voltage or the current.

### Claim 4 (depends on 2)

The method of claim 2 wherein after applying the voltage or the current and during the application of the voltage or the current, introducing an additional additive to the dispersion to form a solid electrolyte interphase having a first layer of a first composition and a second layer of a second composition.

### Claim 5 (depends on 4)

The method of claim 4 further comprising repeating the step of introducing an additional additive and applying the voltage after introducing the additional additive.

### Claim 6 (depends on 1)

The method of claim 1 wherein the anode particles comprise silicon, germanium, tin, bismuth, graphite, antimony, silicon oxide, or a combination of two or more thereof.

### Claim 7 (depends on 1)

The method of claim 1 wherein the anode particles have an average particle size of from 50 nanometers to 100 micrometers.

### Claim 8 (depends on 1)

The method of claim 1 wherein the solid electrolyte interphase has a thickness of 1 to 100 nanometers.

### Claim 9 (depends on 1)

The method of claim 1 wherein the first liquid electrolyte solution comprises a salt in a solvent wherein the salt comprises lithium bis(fluorosulfonyl)imide, lithium bis(trifluoromethanesulfonyl)imide, lithium bis(oxalato) borate, lithium difluorooxalatoborate, or 1,1,2,2-tetra-fluoroethyl-2,2,3,3-tetrafluoropropyl ether and/or the solvent comprises ethylene carbonate, dimethyl carbonate, ethyl methyl carbonate, diethyl carbonate, propylene carbonate, dimethyl sulfoxide, ethyl acetate, gamma butyrolactone, 1,2-dimethoxyethane, or tetraethylene glycol dimethyl ether.

### Claim 10 (depends on 1)

The method of claim 1 wherein the additive comprises a fluorinated carbonate, a vinylene carbonate, an alkoxy silane, or an alkyl acrylamide.

### Claim 11 (depends on 1)

The method of claim 1 wherein the dispersion comprises 1 to 25 weight percent of the anode particles, and 0.001 to 10 weight percent of the additive based on total weight of the dispersion.

### Claim 12 (depends on 1)

The method of claim 1 wherein the electrochemical reaction vessel comprises a conductive shell as a current collector and an electrode comprising lithium metal.

### Claim 13 (depends on 1)

The method of claim 1 wherein voltage is applied at a level of +/−10 to +/−7000 millivolts.

### Claim 14 (depends on 1)

The method of claim 1 wherein current is applied at a level of from +/−0.01 to +/−10 milliamps per square centimeter.

### Claim 15 (depends on 1)

The method of claim 1 wherein the solid electrolyte interphase is a homogeneous composition.

### Claim 16 (depends on 1)

The method of claim 1 wherein the solid electrolyte interphase has a composition which varies along a gradient from a surface of the anode particle to a surface of the solid electrolyte interphase.

### Claim 17 (depends on 1)

The method of claim 1 wherein the solid electrolyte interphase is inorganic, organic, or a combination thereof.

### Claim 18 (depends on 1)

The method of claim 1 further comprising forming a second dispersion comprising the anode particles bearing the solid electrolyte interphase, and a second liquid electrolyte solution which is different from first liquid electrolyte solution and applying a voltage or a current across the dispersion to form a second layer of solid electrolyte interphase on the anode particles.

### Claim 19 (depends on 1)

The method of claim 1 comprising forming a slurry comprising the anode particles bearing the solid electrolyte interphase, a binder, a conductive component and solvent, applying the slurry to a current collector, drying and optionally curing to form an anode.

### Claim 20

A lithium ion battery comprising an anode disposed on an anode current collector, a cathode disposed on a cathode current collector, an optional separator, disposed between the anode and the cathode, and a battery electrolyte, wherein the anode comprises anode particles having a pre-formed solid electrolyte interphase of a composition that could not be formed in situ in the lithium ion battery.