# US 2025/0062310 A1 · Silicon-based active material for lithium secondary battery and secondary battery anode material using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0062310 A1
- Document ID: US20250062310A1
- Status: Published application
- Kind: A1
- Application number: 18/680,217
- Filed: 2024-05-31
- Published: 2025-02-20
- Earliest claimed: 2023-08-18
- Assignees: Korea Institute of Science and Technology
- Applicants: Korea Institute of Science and Technology
- Inventors: Jihyun HONG; Minah LEE; Jinkwan CHOI; Hun-Gi JUNG; Dong-Ik KIM
- Web page: https://patentgrep.com/patent/US20250062310A1

## CPC

- H01M 4/0416: {involving impregnation with a solution, dispersion, paste or dry powder (H01M4/0438 takes precedence)}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/483: {for non-aqueous cells (H01M4/485 takes precedence)}
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/625: {Carbon or graphite}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided are a prelithiation method of a silicon-based active material, the prelithiation method including step S1 of immersing the silicon-based active material in a prelithiation solution including an organic solvent and a lithium-hydrocarbon molecule complex, step S2 of obtaining a powder by washing the silicon-based active material with the organic solvent and drying the silicon-based active material, and step S3 of performing a heat treatment on the powder at a temperature of 400° C. to 800° C. in an inert gas atmosphere, and a silicon-based active material prelithiated by the method.

## Claims

### Claim 1

An prelithiation method of a silicon-based active material, the prelithiation method comprising:
step S1 of immersing the silicon-based active material in a prelithiation solution comprising an organic solvent and a lithium-hydrocarbon molecule complex;
step S2 of obtaining a powder by washing the silicon-based active material with the organic solvent and drying the silicon-based active material; and
step S3 of performing a heat treatment on the powder at a temperature of 400° C. to 800° C. in an inert gas atmosphere.

### Claim 2 (depends on 1)

The prelithiation method of claim 1, wherein a lithium content of the lithium-hydrocarbon molecule complex is 5 to 15 mass % with respect to a mass of the silicon-based active material.

### Claim 3 (depends on 1)

The prelithiation method of claim 1, wherein the silicon-based active material in step S1 is SiOx (0<x<2).

### Claim 4 (depends on 1)

The prelithiation method of claim 1, wherein the organic solvent comprises one or more of a cyclic ether-based solvent and a linear ether-based solvent.

### Claim 5 (depends on 4)

The prelithiation method of claim 4, wherein the cyclic ether-based solvent comprises one or more selected from a group consisting of tetrahydropyran, dioxolane, methyl dioxolane, dimethyl dioxolane, vinyl dioxolane, methoxy dioxolane, ethyl methyl dioxolane, oxane, dioxane, trioxane, tetrahydrofuran, methyl tetrahydrofuran, dimethyl tetrahydrofuran, dimethoxy tetrahydrofuran, ethoxy tetrahydrofuran, ethyl tetrahydrofuran, methyl tetrahydropyran, dimethyl tetrahydropyran, dihydropyran, tetrahydropyran, hexamethylene oxide, furan, dihydrofuran, dimethoxybenzene, and dimethyloxetane.

### Claim 6 (depends on 4)

The prelithiation method of claim 4, wherein the linear ether-based solvent comprises one or more selected from a group consisting of dimethyl ether, diethyl ether, ethyl methyl ether, ethyl propyl ether, dipropyl ether, diisopropyl ether, dibutyl ether, diisobutyl ether, ethyl tertbutyl ether, dimethoxymethane, trimethoxymethane, dimethoxyethane, diethoxyethane, dimethoxypropane, diethylene glycol dimethyl ether, diethylene glycol ethyl methyl ether, diethylene glycol isopropyl methyl ether, diethylene glycol butyl methyl ether, diethylene glycol diethyl ether, diethylene glycol tertbutyl ethyl ether, triethylene glycol dimethyl ether, tetraethylene glycol dimethyl ether, ethylene glycol ethylmethyl ether, ethylene glycol divinyl ether, diethylene glycol divinyl ether, triethylene glycol divinyl ether, and methoxypropane.

### Claim 7 (depends on 1)

The prelithiation method of claim 1, wherein the organic solvent comprises 2-methyltetrahydrofuran.

### Claim 8 (depends on 1)

The prelithiation method of claim 1, wherein the lithium-hydrocarbon molecule complex has an oxidation-reduction potential of 0.5 V or less with respect to lithium.

### Claim 9 (depends on 1)

The prelithiation method of claim 1, wherein
hydrocarbon molecules of the lithium-hydrocarbon molecule complex comprise biphenyl, naphthalene, anthracene, phenanthrene, tetracene, diphenylanthracene, perylene, pyrene, triphenylene, bianthryl, terphenyl, quaterphenyl, and stilbene, and
the hydrocarbon molecules are substituted or unsubstituted with one or more substituents selected from a group consisting of an alkyl group having 1 to 4 carbon atoms, benzene, fluorine, and chlorine.

### Claim 10 (depends on 1)

The prelithiation method of claim 1, wherein the heat treatment is performed in step S3 at a temperature equal to or higher than 450° C. and equal to or lower than 700° C.

### Claim 11 (depends on 1)

A silicon-based active material prelithiated by the prelithiation method of claim 1, the silicon-based active material comprising:
a complex of lithium silicon oxide of Li2SiO3 with a size of 12 nanometers (nm) or less and silicon with a size of 5 nm or less.

### Claim 12 (depends on 11)

The silicon-based active material of claim 11, wherein the complex further comprises lithium silicon oxide of Li2Si2O5 with a size of 10 nm or less, and a content of Li2Si2O5 is less than a content of Li2SiO3.

### Claim 13 (depends on 11)

An anode comprising:
the prelithiated silicon-based active material of claim 11;
a conductive material; and
a binder.

### Claim 14 (depends on 13)

The anode of claim 13, wherein a percentage of the prelithiated silicon-based active material is 70 weight % or more with respect to a total weight of the active material, the conductive material, and the binder constituting the anode.

### Claim 15 (depends on 13)

The anode of claim 13, wherein the prelithiated silicon-based active material further comprises one or more of graphite, amorphous carbon, hard carbon, soft carbon, and magnesium.

### Claim 16 (depends on 15)

The anode of claim 15, wherein a weight ratio of graphite to a silicon complex in the active material is 95:5 to 5:95.